Method to produce a fibrous product comprising microfibrillated cellulose
AssigneeStora Enso OYJ
InventorsKaj Backfolk, Isto Heiskanen, Esa Saukkonen, Katja Lyytikäinen
Life of this patent
Estimating the term…
Loading patent…
AssigneeStora Enso OYJ
InventorsKaj Backfolk, Isto Heiskanen, Esa Saukkonen, Katja Lyytikäinen
Estimating the term…
A method for the production of a fibrous product from a fibrous web, wherein the method comprises the steps of: —providing a fibrous suspension comprising a microfibrillated cellulose, wherein the content of the microfibrillated cellulose of said suspension is in the range of 60 to 99.9 weight-% based on total dry solid content, —adding an uncharged, amphoteric or weakly cationic polymer having a molecular weight of at least 50000 g/mol to said suspension, —adding an anionic polymer having a molecular weight of at least 00000 g/mol to said suspension to provide a mixture of said microfibrillated cellulose, said uncharged, amphoteric or weakly cationic polymer and said anionic polymer, 1—providing said mixture to a substrate to form a fibrous web, wherein the amount of uncharged, amphoteric or weakly cationic polymer in said mixture is in the range of 0.1 to 20 kg/metric ton based on total dry solid content and wherein the amount of anionic polymer in said mixture is in the range of 0.01 to 10 kg/metric ton based on total dry 20 solid content; and—dewatering said fibrous web to form a fibrous product.
A method for the production of a fibrous product from a fibrous suspension, wherein the method comprises the steps of:
Dependencies are inferred from the claim text.