A method for producing low molecular weight polytetrafluoroethylene which includes: (1) feeding into an airtight container in the absence of oxygen: high molecular weight polytetrafluoroethylene: and a halogenated polymer having a halogen atom other than a fluorine atom; and (2) irradiating the high molecular weight polytetrafluoroethylene to provide low molecular weight polytetrafluoroethylene having a melt viscosity at 380° C. of 1.0×102 to 7.0×105 Pa·s.
Claims5
A method for producing low molecular weight polytetrafluoroethylene, comprising:
- (1) feeding into an airtight container in the absence of oxygen:
- high molecular weight polytetrafluoroethylene having a standard specific gravity of 2.130 to 2.230:
- and
- a halogenated polymer having a halogen atom other than a fluorine atom;
- and
- (2) irradiating the high molecular weight polytetrafluoroethylene at a temperature of 320° C. or lower to provide low molecular weight polytetrafluoroethylene having a melt viscosity at 380° C. of 1.0×102 to 7.0×105 Pa·s.
3 more elements