Tarnish and sweat resistant low karat gold alloys
AssigneeLeachGarner, Inc.
InventorsWilliam Guenley, Mossig H. Makhoulian, Joe Esposito, Luke Autry, Scott Suvall
Life of this patent
Estimating the term…
Abstract
This invention provides low karat, low silver, 6 kt gold-copper-zinc alloys with acceptable workability that can be processed into wire, tube, sheet stock, or cast. The alloys are annealed at 1200° F., rapidly cooled, and heat treated at about 600° to 800° F., which increases the hardness and durability in finished parts made from these alloys. The alloys include grain refiners. The alloys are resistant to oxidation from sweat and tarnishing. Additional fabrication operations can form jewelry items such as balls, chain, hoops and studs.
Claims10
A castable 6 karat gold alloy comprising (w/w):
- Au 25%;
- Cu 45-60%;
- Zn 15-21%;
- at least one additional element selected from the group consisting of Al at up to 2%, Pd 4-6%, and Pt 4-6%;
- and
- Co exceeding 3% and not exceeding 4%.
Dependencies are inferred from the claim text.