# US 11,508,924 B2 · Method of formulating perovskite solar cell materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,508,924 B2
- Document ID: US11508924B2
- Status: Granted
- Kind: B2
- Application number: 16/939,907
- Filed: 2020-07-27
- Published: 2020-11-12
- Granted: 2022-11-22
- Earliest claimed: 2014-08-01
- Assignees: CubicPV Inc.
- Applicants: Cubicpv Inc.
- Inventors: Michael D. Irwin; Jerred A. Chute; Vivek V. Dhas
- Web page: https://patentgrep.com/patent/US11508924B2

## CPC

- H10K 71/12: using liquid deposition, e.g. spin coating
- B05D 1/38: with intermediate treatment (intermediate treatment per se B05D3/00)
- B05D 3/107: {Post-treatment of applied coatings}
- H01G 9/2009: {Solid electrolytes}
- H01G 9/2045: {comprising a semiconductor electrode comprising elements of the fourth group of the Periodic Table with or without impurities, e.g. doping materials}
- H03K 5/19: Monitoring patterns of pulse trains (indicating amplitude G01R19/00; indicating frequency G01R23/00; measuring characteristics of individual pulses G01R29/02)
- H03K 5/2472: {using field effect transistors (H03K5/2436 takes precedence)}
- H03K 17/223: {in field-effect transistor switches}
- H10F 77/124: comprising only Group III-V materials, e.g. GaAs
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 85/30: Coordination compounds
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- Y02E 10/542: Dye sensitized solar cells
- Y02E 10/544: Solar cells from Group III-V materials
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H03K: PULSE TECHNIQUE (measuring pulse characteristics G01R; modulating sinusoidal oscillations with pulses H03C; transmission of digital information H04L; discriminator circuits detecting phase difference between two signals by counting or integrating cycles of oscillation H03D3/04; automatic control, starting, synchronisation or stabilisation of generators of electronic oscillations or pulses where the type of generator is irrelevant or unspecified H03L; coding, decoding or code conversion, in general H03M)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing photoactive perovskite materials. The method comprises the step of preparing a germanium halide precursor ink. Preparing a germanium halide precursor ink comprises the steps of: introducing a germanium halide into a vessel, introducing a first solvent to the vessel, and contacting the germanium halide with the first solvent to dissolve the germanium halide. The method further comprises depositing the germanium halide precursor ink onto a substrate, drying the germanium halide precursor ink to form a thin film, annealing the thin film, and rinsing the thin film with a second solvent and a salt.

## Claims

### Claim 1

A method comprising the steps of:
preparing a germanium halide precursor ink, wherein preparing a germanium halide precursor ink comprises the steps of:
introducing a germanium halide into a vessel;
introducing a first solvent to the vessel; and
contacting the germanium halide with the first solvent to dissolve the germanium halide to form the germanium halide precursor ink;
depositing the germanium halide precursor ink onto a substrate;
drying the germanium halide precursor ink to form a thin film;
annealing the thin film; and
rinsing the thin film with a solution comprising:
a second solvent; and
a first salt selected from the group consisting of methylammonium iodide, formamidinium halide, guanidinium halide, 1,2,2-triaminovinylammonium halide, and 5-aminovaleric acid hydrohalide.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first solvent is selected from the group consisting of dry dimethylformamide, dimethylsulfoxide (DMSO), methanol, ethanol, propanol, butanol, tetrahydrofuran, formamide, pyridine, pyrrolidine, chlorobenzene, dichlorobenzene, dichloromethane, chloroform, and combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein contacting the germanium halide with the first solvent to dissolve the germanium halide occurs between about 20° C. to about 150° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein contacting the germanium halide with the first solvent to dissolve the germanium halide occurs at about 85° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein annealing the thin film occurs for between about 5 to about 30 minutes at a temperature between about 40° C. to about 60° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein annealing the thin film occurs for about ten minutes at a temperature of about 50° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second solvent is selected from the group consisting of dimethylformamide, isopropanol, methanol, ethanol, butanol, chloroform, chlorobenzene, dimethylsulfoxide, water, and combinations thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein rinsing the thin film with a solution further comprises:
a second salt selected from the group consisting of methylammonium halide, formamidinium halide, guanidinium halide, 1,2,2-triaminovinylammonium halide, and 5-aminovaleric acid hydrohalide.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first salt comprises formamidinium iodide and the second salt comprises guanidium iodide.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first salt comprises methylammonium iodide and the second salt comprises guanidium iodide.

### Claim 11

A perovskite material prepared by a process comprising the steps of:
preparing a germanium halide precursor ink, wherein preparing a germanium halide precursor ink comprises the steps of:
introducing a germanium halide into a vessel;
introducing a first solvent to the vessel; and
contacting the germanium halide with the first solvent to dissolve the germanium halide;
depositing the germanium halide precursor ink onto a substrate;
drying the germanium halide precursor ink to form a thin film;
annealing the thin film; and
rinsing the thin film, to form the perovskite material, with a solution comprising:
a second solvent; and
a first salt selected from the group consisting of methylammonium iodide, formamidinium halide, guanidinium halide, 1,2,2-triaminovinylammonium halide, and 5-aminovaleric acid hydrohalide.

### Claim 12 (depends on 11)

The perovskite material of claim 11, wherein the first solvent is selected from the group consisting of dry dimethylformamide, dimethylsulfoxide (DMSO), methanol, ethanol, propanol, butanol, tetrahydrofuran, formamide, pyridine, pyrrolidine, chlorobenzene, dichlorobenzene, dichloromethane, chloroform, and combinations thereof.

### Claim 13 (depends on 11)

The perovskite material of claim 11, wherein contacting the germanium halide with the first solvent to dissolve the germanium halide occurs between about 20° C. to about 150° C.

### Claim 14 (depends on 11)

The perovskite material of claim 11, wherein contacting the germanium halide with the first solvent to dissolve the germanium halide occurs at about 85° C.

### Claim 15 (depends on 11)

The perovskite material of claim 11, wherein annealing the thin film occurs for between about 5 to about 30 minutes at a temperature between about 40° C. to about 60° C.

### Claim 16 (depends on 11)

The perovskite material of claim 11, wherein annealing the thin film occurs for about ten minutes at a temperature of about 50° C.

### Claim 17 (depends on 11)

The perovskite material of claim 11, wherein the second solvent is selected from the group consisting of dimethylformamide, isopropanol, methanol, ethanol, butanol, chloroform chlorobenzene, dimethylsulfoxide, water, and combinations thereof.

### Claim 18 (depends on 11)

The perovskite material of claim 11, wherein the solution further comprises:
a second salt selected from the group consisting of methylammonium halide, formamidinium halide, guanidinium halide, 1,2,2-triaminovinylammonium halide, and 5-aminovaleric acid hydrohalide.

### Claim 19 (depends on 18)

The perovskite material of claim 18, wherein the first salt comprises formamidinium iodide and the second salt comprises guanidium iodide.

### Claim 20 (depends on 18)

The perovskite material of claim 18, wherein the first salt comprises methylammonium iodide and the second salt comprises guanidium iodide.