# US 11,121,366 B2 · Electrodes for rechargeable lithium batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,366 B2
- Document ID: US11121366B2
- Status: Granted
- Kind: B2
- Application number: 16/085,371
- Filed: 2017-03-16
- Published: 2019-06-06
- Granted: 2021-09-14
- Earliest claimed: 2016-03-16
- Assignees: Universidad Carlos III De Madrid
- Applicants: Universidad Carlos III De Madrid
- Inventors: Belen Levenfeld Laredo; Maria Eugenia Sotomayor Lozano; Wilmer Oswaldo Bucheli Erazo; Jean Yves Sanchez; Alejandro Varez Alvarez; Jose Manuel Amarilla Alvarez
- Web page: https://patentgrep.com/patent/US11121366B2

## CPC

- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/417: Polyolefins
- H01M 50/42: Acrylic resins
- H01M 50/426: Fluorocarbon polymers
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0022: Room temperature molten salts
- H01M 2300/0037: Mixture of solvents
- H01M 2300/0085: Immobilising or gelification of electrolyte
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to an electrode made of a lithium active ceramic material, without polymer binders and with a thickness more than 50 μm, to the method for manufacturing same, and to the use thereof in rechargeable batteries.

## Claims

### Claim 1

A manufacturing method of an electrode for batteries, wherein an active electrode material is selected from a mixed oxide of lithium or a lithium phosphate, characterized in that the electrode has a thickness in a range between 50 μm and 2000 μm, and a density in a range between 2.2 g/cm3 and 3.6 g/cm3, and the active electrode material is without polymer binders, and wherein the active electrode is selected from:
a) mixed oxides of lithium and titanium of general formula LixTiyOz, wherein x, y, z are in a range between 0.01 and 1;
b) mixed oxides of lithium, cobalt and metal elements with laminar structure of general formula LixCo1-yMyO2,
wherein x is in a range between 0.9 and 1.15;
y is in a range between 0 and 1; and
M comprises one or more elements selected from the group consisting of nickel (Ni), chromium (Cr), manganese (Mn), aluminium (Al), titanium (Ti), iron (Fe), copper (Cu), zinc (Zn), tin (Sn), and vanadium (V);
c) phosphate of lithium, iron and metal elements with olivine structure of general formula LiFe1-yMy(PO4),
wherein y is in a range between 0 and 1; and
M comprises one or more elements selected from the group consisting of nickel (Ni), chromium (Cr), manganese (Mn), cobalt (Co), aluminium (Al), titanium (Ti), iron (Fe), copper (Cu), zinc (Zn), and tin (Sn),
comprising the following stages:
(i) mixing of the active electrode material which is selected from the mixed oxide of lithium or a lithium phosphate, in the form of powder, with a polymer binder;
(ii) granulating of an extrudable mixture obtained in stage i) to obtain the pellets that feed an extruder;
(iii) extruding of the granulate of stage ii) to obtain an electrode of desired thickness and dimensions;
(iv) eliminating the binder by a combined cycle comprising a first stage of elimination with solvent followed by a stage of thermal elimination; and
(v) sintering at a temperature between 750 and 1250° C. in an atmosphere selected from oxygen, air, argon, nitrogen, argon-nitrogen mixtures, and nitrogen-hydrogen mixtures.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the active powder of stage i) is a mixed oxide of lithium and titanium.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the active powder of stage i) is Li4Ti5O12.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the polymer binder of stage i) is a thermoplastic material selected from homopolymers and copolymers of polypropylene, homopolymers and copolymers of high- and low-density polyethylene, homopolymers and copolymers of polyethylene-vinyl-acetate, polystyrene, polyvinyl chloride, polyethylene terephthalate, polyamides, poly (methyl methacrylate), polycarbonate, polyacrylonitrile, polyaniline or mixtures thereof.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the polymer binder is a mixture of polypropylene, paraffin wax and stearic acid.

### Claim 6 (depends on 4)

The method according to claim 4, wherein one or several carbonaceous materials in the form of powder, fibers or sheets are added to the binder.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the carbonaceous material is carbon black.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the debinding stage (iv) takes place by means of a combined cycle comprising a first stage of elimination with solvent at 50° C. for 3 h, followed by a stage of thermal elimination, wherein the product obtained from the previous stage is subjected to 200° C. and later to 450° C.