# US 11,121,357 B2 · Positive electrode active material for secondary battery and method of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,357 B2
- Document ID: US11121357B2
- Status: Granted
- Kind: B2
- Application number: 16/320,859
- Filed: 2018-02-02
- Published: 2019-05-30
- Granted: 2021-09-14
- Earliest claimed: 2017-02-02
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: So Ra Baek; Ji Hye Kim; Tae Gu Yoo; Wang Mo Jung; Byung Chun Park
- Web page: https://patentgrep.com/patent/US11121357B2

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01B 35/10: Compounds containing boron and oxygen (C01B35/06 takes precedence)
- H01M 4/139: Processes of manufacture
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The present invention relates to a positive electrode active material for a secondary battery, which includes a core including a lithium composite metal oxide, and a surface treatment layer which is disposed on the core and includes an amorphous oxide containing a lithium (Li) oxide, a boron (B) oxide, and an aluminum (Al) oxide, wherein an amount of a lithium by-product present on a surface of the positive electrode active material is less than 0.55 wt % based on a total weight of the positive electrode active material, and a method of preparing the same.

## Claims

### Claim 1

A positive electrode active material for a secondary battery, the positive electrode active material comprising:
a core including a lithium composite metal oxide; and
a surface treatment layer which is disposed on the core and includes an amorphous oxide containing a lithium oxide, a boron oxide, and an aluminum oxide,
wherein the lithium oxide, the boron oxide, and the aluminum oxide are chemically bonded to one another, and
wherein, in the amorphous oxide in the surface treatment layer, an amount of the aluminum oxide is greater than an amount of the boron oxide, and wherein the amorphous oxide limits an amount of a lithium by-product present on a surface of the positive electrode active material, created during formation of the core, to less than 0.55 wt % based on a total weight of the positive electrode active material, and
wherein a mole ratio of the boron oxide to the aluminum oxide is in a range of greater than 1:1 to less than 1:2.5.

### Claim 2 (depends on 1)

The positive electrode active material for a secondary battery of claim 1, wherein the lithium composite metal oxide is represented by Formula 1:
Lia(NixCoyM1z)bM2cO2 <Formula 1>
wherein, in Formula 1,
M1 is at least one element selected from the group consisting of manganese and aluminum, and
M2 is at least one element selected from the group consisting of barium, calcium, zirconium, titanium, magnesium, tantalum, niobium, and molybdenum,
wherein 1≤a≤1.5, 0.9≤b≤1, 0≤c≤0.1, 0.6≤x<1, 0<y<0.4, 0<z≤0.4, and b+c=1.

### Claim 3 (depends on 1)

The positive electrode active material for a secondary battery of claim 1, wherein the lithium oxide is Li2O, the boron oxide is B2O3, and the aluminum oxide is Al2O3.

### Claim 4 (depends on 3)

The positive electrode active material for a secondary battery of claim 3, wherein the Li2O, the B2O3, and the Al2O3 are chemically bonded to one another in a form selected from the group consisting of 2LiAl7B4O5, 2LiAlB2O5, and 2Li2AlB2O5.

### Claim 5 (depends on 1)

The positive electrode active material for a secondary battery of claim 1, wherein the surface treatment layer has an average thickness of 20 nm to 100 nm.

### Claim 6 (depends on 1)

The positive electrode active material for a secondary battery of claim 1, wherein the positive electrode active material has an average particle diameter (D50) of 1 μm to 20 μm.

### Claim 7 (depends on 1)

The positive electrode active material for a secondary battery of claim 1, wherein the lithium composite metal oxide is a secondary particle formed by agglomeration of primary particles, and
further comprises a segregation phase of Zr oxide on a surface of the secondary particle or at an interface between the primary particles.

### Claim 8 (depends on 1)

A positive electrode for a secondary battery, the positive electrode comprising the positive electrode active material of claim 1, a binder, a conductive agent, and a positive electrode collector.

### Claim 9 (depends on 8)

A secondary battery comprising: the positive electrode of claim 8, a negative electrode disposed to face the positive electrode, a separator disposed between the positive electrode and the negative electrode, and an electrolyte.

### Claim 10 (depends on 1)

A method of preparing the positive electrode active material for a secondary battery of claim 1, the method comprising:
preparing a mixture by mixing the core, a lithium-containing raw material, a boron-containing raw material, and an aluminum-containing raw material; and
forming the surface treatment layer including the amorphous oxide on the core by performing a heat treatment on the mixture in an oxygen atmosphere at a temperature of 500° C. to 800° C.,
wherein the forming of the amorphous oxide is to form an amorphous oxide containing lithium, boron, and aluminum by reaction of the lithium by-product present on the surface of the lithium composite metal oxide with the boron-containing raw material and the aluminum-containing raw material.

### Claim 11 (depends on 10)

The method of claim 10, wherein the boron-containing raw material is mixed in an amount of 0.1 parts by weight to 0.8 parts by weight and the aluminum-containing raw material is mixed in an amount of 0.1 parts by weight to 1 parts by weight, based on 100 parts by weight of the lithium composite metal oxide.

### Claim 12 (depends on 10)

The method of claim 10, wherein the boron-containing raw material comprises at least one of H3BO3, HBPO4, B2O3, B2O5, Li2B4O7, or (NH4)2B4O7.

### Claim 13 (depends on 10)

The method of claim 10, wherein the aluminum-containing raw material comprises at least one of Al(OH)3, Al2(SO4)3, AlCl3, or Al(NO3)3.

### Claim 14 (depends on 10)

The method of claim 10, wherein the lithium by-product comprises at least one of LiOH or Li2CO3.