Abstract
Described herein are methods of forming a neutron shielding material. Such material may comprise a powder blend comprising a first component comprising a blend of a first metal particle and a first ceramic particle; and a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix.
Claims20
A method of forming a neutron shielding material comprising:
- a) mixing together a first metal particle having a first grain growth temperature;
- a first ceramic particle;
- and a reinforcing chip to form a powder blend;
- and
- b) sintering the powder blend into a billet and extruding the billet at a hot-work temperature;
- wherein the reinforcing chip comprises a second ceramic particle homogeneously dispersed within a chip metal matrix having a second grain growth temperature;
- wherein the first metal particle is virgin aluminum powder;
- and
- wherein the hot-work temperature is lower than both of the first and second grain growth temperatures.
6 more elements
A method of forming a neutron shielding material comprising:
- a) mixing together a first metal particle having a first grain growth temperature;
- a first ceramic particle;
- and a reinforcing chip to form a powder blend;
- and
- b) sintering the powder blend into a billet and extruding the billet at a hot-work temperature;
- wherein the reinforcing chip comprises a second ceramic particle dispersed within a chip metal matrix having a second grain growth temperature;
- wherein the hot-work temperature is lower than both of the first and second grain growth temperatures;
- and
- wherein the reinforcing chip is formed prior to step a) by the steps comprising:
- i) mixing the second ceramic particle and a metal;
- ii) forming a billet from the mixture;
- iii) extruding the billet into a shaped form;
- and
- iv) machining the shaped form into the reinforcing chip mold.
11 more elements
A method of forming a neutron shielding material comprising:
- a) mixing together a first metal particle having a first grain growth temperature;
- a first ceramic particle comprising boron carbide;
- and a reinforcing chip to form a powder blend;
- and
- b) sintering the powder blend into a billet and extruding the billet at a hot-work temperature;
- wherein the reinforcing chip comprises a second ceramic particle dispersed within a chip metal matrix having a second grain growth temperature;
- and
- wherein the hot-work temperature is lower than both of the first and second grain growth temperatures.
5 more elements