# US 11,121,377 B2 · Ionic-electronic conductive material, method of manufacturing same, and lithium-air battery comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,377 B2
- Document ID: US11121377B2
- Status: Granted
- Kind: B2
- Application number: 16/217,595
- Filed: 2018-12-12
- Published: 2020-06-18
- Granted: 2021-09-14
- Earliest claimed: 2018-12-12
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Dong-Hwa Seo; Sang Bok Ma; Hyuk Jae Kwon; Hyunpyo Lee; Dongmin Im
- Web page: https://patentgrep.com/patent/US11121377B2

## CPC

- H01M 4/8673: {Electrically conductive fillers}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/9016: {Oxides, hydroxides or oxygenated metallic salts}
- H01M 12/02: Details (of electrodes H01M4/00; of non-active parts H01M50/00)
- H01M 12/08: composed of a half-cell of a fuel-cell type and a half-cell of the secondary-cell type
- H01M 2004/8689: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An ionic-electronic conductive compound of Formula 1: LixA(1-x-y)MzM′(1-z)O3 (1) wherein, 0<x≤0.5, 0≤y≤0.5, 0≤z≤0.5, A comprises Mg, Ca, Sr, Ba, or a combination thereof, M and M′ each independently comprise As, Sb, Bi, or a combination thereof.

## Claims

### Claim 1

A positive electrode for a lithium-air battery, the positive electrode comprising:
an ionic-electronic conductive compound of Formula 1:
LixA(1-x-y)MzM′(1-z)O3 (1)
wherein,
0<x≤0.5, 0.1≤y≤0.25, 0≤z≤0.5,
A comprises Mg, Ca, Sr, Ba, or a combination thereof,
M and M′ each independently comprise As, Sb, Bi, or a combination thereof,
wherein y is a vacancy content on an A site of the compound,
wherein the compound has an electronic conductivity of greater than 2×10−8 Siemens per centimeter at 20° C., and
an ionic conductivity of greater than 5×10−8 Siemens per centimeter at 20° C.

### Claim 2 (depends on 1)

The positive electrode of claim 1, wherein in Formula 1, 0.1≤x≤0.25.

### Claim 3 (depends on 1)

The positive electrode of claim 1, wherein in Formula 1, A is Ba.

### Claim 4 (depends on 1)

The positive electrode of claim 1, wherein the compound has a perovskite-type structure.

### Claim 5 (depends on 1)

The positive electrode of claim 1, wherein the ionic-electronic conductive compound has an electronic conductivity of 2×10−8 to 2×10−6 Siemens per centimeter at 20° C., and having an ionic conductivity of 3×10−8 to 3×10−6 Siemens per centimeter at 20° C.

### Claim 6 (depends on 1)

The positive electrode of claim 1, wherein the ionic-electronic conductive compound has an electronic conductivity of 8×10−8 to 1×10−5 Siemens per centimeter at 60° C.

### Claim 7 (depends on 1)

The positive electrode of claim 1, wherein the ionic-electronic conductive compound has diffraction peaks at 29.0°, 41.5°, and 51.2° 2θ, when analyzed by X-ray powder diffraction using CuKα radiation.

### Claim 8 (depends on 1)

A lithium-air battery comprising:
a negative electrode;
a separator; and
the positive electrode of claim 1.

### Claim 9

A method of manufacturing a positive electrode for a lithium-air battery, the method comprising:
contacting
a compound comprising Li,
a compound comprising Mg, Ca, Sr, Ba, or a combination thereof, and
a compound comprising As, Sb, Bi, or a combination thereof to form a mixture; and
heat-treating the mixture to form an ionic-electronic conductive compound of Formula 1
LixA(1-x-y)MzM′(1-z)O3 (1)
wherein,
0<x≤0.5, 0.1≤y≤0.25, 0≤z≤0.5,
A comprises Mg, Ca, Sr, Ba, or a combination thereof,
M and M′ each independently comprise As, Sb, Bi, or a combination thereof,
wherein y is a vacancy content on an A site of the compound,
wherein the compound has an electronic conductivity of greater than 2×10−8 Siemens per centimeter at 20° C., and
an ionic conductivity of greater than 5×10−8 Siemens per centimeter at 20° C. to manufacture the positive electrode.

### Claim 10 (depends on 9)

The method of claim 9, wherein the heat-treating is at a temperature of less than 800° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the heat-treating is at a temperature of 600° C. to 800° C.

### Claim 12 (depends on 11)

The method of claim 11, wherein the heat-treating comprises
calcining at a temperature of 650° C. to 750° C., and
sintering at a temperature of 600° C. to 800° C.

### Claim 13 (depends on 1)

The positive electrode of claim 1, further comprising a separator, wherein the ionic-electronic conductive compound is on the separator.

### Claim 14 (depends on 1)

The positive electrode of claim 1, further comprising a gas diffusion layer, wherein the ionic-electronic conductive compound is on the gas diffusion layer.

### Claim 15 (depends on 1)

The positive electrode of claim 1, further comprising a gas diffusion layer, wherein the ionic-electronic conductive compound is between the separator and the gas diffusion layer.

### Claim 16 (depends on 1)

The positive electrode of claim 1, further comprising Li2O2 on the positive electrode.

### Claim 17 (depends on 9)

The method of claim 9, further comprising disposing the ionic-electronic conductive compound on a gas diffusion layer on a separator.