A method for surface treatment of a matte tin-plated product, which is configured for heating the matte tin electroplated on a surface of the product into a bright tin. The method for surface treatment includes heating the surface of the matte tin-plated product with infrared rays.
Claims8
A method for surface treatment of a matte tin-plated product, which is configured for heating the matte tin electroplated already on a surface of the matte tin-plated product into a bright tin, the method for surface treatment comprises heating the surface of the matte tin-plated product with infrared rays,
- wherein the infrared rays are emitted by an infrared radiator and the infrared radiator comprises a plurality of heating zones arranged at intervals, and the method for surface treatment comprises:
- Step S1:
- setting a movement path of the matte tin-plated product according to a position of the infrared radiator, the movement path comprising a waiting position and a heating position;
- Step S2:
- placing the matte tin-plated product at the waiting position, and allowing a side of the matte tin-plated product to be heated to face the infrared radiator;
- and
- Step S3:
- turning on the infrared radiator for preheating, and controlling the matte tin-plated product to sequentially pass through the plurality of heating zones along the movement path to undergo partial heating and then be transported out,
- wherein a width of the matte tin-plated product is 2-10 mm, the infrared radiator comprises a plurality of infrared radiant tubes, and a light-gathering range of each of the plurality of infrared radiant tubes is 1-3 mm,
- wherein the Step S3 further comprises:
- before turning on the infrared radiator for preheating, determining a number of the plurality of infrared radiant tubes to be used according to the width of the matte tin-plated product,
- wherein a distance between the matte tin-plated product and the corresponding infrared radiant tube is 20-80 mm.
Dependencies are inferred from the claim text.