# US 11,121,369 B2 · Positive electrode plate, method for preparing the same and lithium-ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,369 B2
- Document ID: US11121369B2
- Status: Granted
- Kind: B2
- Application number: 17/051,462
- Filed: 2019-08-29
- Published: 2021-05-27
- Granted: 2021-09-14
- Earliest claimed: 2018-08-31
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Zhiqiang Li; Changlong Han; Qifeng Li
- Web page: https://patentgrep.com/patent/US11121369B2

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application discloses a positive electrode plate, a preparation method thereof, and a lithium-ion secondary battery, wherein the positive electrode plate includes a positive electrode current collector and a positive electrode film disposed on at least one surface of the positive electrode current collector, wherein the positive electrode film includes a positive active material which is a lithium manganese-based positive active material; and wherein the volume resistivity ρsum of the positive electrode plate, the powder volume resistivity ρ of the positive active material under a pressure of 20 MPa and the mass percentage a of the positive active material in the positive electrode film satisfy ρsum/ρ97.5-a≤3. The positive electrode plate provided in the present application enables the lithium-ion secondary battery to simultaneously have higher safety performance, rate performance and cycle performance.

## Claims

### Claim 1

A positive electrode plate, including a positive electrode current collector and a positive electrode film disposed on at least one surface of the positive electrode current collector, wherein the positive electrode film includes a positive active material which is a lithium manganese-based positive active material,
wherein the positive electrode plate satisfies formula (1),
ρ
sum
ρ
97.5
⁢
-
⁢
a
≤
3
formula
⁢
⁢
(
1
)
in which psum is volume resistivity of the positive electrode plate, in kΩ·cm; ρ is powder volume resistivity of the positive active material under a pressure of 20 MPa, in kΩ·cm; a is mass percentage of the positive active material in the positive electrode film, in wt %.

### Claim 2 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive electrode plate satisfies formula (2),
10
-
10
≤
ρ
sum
ρ
97.5
⁢
-
⁢
a
≤
3.
formula
⁢
⁢
(
2
)

### Claim 3 (depends on 1)

The positive electrode plate according to claim 1, wherein positive electrode plate has a volume resistivity ρsum≤450 kΩ·cm.

### Claim 4 (depends on 1)

The positive electrode plate according to claim 1, wherein positive electrode plate has a volume resistivity ρsum≤300 kΩ·cm.

### Claim 5 (depends on 1)

The positive electrode plate according to claim 1, wherein positive electrode plate has a volume resistivity ρsum<160 kΩ·cm.

### Claim 6 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive active material has a powder volume resistivity ρ under a pressure of 20 MPa between 0 to 450 kΩ·cm.

### Claim 7 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive active material has a powder volume resistivity ρ under a pressure of 20 MPa between 0 to 400 kΩ·cm.

### Claim 8 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive active material is present in a mass percentage from 80 wt % to 96.5 wt % in the positive electrode film.

### Claim 9 (depends on 1)

The positive electrode plate according to claim 1, wherein the lithium manganese-based positive active material includes a first lithium manganese-based positive active material according to formula (3) and a second lithium manganese-based positive active material according to formula (4),
Li1+xMnaNibM1-a-bO2-yAy formula (3)
Li1+zMneN2-eO4-dBd formula (4)
where in the formula (3), −0.1x0.2, 0<a<1, 0b<1, 0<a+b<1, 0y<0.2, and M includes one or more of Co, Fe, Cr, Ti, Zn, V, Al, Zr and Ce, A includes one or more of S, N, F, Cl, Br and I; and
in the formula (4), −0.1z0.2, 0<e2, 0d<1, and N includes one or more of Ni, Fe, Cr, Ti, Zn, V, Al, Mg, Zr and Ce, B includes one or more of S, N, F, Cl, Br and I.

### Claim 10 (depends on 1)

The positive electrode plate according to claim 1, wherein the mass percentage ω of Mn in the positive active material and the powder volume resistivity ρ of the positive active material under a pressure of 20 MPa satisfy the following relationship: 3≤ω·ρ/100≤200.

### Claim 11 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive active material has an average particle diameter Dv50 from 1 μm to 20 μm, and the positive active material has a BET specific surface area from 0.3 m2/g to 1.5 m2/g.

### Claim 12 (depends on 1)

The positive electrode plate according to claim 1, wherein the positive electrode plate has a packing density from 3.1 g/cm3 to 3.65 g/cm3.

### Claim 13 (depends on 1)

A lithium-ion secondary battery including a positive electrode plate, a negative electrode plate, a separator and an electrolyte, wherein the positive electrode plate is the positive electrode plate according to claim 1.

### Claim 14

A method for preparing a positive electrode plate, comprising:
mixing a first lithium manganese-based positive active material, a conductive agent, a binder, and a solvent to obtain a pre-slurry;
mixing a second lithium manganese-based positive active material with the pre-slurry to obtain a positive electrode slurry;
coating the positive electrode slurry on at least one surface of a positive electrode current collector to form a positive electrode film, thereby obtaining a positive electrode plate, wherein the positive electrode plate satisfies formula (1),
ρ
sum
ρ
97.5
⁢
-
⁢
a
≤
3
formula
⁢
⁢
(
1
)
in which ρsum is volume resistivity of the positive electrode plate, in kΩ·cm; ρ is powder volume resistivity of the positive active material under a pressure of 20 MPa, in kΩ·cm; a is mass percentage of the positive active material in the positive electrode film, in wt %; and
wherein the first lithium manganese-based positive active material is a compound represented by formula (3), and the second lithium manganese-based positive active material is a compound represented by formula (4),
Li1+xMnaNibM1-a-bO2-yAy formula (3)
Li1+zMneN2-eO4-dBd formula (4)
where in the formula (3), −0.1x0.2, 0<a<1, 0b<1, 0<a+b<1, 0y<0.2, and M includes one or more of Co, Fe, Cr, Ti, Zn, V, Al, Zr and Ce, A includes one or more of S, N, F, Cl, Br and I; and
in the formula (4), −0.1z0.2, 0<e2, 0d<1, and N includes one or more of Ni, Fe, Cr, Ti, Zn, V, Al, Mg, Zr and Ce, B includes one or more of S, N, F, Cl, Br and I.