# US 11,121,361 B2 · Method of preparing slurry for secondary battery positive electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,361 B2
- Document ID: US11121361B2
- Status: Granted
- Kind: B2
- Application number: 16/339,598
- Filed: 2018-03-21
- Published: 2020-02-06
- Granted: 2021-09-14
- Earliest claimed: 2017-03-23
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Byoung Hoon Ahn; Sang Hoon Choy; Chang Wan Koo; Hyun Chul Ha
- Web page: https://patentgrep.com/patent/US11121361B2

## CPC

- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/04: Processes of manufacture in general
- H01M 4/364: {as mixtures}
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/622: {being polymers}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a method of preparing a slurry for a secondary battery positive electrode which includes forming a first mixture in a paste state by adding a lithium iron phosphate-based positive electrode active material, a conductive agent, a binder, and a solvent, and preparing a slurry for a positive electrode by mixing while further adding a solvent to the first mixture in the paste state.

## Claims

### Claim 1

A method of preparing a slurry for a secondary battery positive electrode, the method comprising:
forming a first mixture in a paste state by adding a lithium iron phosphate-based positive electrode active material, a conductive agent, a binder, and a solvent; and
preparing a slurry for a positive electrode by mixing while further adding a solvent to the first mixture in the paste state,
wherein the first mixture has a shear viscosity of 1,000 Pa·s to 5,000 Pa·s at a shear rate of 10−1/s and at a temperature of 23° C, and the first mixture has a solid content of 60 wt % to 70 wt %.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first mixture has a shear viscosity of 100 Pa·s to 500 Pa·s at a shear rate of 1/s and at a temperature of 23° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first mixture has a shear viscosity of 2,000 Pa·s to 3,000 Pa·s at a shear rate of 10−1/s and at a temperature of 23° C., and has a shear viscosity of 200 Pa·s to 300 Pa·s at a shear rate of 1/s and at a temperature of 23° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the lithium iron phosphate-based positive electrode active material is a primary particle having an average particle diameter of less than 1 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the lithium iron phosphate-based positive electrode active material is represented by Formula 1:
Li1+aFe1-xMxPO4-bAb [Formula 1]
wherein, in Formula 1, M is at least one selected from the group consisting of manganese, nickel, cobalt, copper, scandium, titanium, chromium, vanadium, and zinc, A is at least one selected from the group consisting of sulfur, selenium, fluorine, chlorine, and iodine, −0.5<a<0.5, 0≤x<0.5, and 0≤b≤0.1.

### Claim 6 (depends on 1)

The method of claim 1, further adding a dispersant during the formation of the first mixture.

### Claim 7 (depends on 6)

The method of claim 6, wherein the dispersant comprises a hydrogenated nitrile butadiene rubber.

### Claim 8 (depends on 6)

The method of claim 6, wherein the dispersant is mixed in an amount of 0.8 part by weight to 1.5 parts by weight based on 100 parts by weight of the lithium iron phosphate-based positive electrode active material.