# US 11,121,351 B2 · Flexible display panel and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,351 B2
- Document ID: US11121351B2
- Status: Granted
- Kind: B2
- Application number: 16/639,749
- Filed: 2019-11-20
- Published: 2021-03-04
- Granted: 2021-09-14
- Earliest claimed: 2019-08-26
- Assignees: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Applicants: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Inventors: Fuyang Zhang
- Web page: https://patentgrep.com/patent/US11121351B2

## CPC

- H10K 77/111: {Flexible substrates}
- H10K 59/8722: {Peripheral sealing arrangements, e.g. adhesives, sealants}
- H10K 59/12: Active-matrix OLED [AMOLED] displays
- H10K 59/1201: {Manufacture or treatment}
- H10K 59/8731: {multilayered coatings having a repetitive structure, e.g. having multiple organic-inorganic bilayers}
- H10K 71/80: using temporary substrates
- H10K 71/851: {Division of substrate}
- H10K 2102/311: {Flexible OLED}
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A flexible display panel and a preparation method thereof are provided. A composite substrate structure composed of a first polyimide layer, a water-oxygen barrier layer, a protective layer, and a second polyimide layer is prepared, and the protective layer covers a partial lateral side of the second polyimide layer in a non-display area and a lateral side of the water-oxygen barrier layer in the non-display area. Thus, the water and oxygen barrier property of the composite substrate structure is improved.

## Claims

### Claim 1

A preparation method of a flexible display panel, comprising steps of:
providing a rigid substrate, the rigid substrate having a panel area and a panel edge area divided by a laser cut line;
preparing a first polyimide layer on the rigid substrate, the first polyimide layer being formed in the panel area and the panel edge area;
depositing a water-oxygen barrier layer on the first polyimide layer, the water-oxygen barrier layer covering the first polyimide layer;
preparing a protective layer on the water-oxygen barrier layer, the protective layer extending from the laser cut line to the panel area and the panel edge area respectively, wherein an initial thickness of the protective layer ranges from 0.5 to 5 μm;
preparing a second polyimide layer on the protective layer and the water-oxygen barrier layer;
preparing a panel display assembly on the second polyimide layer corresponding to the panel area; and
separating the rigid substrate from the first polyimide layer, and cutting the panel edge area along the laser cut line to obtain the flexible display panel, wherein the protective layer retained in the panel area after being cut covers a partial lateral side of the second polyimide layer at the laser cut line and a lateral side of the water-oxygen barrier layer at the laser cut line.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein a material of the protective layer comprises at least one of aluminum, tin, lead, bismuth, silver, and copper.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein a material of the protective layer comprises at least one of an aluminum-based alloy, a tin-based alloy, a lead-based alloy, a bismuth-based alloy, a silver-based alloy, and a copper-based alloy.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein a thickness of the protective layer retained in the panel area after being cut ranges from 1 to 10 μm.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the step of preparing the panel display assembly on the second polyimide layer corresponding to the panel area further comprises: sequentially preparing a thin film transistor array layer, a light emitting layer, and an encapsulation layer on the second polyimide layer corresponding to the panel area, wherein the encapsulation layer covers a lateral side of the thin film transistor array layer and a lateral side of the light emitting layer near the laser cut line, and partially covers the second polyimide layer.

### Claim 6

A preparation method of a flexible display panel, comprising steps of:
providing a rigid substrate, the rigid substrate having a panel area and a panel edge area divided by a laser cut line;
preparing a first polyimide layer on the rigid substrate, the first polyimide layer being formed in the panel area and the panel edge area;
depositing a water-oxygen barrier layer on the first polyimide layer, the water-oxygen barrier layer covering the first polyimide layer;
preparing a protective layer on the water-oxygen barrier layer, the protective layer extending from the laser cut line to the panel area and the panel edge area respectively;
preparing a second polyimide layer on the protective layer and the water-oxygen barrier layer;
preparing a panel display assembly on the second polyimide layer corresponding to the panel area; and
separating the rigid substrate from the first polyimide layer, and cutting the panel edge area along the laser cut line to obtain the flexible display panel.

