# US 11,121,382 B2 · Solid oxide fuel cell stacks having a barrier layer and associated methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,382 B2
- Document ID: US11121382B2
- Status: Granted
- Kind: B2
- Application number: 15/863,995
- Filed: 2018-01-08
- Published: 2019-07-11
- Granted: 2021-09-14
- Earliest claimed: 2018-01-08
- Assignees: Cummins Enterprise LLC
- Applicants: Cummins Enterprise LLC
- Inventors: Todd Michael Striker; Matthew Joseph Alinger; Simon William Gaunt; Nicole Virginia Gonyeau
- Web page: https://patentgrep.com/patent/US11121382B2

## CPC

- H01M 8/0228: in the form of layered or coated products
- C03C 27/044: {of glass, glass-ceramic or ceramic material only}
- C23C 4/12: characterised by the method of spraying
- H01M 8/0206: Metals or alloys
- H01M 8/0271: Sealing or supporting means around electrodes, matrices or membranes
- H01M 8/0273: with sealing or supporting means in the form of a frame
- H01M 8/0282: Inorganic material
- H01M 8/1246: the electrolyte consisting of oxides
- H01M 8/2425: High-temperature cells with solid electrolytes
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid oxide fuel cell stack having a metallic layer and a glass layer, and a method for preventing or reducing a chemical reaction between the metallic layer and the glass layer are disclosed. The solid oxide fuel cell stack has a barrier layer disposed between the metallic layer and the glass layer. The barrier layer includes alumina and a phosphate. The phosphate includes an aluminum dihydrogen phosphate, an aluminum-containing phosphate, a phosphate of an element of the metallic layer, a phosphate of an element of the glass layer, or combinations thereof. The method includes disposing a barrier layer between the metallic layer and the glass layer.

## Claims

### Claim 1

A solid oxide fuel cell stack comprising:
a metallic interconnect of a solid oxide fuel cell;
a glass seal of the solid oxide fuel cell; and
a barrier layer disposed directly between and adjacent to both the metallic interconnect and the glass seal,
wherein the barrier layer comprises alumina and a total phosphate, and
the total phosphate of the barrier layer comprises one or more of an aluminum dihydrogen phosphate, an aluminum-containing phosphate, a phosphate of an element of the metal interconnect, a phosphate of an element of the glass seal, or combinations thereof,
wherein the barrier layer further comprises a first sublayer, a second sublayer, and a third sublayer disposed between the first sublayer and the second sublayer, and
the first sublayer comprises the phosphate of an element of the metallic interconnect; the second sublayer comprises the phosphate of an element of the glass seal; and the third sublayer comprises alumina and the aluminum-containing phosphate.

### Claim 2 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the total phosphate in the barrier layer is in a range from about 1 mol % to about 75 mol % of the barrier layer.

### Claim 3 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the total phosphate comprises the aluminum dihydrogen phosphate, and wherein the aluminum dihydrogen phosphate is present in the barrier layer in a range from about 1 mol % to about 45 mol % of the barrier layer.

### Claim 4 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the total phosphate comprises the aluminum-containing phosphate, and wherein the aluminum-containing phosphate is present in the barrier layer in a range from about 3 mol % to about 60 mol % of the barrier layer.

### Claim 5 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the phosphate of an element of the metallic interconnect comprises a chromium phosphate, an iron phosphate, a silicon phosphate, a titanium phosphate, a manganese phosphate, a nickel phosphate, or combinations thereof.

### Claim 6 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the phosphate of an element of the glass seal comprises a barium phosphate, a silicon phosphate, a boron phosphate, a zirconium phosphate, a calcium phosphate, a magnesium phosphate, an yttrium phosphate, a zinc phosphate, or combinations thereof.

### Claim 7 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the first sublayer comprises a chromium phosphate, an iron phosphate, a silicon phosphate, a manganese phosphate, a titanium phosphate, nickel phosphate or combinations thereof; the second sublayer comprises a barium phosphate, a silicon phosphate, a boron phosphate, a zirconium phosphate, a calcium phosphate, a magnesium phosphate, an yttrium phosphate, a zinc phosphate, or combinations thereof.

### Claim 8 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein a mol % of the phosphate of the element of the metallic interconnect present in the first sublayer is greater than a mol % of the aluminum-containing phosphate present in the third sublayer.

### Claim 9 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein a thickness of the third sublayer is greater than 5 microns.

### Claim 10 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the metallic interconnect is substantially free of aluminum.

### Claim 11 (depends on 1)

A method of fabricating the solid oxide fuel cell stack of claim 1, the method comprising:
stacking at least two adjacent solid oxide fuel cells, each solid oxide fuel cell of the at least two adjacent solid oxide fuel cells supported on the metallic interconnect and comprising an anode, a cathode, and an electrolyte;
disposing the glass seal between the electrolyte of at least one solid oxide fuel cell of the at least two adjacent solid oxide fuel cells and the metallic interconnect supporting the adjacent solid oxide fuel cell;
disposing a layer comprising alumina and aluminum dihydrogen phosphate directly between and adjacent to both the metallic interconnect and the glass seal to form a disposed barrier layer,
heating the disposed barrier layer to a temperature greater than 300° C. to form an intermediate barrier layer comprising the aluminum-containing phosphate,
heating the intermediate barrier layer to a temperature greater than 500° C.,
reacting the aluminum-containing phosphate and chromium of the metallic interconnect to form the first sublayer, and
reacting the aluminum-containing phosphate and barium of the glass seal to form the second sublayer,
wherein the third sublayer is present as a barrier between the first sublayer and the second sublayer.

### Claim 12 (depends on 11)

The method of claim 11, wherein heating the disposed barrier layer to a temperature greater than 300° C. comprises partially reacting the aluminum dihydrogen phosphate and the alumina to form the intermediate barrier layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein heating the intermediate barrier layer to a temperature greater than 500° C. forms a reacted barrier layer.

### Claim 14 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the element of the metallic interconnect is chromium.

### Claim 15 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the element of the glass seal is barium.

### Claim 16 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the element of the glass seal is barium and the element of the metallic interconnect is chromium.

### Claim 17 (depends on 1)

The solid oxide fuel cell stack of claim 1, wherein the third sublayer is present as a barrier that prevents or reduces a reaction between chromium of the metallic interconnect an barium of the glass.

### Claim 18 (depends on 17)

The solid oxide fuel cell stack of claim 17, wherein the third sublayer prevents or reduces the formation of barium chromate.