# US 11,121,338 B2 · Quantum dot material, preparation method, and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,338 B2
- Document ID: US11121338B2
- Status: Granted
- Kind: B2
- Application number: 15/761,670
- Filed: 2017-04-14
- Published: 2019-01-03
- Granted: 2021-09-14
- Earliest claimed: 2016-12-30
- Assignees: Tcl Technology Group Corporation
- Applicants: Tcl Technology Group Corporation
- Inventors: Yixing Yang; Zheng Liu; Lei Qian
- Web page: https://patentgrep.com/patent/US11121338B2

## CPC

- C09K 11/565: {with zinc cadmium}
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C09K 11/883: {with zinc or cadmium}
- H10K 50/115: comprising active inorganic nanostructures, e.g. luminescent quantum dots
- C23C 28/32: {including at least one pure metallic layer}
- C23C 28/345: {with at least one oxide layer}
- H10K 50/15: Hole transporting layers
- H10K 50/16: Electron transporting layers
- H10K 85/111: {comprising aromatic, heteroaromatic, or aryl chains, e.g. polyaniline, polyphenylene or polyphenylene vinylene}
- H10K 85/1135: {Polyethylene dioxythiophene [PEDOT]; Derivatives thereof}
- H10K 85/146: {poly N-vinylcarbazol; Derivatives thereof}
- H10K 85/626: {containing more than one polycyclic condensed aromatic rings, e.g. bis-anthracene}
- H10K 85/633: {comprising polycyclic condensed aromatic hydrocarbons as substituents on the nitrogen atom}
- H10K 2101/80: {Composition varying spatially, e.g. having a spatial gradient}
- H10K 2102/00: Constructional details relating to the organic devices covered by this subclass
- H10K 2102/103: {comprising indium oxides, e.g. ITO}
- H10K 2102/321: {Inverted OLED, i.e. having cathode between substrate and anode}
- Y02E 10/549: Organic PV cells
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a QD material, a preparation method, and a semiconductor device. The QD material includes at least one QD structural unit arranged sequentially along a radial direction of the QD material. Each QD structural unit has a gradient alloy composition structure with a changing energy level width along the radial direction or a homogeneous alloy composition structure with a constant energy level width along the radial direction. The disclosed QD material not only achieves higher light-emission efficiency of QD material, but also meets the comprehensive requirements of semiconductor devices and the corresponding display technologies on QD materials. Therefore, the disclosed QD material is a desired QD light-emitting material suitable for semiconductor devices and display technologies.

## Claims

### Claim 1

A quantum dot (QD) material, comprising:
at least one QD structural unit arranged sequentially along a radial direction of the QD material, wherein:
each QD structural unit has a gradient alloy composition structure with a changing energy level width along the radial direction or a homogeneous alloy composition structure with a constant energy level width along the radial direction; and
the QD material includes two types of QD structural units; wherein:
one type of QD structural unit has the homogeneous alloy composition structure;
another type of QD structural unit has the gradient alloy composition structure with an energy level width increasing along the radial direction from a center to a surface of the QD material;
an inner part of the QD material includes one or more QD structural units having the homogeneous alloy composition structure; and
an outer part of the QD material includes one or more QD structural units having the gradient alloy composition structure, and along the radial direction, energy levels of adjacent gradient alloy composition structures of the QD structural units are continuous.

### Claim 2 (depends on 1)

The QD material according to claim 1, wherein:
the QD structural unit having the gradient alloy composition structure or the homogeneous alloy composition structure includes Group II elements and Group VI elements.

### Claim 3 (depends on 1)

The QD material according to claim 1, wherein:
the plurality of monatomic layers includes 2-20 monatomic layers, or the at least one unit-cell layer includes 1-10 unit-cell layers.

### Claim 4 (depends on 3)

The QD material according to claim 3, wherein:
each monatomic layer or each unit-cell layer is a smallest structural unit, and an alloy composition of each monatomic layer or each unit-cell layer is fixed; and
each unit-cell layer has a closed unit-cell surface formed through a continuous connection of the unit-cell layers.

### Claim 5 (depends on 1)

The QD material according to claim 1, wherein:
a light-emission peak wavelength of the QD material is in a range of approximately 400 nm to 700 nm.