### Claim 7 (depends on 6)

The preparation method according to claim 6, wherein the step of cutting the panel edge area along the laser cut line further comprises: melting and solidifying the protective layer in a cutting process, wherein the protective layer retained in the panel area after being cut covers a partial lateral side of the second polyimide layer at the laser cut line and a lateral side of the water-oxygen barrier layer at the laser cut line.

### Claim 8 (depends on 7)

The preparation method according to claim 7, wherein the protective layer retained in the panel area after being cut further covers a partial lateral side of the first polyimide layer at the laser cut line.

### Claim 9 (depends on 6)

The preparation method according to claim 6, wherein a material of the protective layer comprises at least one of aluminum, tin, lead, bismuth, silver, and copper.

### Claim 10 (depends on 6)

The preparation method according to claim 6, wherein a material of the protective layer comprises at least one of an aluminum-based alloy, a tin-based alloy, a lead-based alloy, a bismuth-based alloy, a silver-based alloy, and a copper-based alloy.

### Claim 11 (depends on 6)

The preparation method according to claim 6, wherein an initial thickness of the protective layer ranges from 0.5 to 5 μm.

### Claim 12 (depends on 6)

The preparation method according to claim 6, wherein a thickness of the protective layer retained in the panel area after being cut ranges from 1 to 10 μm.

### Claim 13 (depends on 6)

The preparation method according to claim 6, wherein the step of preparing the panel display assembly on the second polyimide layer corresponding to the panel area further comprises: sequentially preparing a thin film transistor array layer, a light emitting layer, and an encapsulation layer on the second polyimide layer corresponding to the panel area, wherein the encapsulation layer covers a lateral side of the thin film transistor array layer and a lateral side of the light emitting layer near the laser cut line, and partially covers the second polyimide layer.

### Claim 14

A flexible display panel comprising a panel area, the panel area comprising a display area and a non-display area, wherein the flexible display panel further comprises:
a flexible base substrate comprising a first polyimide layer, a water-oxygen barrier layer, and a second polyimide layer sequentially stacked and disposed, the flexible base substrate further comprising a protective layer disposed in the non-display area, wherein the protective layer covers a partial lateral side of the second polyimide layer in the non-display area and a lateral side of the water-oxygen barrier layer in the non-display area; and
a panel display assembly disposed on the flexible base substrate,
wherein a material of the protective layer comprises at least one of aluminum, tin, lead, bismuth, silver, and copper, or at least one of an aluminum-based alloy, a tin-based alloy, a lead-based alloy, a bismuth-based alloy, a silver-based alloy, and a copper-based alloy.

### Claim 15 (depends on 14)

The flexible display panel according to claim 14, wherein an outer surface of the protective layer protrudes from a side of the non-display area.

### Claim 16 (depends on 14)

The flexible display panel according to claim 14, wherein a material of the protective layer comprises at least one of an aluminum-based alloy, a tin-based alloy, a lead-based alloy, a bismuth-based alloy, a silver-based alloy, and a copper-based alloy.

### Claim 17 (depends on 14)

The flexible display panel according to claim 14, wherein a thickness of the protective layer ranges from 1 to 10 μm.

### Claim 18 (depends on 14)

The flexible display panel according to claim 14, wherein the protective layer further covers a partial lateral side of the first polyimide layer at the laser cut line.

### Claim 19 (depends on 14)

The flexible display panel according to claim 14, wherein the panel display assembly comprise a thin film transistor array layer, a light emitting layer, and an encapsulation layer sequentially stacked and disposed on the second polyimide layer corresponding to the display area, wherein the encapsulation layer covers a lateral side of the thin film transistor array layer and a lateral side of the light emitting layer in the non-display area, and partially covers the second polyimide layer.