# US 11,305,363 B2 · Repair of through-hole damage using braze sintered preform

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,305,363 B2
- Document ID: US11305363B2
- Status: Granted
- Kind: B2
- Application number: 16/272,664
- Filed: 2019-02-11
- Published: 2020-08-13
- Granted: 2022-04-19
- Earliest claimed: 2019-02-11
- Assignees: ROLLS-ROYCE plc
- Applicants: Rolls-Royce Corporation
- Inventors: Raymond Ruiwen Xu; Scott Nelson; Joseph Peter Henderkott
- Web page: https://patentgrep.com/patent/US11305363B2

## CPC

- B23K 1/0008: {specially adapted for particular articles or work}
- B23K 1/0018: {Brazing of turbine parts}
- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- B23K 35/0244: {Powders, particles or spheres; Preforms made therefrom}
- B23K 35/3033: {Ni as the principal constituent}
- B23K 35/3046: {Co as the principal constituent}
- B23P 6/002: {Repairing turbine components, e.g. moving or stationary blades, rotors, (B23P6/045 takes precedence)}
- B23P 6/045: {of turbine components, e.g. moving or stationary blades, rotors, etc.}
- C21D 9/50: for welded joints
- F01D 5/005: {Repairing methods or devices}
- F01D 25/005: {Selecting particular materials}
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- B23K 2101/001: {Turbines}
- B23P 6/005: {using only replacement pieces of a particular form}
- C23C 4/073: containing MCrAl or MCrAlY alloys, where M is nickel, cobalt or iron, with or without non-metal elements
- F05D 2230/22: by sintering
- F05D 2230/237: Brazing
- F05D 2230/40: Heat treatment
- F05D 2300/171: Steel alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A method may include removing a portion of a base component adjacent to a damaged portion of the base component to define a repair portion of the base component. The base component may include a cobalt- or nickel-based superalloy, and the repair portion of the base component may include a through-hole extending from a first surface of the base component to a second surface of the base component. The method also may include forming a braze sintered preform to substantially reproduce a shape of the through-hole. The braze sintered preform may include a Ni- or Co-based alloy. The method additionally may include placing the braze sintered preform in the through-hole and heating at least the braze sintered preform to cause the braze sintered preform to join to the repair portion of the base component and change a microstructure of the braze sintered preform to a brazed and diffused microstructure.

## Claims

### Claim 1

A method comprising:
removing a portion of a base component adjacent to a damaged portion of the base component to define a repair portion of the base component, wherein the base component comprises a cobalt- or nickel-based superalloy, and wherein the repair portion of the base component comprises a through-hole extending from a first surface of the base component to a second surface of the base component;
forming a braze sintered preform to substantially reproduce a shape of the through-hole, wherein the braze sintered preform comprises a Ni- or Co-based alloy;
placing the braze sintered preform in the through-hole;
positioning additional braze material comprising the Ni- or Co- based alloy adjacent to the braze sintered preform to cover parts of adjacent damage that the braze sintered preform does not fill, wherein:
the additional braze material comprises a braze paste, and wherein the additional braze material fills cracks adjacent to the through-hole; or
the additional braze material comprises a second braze sintered preform, wherein the second braze sintered preform comprises a sheet, and wherein the sheet overlies the braze sintered preform and at least part of the repair portion of the base component and
heating at least the braze sintered preform and the additional braze material to cause the braze sintered preform to join to the repair portion of the base component and change a microstructure of the braze sintered preform and the additional braze material to a brazed and diffused microstructure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the additional braze material comprises a composition substantially similar to the braze sintered preform.

### Claim 3 (depends on 1)

The method of claim 1, further comprising placing braze stop-off material adjacent to the additional braze material to maintain the additional braze material at desired locations of the base component.

### Claim 4 (depends on 1)

The method of claim 1, wherein the braze sintered preform substantially fills a depth of the through-hole.

### Claim 5 (depends on 1)

The method of claim 1, wherein the braze sintered preform comprises three-dimensional surface features on a first side of the braze sintered preform, wherein the first side of the braze sintered preform in positioned adjacent the second side of the base component, and wherein the three-dimensional features substantially reproduce three-dimensional features of the damaged portion of the base component.

### Claim 6 (depends on 1)

The method of claim 1, further comprising spot welding the braze sintered preform in place relative to the base component prior to heating at least the braze sintered preform and the additional braze material.

