# US 11,121,367 B2 · Modified positive electrode active material, method for preparing the same and electrochemical energy storage device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,367 B2
- Document ID: US11121367B2
- Status: Granted
- Kind: B2
- Application number: 15/577,290
- Filed: 2017-08-24
- Published: 2019-02-07
- Granted: 2021-09-14
- Earliest claimed: 2017-05-15
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Rui Du; Na Liu; Yongchao Liu; Sihui Wang; Zhongling Xu; Chao Yang
- Web page: https://patentgrep.com/patent/US11121367B2

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/139: Processes of manufacture
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/502: {for non-aqueous cells (H01M4/505 takes precedence)}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/621: {Binders}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The disclosure provides a modified positive electrode active material, a preparation method thereof, and an electrochemical energy storage device. The modified positive electrode active material comprises positive electrode active material substrate; first oxide layer, coated on the surface of the positive electrode active material substrate and selected from one or more of oxides of element M being selected from the group of one or more of Li, Al, Zr, Mg, Ti, Y, Si, Ca, Cr, Fe, Zn, Nb, Sn, Ba, and Cd; and second oxide layer having a continuous layered structure, coated on the surface of the first oxide layer and selected from one or more of oxides of element M′ being selected from one or more of Li, B, P, As, Pb, V, Mo, and Sn. High temperature storage performance and cycling performance of electrochemical energy storage device are improved by the modified positive electrode active material.

## Claims

### Claim 1

A modified positive electrode active material, comprising:
a positive electrode active material substrate, wherein, the positive electrode active material substrate is lithium-nickel-manganese-cobalt-based oxide ternary material LiNi0.8Co0.1Mn0.1O2;
a first oxide layer, coated on the surface of the positive electrode active material substrate and selected from one or more of oxides of element M, wherein the element M is Al, and the one or more of oxides is Al2O3; and
a second oxide layer having a continuous layered structure, coated on the surface of the first oxide layer and selected from one or more of oxides of element M′, wherein the element M′ is B, and one or more of oxides is B2O3;
wherein based on the mass of the positive electrode active material substrate, the element M is present in an amount of 0.01% to 2% in the first oxide layer and the element M′ is present in an amount of 0.01% to 1% in the second oxide layer; and
wherein the positive electrode active material substrate comprises primary particles and secondary particles formed by agglomeration of primary particles; and wherein the primary particles have a particle diameter of 0.2 μm to 1 μm and the secondary particles have a particle diameter of 5 μm to 18 μm.

### Claim 2 (depends on 1)

The modified positive electrode active material according to claim 1, wherein the first oxide layer coated on the surface of the positive electrode active material substrate has an island-like shape.

### Claim 3 (depends on 1)

The modified positive electrode active material according to claim 1, wherein based on the mass of the positive electrode active material substrate, the element M and the element M′ are present in the following amounts:
(i) the element M is present in an amount of 0.3%, and the element M′ is present in an amount of 0.2%;
(ii) the element M is present in an amount of 0.01%, and the element M′ is present in an amount of 0.1%;
(iii) the element M is present in an amount of 2%, and the element M′ is present in an amount of 0.01%; or
(iv) the element M is present in an amount of 2%, and the element M′ is present in an amount of 1%.

### Claim 4 (depends on 1)

A method for preparing the modified positive electrode active material according to claim 1, comprising the steps of:
(i) mixing homogeneously a positive electrode active material substrate with first oxide layer substance itself or the precursor thereof, followed by sintering, to coat the surface of the positive electrode active material substrate with the first oxide layer selected from one or more of the oxides of element M, wherein the element M is Al, and the one or more of oxides is Al2O3;
(ii) mixing homogeneously the substance obtained in step (i) with second oxide layer substance itself or the precursor thereof, followed by sintering, so that the formed second oxide layer is coated on the surface of the first oxide layer and has a continuous layered structure, wherein the second oxide layer is selected from one or more of the oxides of element M′, wherein the element M′ is B, and one or more of oxides is B2O3, thus yielding the modified positive electrode active material;
wherein based on the mass of the positive electrode active material substrate, the element M is present in an amount of 0.01% to 2% in the first oxide layer and the element M′ is present in an amount of 0.01% to 1% in the second oxide layer; and
wherein the positive electrode active material substrate comprises primary particles and secondary particles formed by agglomeration of primary particles; and wherein the primary particles have a particle diameter of 0.2 μm to 1 μm and the secondary particles have a particle diameter of 5 μm to 18 μm;
wherein the positive electrode active material substrate is lithium-nickel-manganese-cobalt-based oxide ternary material LiNi0.8Co0.1Mn0.1O2.

### Claim 5 (depends on 4)

The method for preparing the modified positive electrode active material according to claim 4, wherein melting point of the first oxide layer substance is higher than melting point of the precursor of the second oxide layer substance, so that the second oxide layer after sintering is uniformly coated on the surface of the first oxide layer; and wherein the formed second oxide layer has a continuous layered structure.

### Claim 6 (depends on 4)

The method for preparing the modified positive electrode active material according to claim 4, wherein melting point of the first oxide layer substance is higher than melting point of the second oxide layer substance itself, so that the second oxide layer after sintering is uniformly coated on the surface of the first oxide layer; and wherein the formed second oxide layer has a continuous layered structure.

### Claim 7 (depends on 5)

The method for preparing the modified positive electrode active material according to claim 5, wherein
the temperature of sintering in step (ii) is lower than that in step (i) and is equal to or greater than the melting point of the precursor of the second oxide layer substance;
the temperature of sintering in step (i) is 600° C. to 750° C.;
the temperature of sintering in step (ii) is 400° C. to 600° C.

### Claim 8 (depends on 6)

The method for preparing the modified positive electrode active material according to claim 6, wherein
the temperature of sintering in step (ii) is lower than that in step (i) and is equal to or greater than the melting point of the second oxide layer substance itself;
the temperature of sintering in step (i) is 600° C. to 750° C.;
the temperature of sintering in step (ii) is 400° C. to 600° C.

### Claim 9

An electrochemical energy storage device, comprising the modified positive electrode active material, wherein the modified positive electrode active material comprises:
a positive electrode active material substrate, wherein the positive electrode active material substrate is lithium-nickel-manganese-cobalt-based oxide ternary material LiNi0.8Co0.1Mn0.1O2;
a first oxide layer, coated on the surface of the positive electrode active material substrate and selected from one or more of oxides of element M, wherein the element M is Al, and the one or more of oxides is Al2O3; and
a second oxide layer having a continuous layered structure, coated on the surface of the first oxide layer and selected from one or more of oxides of element M′, wherein the element M′ is B, and one or more of oxides is B2O3;
wherein based on the mass of the positive electrode active material substrate, the element M is present in an amount of 0.01% to 2% in the first oxide layer and the element M′ is present in an amount of 0.01% to 1% in the second oxide layer; and
wherein the positive electrode active material substrate comprises primary particles and secondary particles formed by agglomeration of primary particles; and wherein the primary particles have a particle diameter of 0.2 μm to 1 μm and the secondary particles have a particle diameter of 5 μm to 18 μm.