High purity tungsten pentachloride and production method thereof
AssigneeJX Nippon Mining & Metals Corporation
InventorHideyuki Takahashi
Life of this patent
Estimating the term…
Loading patent…
AssigneeJX Nippon Mining & Metals Corporation
InventorHideyuki Takahashi
Estimating the term…
Provided are high purity tungsten pentachloride, and a method for obtaining such high purity tungsten pentachloride at a high yield and in an efficient manner. Tungsten pentachloride in which a total content of metal impurities excluding Sb, Ti, and As is less than 10 wtppm is obtained by uniformly mixing one or more types of reducing agents selected from Sb, Ti, and As and tungsten hexachloride at a molar ratio of 1.0:2.0 to 1.0:5.0 (reducing agent/WCl6 ratio) in an inert atmosphere to obtain a mixture, heating and reducing the mixture for 1 to 100 hours in a temperature range in which a chloride of tungsten and the reducing agent becomes a liquid phase to obtain a reduced product, heating the reduced product for 1 to 100 hours at 100 Pa or less and in a temperature range of 90 to 130° C., and performing reduced-pressure distillation thereto to obtain a reduced-pressure distilled product, heating and sublimating the reduced-pressure distilled product for 1 to 100 hours at 100 Pa or less and in a temperature range of 130 to 170° C., and performing sublimation purification of achieving precipitation at 70 to 120° C.
Tungsten pentachloride, wherein a total content of metal impurities excluding Sb, Ti, and As is less than 10 wtppm, and wherein a content of is 0.2 wtppm or more and 32000 wtppm or less.
Tungsten pentachloride, wherein a total content of metal impurities excluding Sb, Ti and As is less than 10 wtppm, and wherein a content of As is 5000 wtppm or more and 20000 wtppm or less.