### Claim 7 (depends on 1)

The method of claim 1, wherein the braze sintered preform comprises a substantially homogeneous mixture of a high melt Ni- or Co-based superalloy powder and a low melt braze powder.

### Claim 8 (depends on 1)

The method of claim 1, wherein the braze sintered preform comprises between 0.05 and 0.116 wt. % carbon, between 0.11 and 0.376 wt. % silicon, between 8.424 wt. % and 11.640 wt. % chromium, between 0.284 wt. % and 0.835 wt. % boron, between 4.8 wt. % and 5.8 wt. % aluminum, between 2.675 wt. % and 4.232 wt. % tungsten, between 0.650 wt. % and 1.362 wt. % molybdenum, between 1.4 wt. % and 2.462 wt. % rhenium, between 7.184 wt. % and 8.942 wt. % tantalum, between 0.690 wt. % and 1.386 wt. % hafnium, and between 8.725 wt. % and 10.964 wt. % cobalt, and nickel.

### Claim 9 (depends on 7)

The method of claim 7, wherein the braze sintered preform comprises a maximum of 0.082 wt. % manganese, a maximum of 0.003 wt. % sulfur, a maximum of 0.013 wt. % phosphorus, a maximum of 0.018 wt. % titanium, a maximum of 0.161 wt. % yttrium, a maximum of 0.034 wt. % zirconium, a maximum of 0.180 wt. % iron, a maximum of 0.093 wt. % vanadium, a maximum of 0.10 wt. % copper, a maximum of 0.007 wt. % magnesium, a maximum of 0.084 wt. % oxygen, a maximum of 0.030 wt. % nitrogen, a maximum of 0.242 wt. % platinum, and a maximum of 0.150 wt. % other elements.

### Claim 10 (depends on 8)

The method of claim 8, wherein the braze sintered preform comprises about 0.3 wt. % silicon, about 11.4 wt. % chromium, about 0.8 wt. % boron, about 4.9 wt. % aluminum, about 2.8 wt. % tungsten, about 0.8 wt. % molybdenum, about 1.5 wt. % rhenium, about 52 wt. % nickel, about 0.2 wt. % niobium, about 8.8 wt. % tantalum, about 0.8 wt. % hafnium, and about 9 wt. % Co.

### Claim 11 (depends on 8)

The method of claim 8, wherein the braze sintered preform comprises about 0.3 wt. % silicon, about 10.2 wt. % chromium, about 0.6 wt. % boron, about 5.2 wt. % aluminum, about 3.3 wt. % tungsten, about 0.9 wt. % molybdenum, about 1.8 wt. % rhenium, about 52.1 wt. % nickel, about 0.2 wt. % niobium, about 8.1 wt. % tantalum, about 1.0 wt. % hafnium, and about 9.6 wt. % Co.

### Claim 12 (depends on 8)

The method of claim 8, wherein the braze sintered preform comprises about 0.2 wt. % silicon, about 8.6 wt. % chromium, about 0.3 wt. % boron, about 5.7 wt. % aluminum, about 4.1 wt. % tungsten, about 1.2 wt. % molybdenum, about 2.3 wt. % rhenium, about 52.2 wt. % nickel, about 0.1 wt. % niobium, about 7.3 wt. % tantalum, about 1.2 wt. % hafnium, and about 10.7 wt. % Co.

### Claim 13 (depends on 1)

The method of claim 1, wherein heating at least the braze sintered preform and the additional braze material comprises heating at least the braze sintered preform in a vacuum furnace at a temperature between about 1093° C. and about 1260° C.

### Claim 14 (depends on 1)

The method of claim 1, further comprising subjecting at least the braze sintered preform and the additional braze material to a diffusion heat treatment cycle in a vacuum furnace back filled with argon gas at a pressure between 100 to 800 microns Hg at a temperature between about 1038° C. and about 1149° C. for at least 17 hours.

### Claim 15 (depends on 1)

The method of claim 1, further comprising, after heating at least the braze sintered preform and the additional braze material to cause the braze sintered preform and the additional braze material to join to the repair portion of the base component, machining at least the braze sintered preform and the additional braze material to remove excess braze sintered preform material and the additional braze material and restore the base component to a nominal part geometry.