# US 11,121,376 B2 · Positive electrode, non-aqueous electrolyte secondary battery, and method of producing positive electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,376 B2
- Document ID: US11121376B2
- Status: Granted
- Kind: B2
- Application number: 16/381,256
- Filed: 2019-04-11
- Published: 2019-10-17
- Granted: 2021-09-14
- Earliest claimed: 2018-04-13
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Koji Torita; Akihiro Ochiai; Yusuke Fukumoto; Harunari Shimamura; Takuya Asari
- Web page: https://patentgrep.com/patent/US11121376B2

## CPC

- H01M 4/664: {Ceramic materials}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode includes at least a positive electrode current collector and a positive electrode active material layer. The positive electrode current collector includes an aluminum foil and an aluminum hydrated oxide film. The aluminum hydrated oxide film covers a surface of the aluminum foil. The positive electrode active material layer is formed on a surface of the aluminum hydrated oxide film. The aluminum hydrated oxide film has a thickness not smaller than 50 nm and not greater than 1000 nm. The aluminum hydrated oxide film contains at least one selected from the group consisting of phosphorus, fluorine, and sulfur.

## Claims

### Claim 1

A positive electrode for a non-aqueous electrolyte secondary battery, the positive electrode comprising at least:
a positive electrode current collector; and
a positive electrode active material layer,
the positive electrode current collector comprising an aluminum foil and an aluminum hydrated oxide film,
the aluminum hydrated oxide film covering a surface of the aluminum foil,
the positive electrode active material layer being formed on a surface of the aluminum hydrated oxide film,
the aluminum hydrated oxide film having a thickness not smaller than 50 nm and not greater than 1000 nm,
the aluminum hydrated oxide film containing at least one selected from the group consisting of phosphorus, fluorine, and sulfur,
wherein a ratio of a total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to a sum of a total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.05 mass % and not greater than 30 mass %.

### Claim 2 (depends on 1)

The positive electrode according to claim 1, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass %.

### Claim 3 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film has a thickness not smaller than 100 nm.

### Claim 4 (depends on 1)

A non-aqueous electrolyte secondary battery comprising at least the positive electrode according to claim 1 and a negative electrode.

### Claim 5 (depends on 1)

A method of producing positive the positive electrode according to claim 1, the method comprising at least:
preparing the aluminum foil;
forming the aluminum hydrated oxide film on the surface of the aluminum foil by heating the aluminum foil in an aqueous solution to produce the positive electrode current collector; and
forming the positive electrode active material layer on the surface of the aluminum hydrated oxide film to produce the positive electrode,
the aqueous solution containing at least one selected from the group consisting of the phosphorus compound, the fluorine compound, and the sulfur compound dissolved in the aqueous solution.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 20 mass %.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 10 mass %.

### Claim 8 (depends on 5)

The method according to claim 5, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 5 mass %.

### Claim 9 (depends on 5)

The method according to claim 5, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 1 mass % and not greater than 5 mass %.

### Claim 10 (depends on 1)

The positive electrode according to claim 1, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 20 mass %.

### Claim 11 (depends on 1)

The positive electrode according to claim 1, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 10 mass %.

### Claim 12 (depends on 1)

The positive electrode according to claim 1, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 0.1 mass % and not greater than 5 mass %.

### Claim 13 (depends on 1)

The positive electrode according to claim 1, wherein the ratio of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film to the sum of the total mass of the at least one selected from the group consisting of phosphorus, fluorine, and sulfur contained in the aluminum hydrated oxide film and the mass of aluminum contained in the aluminum hydrated oxide film is not lower than 1 mass % and not greater than 5 mass %.

### Claim 14 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film consists of aluminum hydrated oxide and at least one selected from the group consisting of aluminum phosphate, aluminum fluoride, and aluminum sulfate.

### Claim 15 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains aluminum hydrated oxide and at least two selected from the group consisting of aluminum phosphate, aluminum fluoride, and aluminum sulfate.

### Claim 16 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains aluminum hydrated oxide, aluminum phosphate, aluminum fluoride, and aluminum sulfate.

### Claim 17 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains at least two selected from the group consisting of phosphorus, fluorine, and sulfur.

### Claim 18 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains phosphorus, fluorine, and sulfur.

### Claim 19 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains aluminum hydrated oxide in an amount not lower than 70 mass %.

### Claim 20 (depends on 1)

The positive electrode according to claim 1, wherein the aluminum hydrated oxide film contains aluminum hydrated oxide in an amount not lower than 80 mass %.