# US 11,411,258 B2 · Pulse reverse current high rate electrodeposition and charging while mitigating the adverse effects of dendrite formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,411,258 B2
- Document ID: US11411258B2
- Status: Granted
- Kind: B2
- Application number: 16/560,172
- Filed: 2019-09-04
- Published: 2020-03-05
- Granted: 2022-08-09
- Earliest claimed: 2018-09-05
- Assignees: Faraday Technology Corp.
- Applicants: Faraday Technology, Inc.
- Inventors: Earl Jennings Taylor; Maria E. Inman; Timothy D. Hall; Danny Xin Liu
- Web page: https://patentgrep.com/patent/US11411258B2

## CPC

- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- C25C 1/12: of copper
- C25C 7/06: Operating or servicing
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 10/052: Li-accumulators
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR

## Abstract

The problem of high rate electrodeposition of metals such as copper during electrowinning operations or high rate charging of lithium or zinc electrodes for rechargeable battery applications while avoiding the adverse effects of dendrite formation such as causing short-circuiting and/or poor deposit morphology is solved by pulse reverse current electrodeposition or charging whereby the forward cathodic (electrodeposition or charging) pulse current is “tuned” to minimize dendrite formation for example by creating a smaller pulsating boundary layer and thereby minimizing mass transport effects leading to surface asperities and the subsequent reverse anodic (electropolishing) pulse current is “tuned” to eliminate the micro- and macro-asperities leading to dendrites.

## Claims

### Claim 1

A method of electrowinning a metal, the method comprising:
applying a microprofile charge to the electrowinning cell including:
forward cathodic pulses to deposit metal on the electrowinning anode, and
between selected successive forward cathodic pulses, applying one or more reverse anodic pulses to polish the electrowinning anode; and
subsequent to the application of the microprofile charge to the electrowinning cell, applying a macroprofile charge to the electrowinning cell including:
forward cathodic pulses to deposit metal on the electrowinning anode, and
between selected successful forward cathodic pulses applying one or more reverse anodic pulses to polish the electrowinning anode; and
said microprofile charge and macroprofile charge applied to the electrowinning cell sequentially.

### Claim 2 (depends on 1)

The method of claim 1 in which the microprofile charge includes a cathodic to anodic charge ratio of greater than one, an average current density of greater than 5 mA/cm2, a frequency of between 0.10 to 100 Hz, a cathodic duty cycle of less than 10%, and an anodic duty cycle of greater than 50%.

### Claim 3 (depends on 1)

The method of claim 1 where in the macroprofile charge includes a cathodic to anodic charge ratio of greater than 1, an average current density of greater than 5 mA/cm2, a frequency of 0.102 100 Hz, a cathodic duty cycle of greater than 50%, and anodic duty cycle of less than 10%.