Abstract
A technique comprising: producing an unencapsulated stack of layers defining one or more electronic devices including an organic semiconductor element; and then subjecting the unencapsulated stack of layers to a water removal treatment in a vacuum oven in the presence of an external water adsorbent; wherein the water removal treatment comprises heating the unencapsulated stack of layers in the vacuum oven for a time period longer than a control time period at which a spike in oven pressure attributable to the release of water from the stack of layers would occur with heating under the same treatment conditions but without the water absorbing material.
Claims13
A method comprising:
- producing an unencapsulated stack of layers defining one or more electronic devices including an organic semiconductor element;
- and then subjecting the unencapsulated stack of layers to a water removal treatment in a vacuum oven in the presence of an external water adsorbent;
- wherein the water removal treatment comprises heating the unencapsulated stack of layers in the vacuum oven for a time period longer than a control time period at which a spike in oven pressure attributable to the release of water from the stack of layers would occur with heating under the same treatment conditions but without the water absorbing material.
A method comprising:
- producing an unencapsulated stack of layers defining one or more transistor devices including an organic semiconductor channel;
- and then subjecting the unencapsulated stack of layers to a water removal treatment in a vacuum oven;
- wherein the water removal treatment comprises heating the unencapsulated stack of layers in the vacuum oven in the presence of a water adsorbent for a time sufficient to remove water to an extent that the one or more transistor devices exhibit, after encapsulation of the stack, a variation in gate voltage of less than 6% in a stress test in air involving maintaining the gate voltage at a level required to achieve a current of 2.5 μA through the organic semiconductor channel for 60 hours.
A method comprising:
- producing an unencapsulated stack of layers defining one or more transistor devices including an organic semiconductor channel;
- and then subjecting the unencapsulated stack of layers to a water removal treatment in a vacuum oven;
- wherein the water removal treatment comprises heating the unencapsulated stack of layers in the vacuum oven in the presence of a water adsorbent for a time sufficient to remove water to an extent that the one or more transistor devices exhibit, after encapsulation of the stack, a variation in forward current through the organic semiconductor channel of less than about 5% in a stress test involving operating the one or more transistor devices at a fixed gate voltage and a fixed source-drain voltage for 90 hours in air at 60° C.