# US 11,511,344 B2 · Iron nitride powder with anisotropic shape

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,511,344 B2
- Document ID: US11511344B2
- Status: Granted
- Kind: B2
- Application number: 16/737,156
- Filed: 2020-01-08
- Published: 2020-05-07
- Granted: 2022-11-29
- Earliest claimed: 2015-01-26
- Assignees: Regents of the University of Minnesota
- Applicants: Regents of the University of Minnesota
- Inventors: Jian-Ping Wang; YanFeng Jiang
- Web page: https://patentgrep.com/patent/US11511344B2

## CPC

- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B02C 17/005: {the charge being turned over by magnetic forces}
- B02C 17/14: Mills in which the charge to be ground is turned over by movements of the container other than by rotating, e.g. by swinging, vibrating, tilting {(mills provided with vibrators in general B02C19/16)}
- B02C 19/16: Mills provided with vibrators ({roller mills B02C4/423}; tumbling mills B02C17/14)
- B02C 19/18: Use of auxiliary physical effects, e.g. ultrasonic waves or irradiation, for disintegrating
- B22F 1/054: Nanosized particles
- B22F 1/0551: {Flake form nanoparticles}
- B22F 1/145: Chemical treatment, e.g. passivation or decarburisation
- C22C 33/02: by powder metallurgy
- H01F 1/065: {obtained by a reduction}
- H01F 1/083: {in a bonding agent}
- H01F 1/086: {sintered}
- B22F 2009/045: {by other means than ball or jet milling}
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

Techniques are disclosed for milling an iron-containing raw material in the presence of a nitrogen source to generate anisotropically shaped particles that include iron nitride and have an aspect ratio of at least 1.4. Techniques for nitridizing an anisotropic particle including iron, and annealing an anisotropic particle including iron nitride to form at least one α″-Fe16N2 phase domain within the anisotropic particle including iron nitride also are disclosed. In addition, techniques for aligning and joining anisotropic particles to form a bulk material including iron nitride, such as a bulk permanent magnet including at least one α″-Fe16N2 phase domain, are described. Milling apparatuses utilizing elongated bars, an electric field, and a magnetic field also are disclosed.

## Claims

### Claim 1

A material comprising:
an anisotropic particle comprising at least one iron nitride crystal,
wherein the anisotropic particle has an aspect ratio of at least 2.2,
wherein the aspect ratio comprises the ratio of the length of a longest dimension of the anisotropic particle to the length of a shortest dimension of the anisotropic particle, and
wherein the longest dimension and the shortest dimension are substantially orthogonal,
wherein the at least one iron nitride crystal's magnetic easy axis is substantially parallel to the longest dimension of the anisotropic particle;
wherein the at least one iron nitride crystal comprises a plurality of iron nitride crystals, and wherein the respective <001> crystal axes of the plurality of iron nitride crystals are substantially parallel;
wherein the length of the anisotropic particle measured in the direction of the substantially parallel <001> crystal axes of the plurality of iron nitride crystals is at least about 2.2 times the length of the anisotropic particle measured in at least one of a substantially orthogonal direction of the <100> crystal axes of the plurality of iron nitride crystals of the anisotropic particle or a substantially orthogonal direction of the <010> crystal axes of the plurality of iron nitride crystals of the anisotropic particle;
wherein the length of the anisotropic particle measured in the direction of the substantially parallel <001> crystal axes is about 1 micron (μm) and the length of the anisotropic particle measured in the direction of at least one of the substantially parallel <100> crystal axes or the substantially parallel <010> crystal axes is between about 200 nanometers (nm) and 500 nm.

### Claim 2 (depends on 1)

The material of claim 1, wherein the at least one iron nitride crystal comprises α″-Fe16N2.

### Claim 3 (depends on 1)

The material of claim 1, wherein the longest dimension of the anisotropic particle is substantially parallel to the substantially parallel respective <001> crystal axes of the plurality of iron nitride crystals.

### Claim 4 (depends on 1)

The material of claim 1, wherein at least some iron nitride crystals of the plurality of iron nitride crystals comprise at least one α″-Fe16N2 phase domain.

### Claim 5 (depends on 1)

The material of claim 1, wherein the anisotropic particle comprises a plurality of anisotropic particles.

### Claim 6 (depends on 5)

The material of claim 5, wherein the respective longest dimensions of respective particles of the plurality of anisotropic particles are substantially parallel.

### Claim 7 (depends on 5)

A bulk permanent magnet comprising the material of claim 5.

### Claim 8 (depends on 1)

The material of claim 1, wherein the anisotropic particle has a shape comprising that of a needle, flake, or lamination.

### Claim 9 (depends on 1)

A method of producing the material of claim 1, comprising:
aligning a plurality of anisotropic particles by at least exposing the anisotropic particles to a magnetic field, such that the longest dimensions of respective anisotropic particles of the plurality of anisotropic particles are substantially parallel,
wherein at least some anisotropic particles of the plurality of anisotropic particles comprise iron nitride and have an aspect ratio of at least 2.2,
wherein each anisotropic particle of the plurality of anisotropic particles includes at least one iron nitride crystal, and wherein the respective <001> crystal axes of at least some of the at least one iron nitride crystals of the plurality of anisotropic particles are substantially parallel to the longest dimensions of the respective anisotropic particles; and
joining the plurality of anisotropic particles to form a bulk material comprising iron nitride.

### Claim 10 (depends on 9)

The method of claim 9, wherein the magnetic field has a strength between about 0.01 Tesla (T) and about 50 T.

### Claim 11 (depends on 9)

The method of claim 9, wherein joining the plurality of anisotropic particles comprises at least one of sintering, adhering, alloying, soldering, using a resin or binder on, using shock compression on, or using electrodischarge on the plurality of anisotropic particles.

### Claim 12 (depends on 11)

The method of claim 11, wherein sintering the plurality of anisotropic particles comprises heating the plurality of anisotropic particles at a temperature between about 23° C. and about 200° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein the bulk material comprises a bulk permanent magnet.

### Claim 14 (depends on 9)

The method of claim 9, wherein the iron nitride comprises at least one α″-Fe16N2 phase domain.

### Claim 15 (depends on 9)

The method of claim 9, wherein the anisotropic particle has a shape comprising that of a needle, flake, or lamination.