### Claim 6 (depends on 1)

The QD material according to claim 1, wherein:
a full width at half maximum of a light-emission peak of the QD material is in a range of approximately 12 nm to 80 nm.

### Claim 7 (depends on 1)

A method for preparing the QD material according to claim 1, comprising:
synthesizing a first compound;
synthesizing a second compound on a surface of the first compound, wherein the second compound and the first compound have same elements in different alloy compositions; and
forming the QD material through a cation exchange reaction between the first compound and the second compound, wherein a light-emission peak wavelength of the QD material experiences one or more of a blue-shift, a red-shift, and no-shift.

### Claim 8 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
a cation precursor of the first compound and/or the second compound includes a zinc precursor, wherein the zinc precursor includes at least one of dimethyl zinc, diethyl zinc, zinc acetate, zinc acetylacetonate, zinc iodide, zinc bromide, zinc chloride, zinc fluoride, zinc carbonate, zinc cyanide, zinc nitrate, zinc oxide, zinc peroxide, zinc perchlorate, zinc sulfate, zinc oleate, and zinc stearate.

### Claim 9 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
a cation precursor of the first compound and/or the second compound includes a cadmium precursor, wherein the cadmium precursor includes at least one of dimethyl cadmium, diethyl cadmium, cadmium acetate, cadmium acetylacetonate, cadmium iodide, cadmium bromide, cadmium chloride, cadmium fluoride, cadmium carbonate, cadmium nitrate, cadmium oxide, cadmium perchlorate, cadmium phosphate, cadmium sulfate, cadmium oleate, and cadmium stearate.

### Claim 10 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
an anion precursor of the first compound and/or the second compound includes a selenium precursor, wherein the selenium precursor includes at least one of Se-TOP (selenium-trioctylphosphine), Se-TBP (selenium-tributylphosphine), Se-TPP (selenium-triphenylphosphine), Se-ODE (selenium-1-octadecene), Se-OA (selenium-oleic acid), Se-ODA (selenium-octadecylamine), Se-TOA (selenium-trioctylamine), Se-ODPA (selenium-octadecylphosphonic acid), and Se-OLA (selenium-oleylamine).

### Claim 11 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
an anion precursor of the first compound and/or the second compound includes a sulfur precursor, wherein the sulfur precursor includes at least one of S-TOP (sulfur-trioctylphosphine), S-TBP (sulfur-tributylphosphine), S-TPP (sulfur-triphenylphosphine), S-ODE (sulfur-1-octadecene), S-OA (sulfur-oleic acid), S-ODA (sulfur-octadecylamine), S-TOA (sulfur-trioctylamine), S-ODPA (sulfur-octadecylphosphonic acid), S-OLA (sulfur-oleylamine), and alkyl thiol.

### Claim 12 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
an anion precursor of the first compound and/or the second compound includes a tellurium precursor, wherein the tellurium precursor includes at least one of Te-TOP (tellurium-trioctylphosphine), Te-TBP (tellurium-tributylphosphine), Te-TPP (tellurium-triphenylphosphine), Te-ODE (tellurium-1-octadecene), Te-OA (tellurium-oleic acid), Te-ODA (tellurium-octadecylamine), Te-TOA (tellurium-trioctylamine), Te-ODPA (tellurium-octadecylphosphonic acid), and Te-OLA (tellurium-oleylamine).

### Claim 13 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
the cation exchange reaction between the first compound and the second compound is performed under a heating condition.

### Claim 14 (depends on 13)

The method for preparing the QD material according to claim 13, wherein:
a heating temperature is in a range of approximately 100° C. to 400° C.

### Claim 15 (depends on 13)

The method for preparing the QD material according to claim 13, wherein:
a heating time is in a range of approximately 2 seconds to 24 hours.

### Claim 16 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
a molar feed ratio of a cationic precursor to an anion precursor used for forming the first compound is in a range of approximately 100:1 to 1:50.

### Claim 17 (depends on 7)

The method for preparing the QD material according to claim 7, wherein:
a molar feed ratio of a cationic precursor to an anion precursor used for forming the second compound is in a range of approximately 100:1 to 1:50.

### Claim 18 (depends on 1)

A semiconductor device including the QD material according to claim 1, wherein:
the semiconductor device is one of an electroluminescent device, a photoluminescent device, a solar cell, a display device, a photoelectric detector, a biological probe, and nonlinear optical device.