# US 11,524,424 B2 · Production of oriented strand board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,524,424 B2
- Document ID: US11524424B2
- Status: Granted
- Kind: B2
- Application number: 16/536,574
- Filed: 2019-08-09
- Published: 2020-02-13
- Granted: 2022-12-13
- Earliest claimed: 2018-08-10
- Applicants: Norbord Inc.
- Inventors: Alain Laplante; Mathieu Thibault; Aleksander Nadezhdin
- Web page: https://patentgrep.com/patent/US11524424B2

## CPC

- B27N 3/20: characterised by using platen-presses
- B27N 3/002: {characterised by the type of binder (compositions of macromolecular compounds C08L)}
- B27N 3/02: from particles
- B27N 3/083: {Agents for facilitating separation of moulds from articles}
- B27N 3/086: {Presses with means for extracting or introducing gases or liquids in the mat}
- B27N 3/18: Auxiliary operations, e.g. preheating, humidifying, cutting-off
- B27N 3/203: {with heating or cooling means}
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)

## Abstract

A method of making a wood particle board containing sticking type resin coated wood particles wherein the top of a layup of the coated wood particles is smoothed to provide a smooth a top surface on the layup and a release agent is applied on the top surface and the so coated layup is consolidated into a board in a consolidating press under heat and pressure with the coated top surface in direct contact with a press platen.

## Claims

### Claim 1

A method for making wood particle boards, the method comprising:
forming a layup of resin coated strands, wherein a resin of the resin coated strands is an isocyanate resin, and wherein the layup comprises a top surface;
smoothing, by a steam press, the top surface of the layup, wherein smoothing comprises pre-pressing and steaming the top surface of the layup at the same time thereby forming a pre-pressed layup;
applying a release agent to the smoothed top surface thereby forming a release agent coated top surface;
cutting the pre-pressed layup into panels;
consolidating, by a consolidating press, the panels by contacting a coated top surface of each panel with a metal press platen of the consolidating press thereby forming the wood particle boards; and
removing the wood particle boards from the consolidating press,
wherein steaming comprises applying a steam dosage per unit area of between 21 g/square meter and 140 g/square meter.

### Claim 2 (depends on 1)

The method of claim 1, wherein the top surface of the layup is steamed in order to reduce stickiness of the top surfaces of the panels to metal press platens.

### Claim 3 (depends on 1)

The method of claim 1, wherein steaming comprises applying the steam dosage per unit area of between 80 g/square meter and 120 g/square meter.

### Claim 4 (depends on 1)

The method of claim 1, wherein the isocyanate resin is a polymeric diphenylmethane diisocyanate (pmdi) resin.

### Claim 5 (depends on 1)

The method of claim 1, wherein the wood particle boards are oriented strand boards (OSBs).

### Claim 6 (depends on 1)

The method of claim 1, wherein pre-pressing comprises reducing an initial layup height by 50% to 67%.

### Claim 7 (depends on 1)

The method of claim 1, further comprising, after applying the release agent and before consolidating, delaying the pre-pressed layup at a loader.

### Claim 8 (depends on 7)

The method of claim 7, wherein delaying the pre-pressed layup at the loader comprises delaying the panels so that they spend an average of 3 minutes at the loader.

### Claim 9

A method for making wood particle boards, the method comprising:
forming a layup of resin coated strands, wherein a resin of the resin coated strands is an adhesive resin capable of adhering to a metal surface of a press platen of a consolidating press, and wherein the layup comprises a top surface;
smoothing, by a steam press, the top surface of the layup, wherein smoothing comprises pre-pressing and steaming the top surface of the layup at the same time thereby forming a pre-pressed layup;
applying a release agent to the smoothed top surface thereby forming a release agent coated top surface;
cutting the pre-pressed layup into panels;
consolidating, by the consolidating press, the panels by contacting a coated top surface of each panel with the press platen of the consolidating press thereby forming the wood particle boards; and
removing the wood particle boards from the consolidating press,
wherein steaming comprises applying a steam dosage per unit area of between 80 g/square meter and 120 g/square meter, and
wherein the top surface of the layup is steamed in order to reduce stickiness of the top surfaces of the panels to press platens.

### Claim 10 (depends on 9)

The method of claim 9, wherein the adhesive resin is an isocyanate resin.

### Claim 11 (depends on 10)

The method of claim 10, wherein the adhesive resin is a polymeric diphenylmethane diisocyanate (pmdi) resin.

### Claim 12 (depends on 9)

The method of claim 9, further comprising, after applying the release agent and before consolidating, delaying the pre-pressed layup at a loader.

### Claim 13 (depends on 9)

The method of claim 9, further comprising, after applying the release agent and before consolidating, delaying the pre-pressed layup at a loader so that it spends an average of 3 minutes at the loader.

### Claim 14 (depends on 9)

The method of claim 9, wherein pre-pressing comprises reducing an initial layup height by 50% to 67%.

### Claim 15

A method for making wood particle boards, the method comprising:
forming a layup of resin coated strands, wherein a resin of the resin coated strands is an isocyanate resin, and wherein the layup comprises a top surface;
smoothing, by a steam press, the top surface of the layup, wherein smoothing comprises pre-pressing and steaming the top surface of the layup thereby forming a pre-pressed layup;
applying a release agent to the smoothed top surface thereby forming a release agent coated top surface;
after applying the release agent and before consolidating, delaying the pre-pressed layup at a loader;
cutting the pre-pressed layup into panels;
consolidating, by a consolidating press, the panels by contacting a coated top surface of each panel with a metal press platen of the consolidating press thereby forming the wood particle boards; and
removing the wood particle boards from the consolidating press,
wherein delaying the pre-pressed layup at the loader comprises delaying the panels so that they spend an average of 3 minutes at the loader.