# US 11,121,423 B2 · Alkaline metal-air battery cathode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,423 B2
- Document ID: US11121423B2
- Status: Granted
- Kind: B2
- Application number: 16/174,648
- Filed: 2018-10-30
- Published: 2019-02-28
- Granted: 2021-09-14
- Earliest claimed: 2012-04-11
- Assignees: Ionic Materials, Inc.
- Applicants: Ionic Materials, Inc.
- Inventors: Michael A. Zimmerman; Alexei B. Gavrilov; G. Stephen Kelsey; Keith Smith
- Web page: https://patentgrep.com/patent/US11121423B2

## CPC

- H01M 12/06: with one metallic and one gaseous electrode
- H01M 4/50: of manganese
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/624: {Electric conductive fillers}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

A metal-air battery and a component air cathode including a solid ionically conductive polymer material.

## Claims

### Claim 1

A metal-air battery comprising:
an air electrode that includes: an electrically conductive material, and a solid ionically conducting polymer material;
wherein the air electrode acts to produce an hydroxide ion when the air electrode is exposed to an oxygen gas source and when the battery is under load;
wherein the solid ionically conducting polymer material ionically conducts the hydroxide ion;
wherein the solid ionically conducting polymer material is ionically conductive through the solid and not through any solvent, gel or liquid phase;
wherein the solid ionically conducting polymer material has an ionic conductivity greater than 1×10−5 S/cm at room temperature;
wherein the solid ionically conducting polymer material has an electronic conductivity of less than 1×10−5 S/cm at room temperature; and
wherein the solid ionically conducting polymer material has a glassy state, and wherein the solid ionically conducting polymer material conducts the hydroxide ion in the glassy state.

### Claim 2 (depends on 1)

The battery of claim 1, further comprising a negative electrode including a first electrochemically active metal; and an ionically conducting, dielectric material interposed between the air electrode and the negative electrode and in contact with the air electrode.

### Claim 3 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material comprises a cationic diffusing ion, wherein the diffusivity of the cationic diffusing ion is greater than 1.0×10−12 m2/S at room temperature.

### Claim 4 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material comprises an anionic diffusing ion comprising the hydroxide ion, wherein the diffusivity of the anionic diffusing ion is greater than 1.0×10−12 m2/S at room temperature.

### Claim 5 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material comprises both an anionic diffusing ion comprising the hydroxide ion and a cationic diffusing ion, wherein each at least one cationic and anionic diffusing ion have a diffusivity, wherein the anionic diffusivity is greater than the cationic diffusivity at room temperature.

### Claim 6 (depends on 1)

The battery of claim 1, wherein the cationic transference number of the solid ionically conducting polymer material is greater than 0.5 and less than 1.0 at room temperature.

### Claim 7 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material comprises lithium.

### Claim 8 (depends on 7)

The battery of claim 7, wherein the concentration of lithium is greater than 3 moles of lithium per liter of solid ionically conducting polymer material.

### Claim 9 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material has an ionic conductivity greater than 1×10−4 S/cm at room temperature.

### Claim 10 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material has an ionic conductivity greater than 1×10−3 S/cm at 80° C.

### Claim 11 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material has an ionic conductivity greater than 1×10−5 S/cm at 40° C.

### Claim 12 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material comprises both an anionic diffusing comprising the hydroxide ion and a cationic diffusing ion, wherein the cationic diffusing ion comprises lithium, and wherein the diffusivity of lithium ion and the hydroxide ion are both greater than 1.0×10−13 m2/s at room temperature.

### Claim 13 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material exhibits UL 94 V-0 flame retardancy.

### Claim 14 (depends on 1)

The battery of claim 1, wherein the solid ionically conducting polymer material is formed from the reaction product of a base polymer, electron acceptor and an ionic compound.

### Claim 15 (depends on 14)

The battery of claim 14, wherein the base polymer is polyphenylene sulfide (PPS) or a liquid crystal polymer.

### Claim 16 (depends on 1)

The battery of claim 1, wherein the air electrode further comprises a metal oxide.

### Claim 17 (depends on 16)

The battery of claim 16, wherein the metal oxide is manganese dioxide.

### Claim 18 (depends on 1)

The battery of claim 1 wherein the air electrode further comprises manganese dioxide, and the manganese dioxide is selected from a group comprising β-MnO2 (pyrolusite), ramsdellite, γ-MnO2, ε-MnO2, λ-MnO2, EMD, CMD, and combinations thereof.

### Claim 19 (depends on 2)

The battery of claim 2, wherein the first electrochemically active metal comprises zinc, aluminum, calcium, magnesium, potassium, sodium or lithium.