# US 11,121,319 B2 · Phase-change memory with no drift

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,319 B2
- Document ID: US11121319B2
- Status: Granted
- Kind: B2
- Application number: 16/710,069
- Filed: 2019-12-11
- Published: 2021-06-17
- Granted: 2021-09-14
- Earliest claimed: 2019-12-11
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Ning Li; Joel P. de Souza; Stephen W. Bedell; Devendra K. Sadana
- Web page: https://patentgrep.com/patent/US11121319B2

## CPC

- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/8265: {on sidewalls of dielectric structures, e.g. mesa-shaped or cup-shaped devices}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/046: {by diffusion, e.g. photo-dissolution}
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8413: {adapted for resistive heating}
- H10N 70/8828: {Tellurides, e.g. GeSbTe}
- G03F 7/162: {Coating on a rotating support, e.g. using a whirler or a spinner}
- G03F 7/2002: {with visible light or UV light, through an original having an opaque pattern on a transparent support, e.g. film printing, projection printing; by reflection of visible or UV light from an original such as a printed image}
- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A bottom electrode is deposited on top of a substrate. A dielectric material layer is deposited on top of the bottom electrode. A hole is created in the dielectric material layer. A lift off layer is spun on and baked on the dielectric material layer. A photoresist layer is spun on and baked on the lift off layer. UV lithography is performed to create an opening above the hole in the dielectric material layer. An Ag layer is deposited on top of the remaining patterned dielectric material layer and the photoresist layer. A Germanium Antimony Telluride (GST) layer is deposited on top of the Ag layer. A top electrode is deposited on top of the GST layer. The Ag layer, the GST layer, and the top electrode located on top of the photoresist layer along with the photoresist layer and the lift off layer are removed.

## Claims

### Claim 1

A method for fabricating a phase-change memory (PCM), the method comprising:
depositing a bottom electrode on top of a substrate;
depositing a dielectric material layer on top of the bottom electrode;
creating a hole in the dielectric material layer;
spinning on and baking a lift off layer on the remaining dielectric material layer;
spinning on and baking a photoresist layer on top of the lift off layer;
performing UV lithography to create an opening above the hole in the dielectric material layer;
depositing an Ag layer on top of the bottom electrode and on the remaining dielectric material layer and the photoresist layer;
depositing a Germanium Antimony Telluride (GST) layer on top of the Ag layer;
depositing a top electrode on top of the GST layer; and
removing the Ag layer, the GST layer, and the top electrode stack located on top of the photoresist layer along with the photoresist layer and the lift off layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein during the deposition of the Ag layer and the GST layer both layers create an Ag-doped GST alloy layer by thermal mixing.

### Claim 3 (depends on 1)

The method of claim 1, wherein the Ag layer has a thickness less than 20 nm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the Ag layer has a thickness between 5 nm and 10 nm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the GST layer has a thickness less than 200 nm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the GST layer has a thickness between 20 nm and 50 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the hole in the dielectric layer is 1 micron or less of lateral dimension.

### Claim 8

A method for fabricating a phase-change memory (PCM), the method comprising:
depositing a bottom electrode on top of a substrate;
depositing a dielectric material layer on top of the bottom electrode;
creating a hole in the dielectric material layer;
spinning on and baking a lift off layer on the dielectric material layer with the hole;
spinning on and baking a photoresist layer on the lift off layer;
performing UV lithography to create an opening above the hole in the dielectric material layer;
depositing a first Ag layer on top of the bottom electrode and on the remaining dielectric material layer and the photoresist layer;
depositing a Germanium Antimony Telluride (GST) layer on top of the first Ag layer;
depositing a second Ag layer on top of the GST layer;
depositing a top electrode on top of the second Ag layer; and
removing the first Ag layer, the GST layer, the second Ag layer and the top electrode located on top of the photoresist layer along with the photoresist layer and the lift off layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein during the deposition of the first Ag layer, the GST layer, and the second Ag layer, all three layers can create an Ag-doped GST alloy layer by thermal mixing.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first Ag layer and the second Ag layer have a thickness less than 20 nm.

### Claim 11 (depends on 8)

The method of claim 8, wherein the first Ag layer and the second Ag layer have a thickness between 5 nm and 10 nm.

### Claim 12 (depends on 8)

The method of claim 8, wherein the GST layer has a thickness less than 200 nm.

### Claim 13 (depends on 8)

The method of claim 8, wherein the GST layer has a thickness between 20 nm and 50 nm.

### Claim 14 (depends on 8)

The method of claim 8, wherein the hole is 1 micron or less of lateral dimension.

### Claim 15

A method for fabricating a phase-change memory (PCM), the method comprising:
depositing a bottom electrode on top of a substrate;
depositing a dielectric material layer on top of the bottom electrode;
creating a hole in the dielectric material layer;
spinning on and baking a lift off the dielectric material layer;
spinning on and baking a photoresist layer on the lift off layer;
performing UV lithography to create an opening above the hole in the dielectric material layer;
depositing a Germanium Antimony Telluride (GST) on top of the bottom electrode and on the remaining dielectric material layer and the photoresist layer;
depositing an Ag layer on top of the GST layer;
depositing a top electrode on top of the Ag layer; and
removing the GST layer, the Ag layer, and the top electrode located on top of the photoresist layer along with the photoresist layer and the lift off layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein during the deposition of the GST layer and the Ag layer both layers can create an Ag-doped GST alloy layer by thermal mixing.

### Claim 17 (depends on 15)

The method of claim 15, wherein the Ag layer has a thickness less than 20 nm.

### Claim 18 (depends on 15)

The method of claim 15, wherein the Ag layer has a thickness between 5 nm and 10 nm.

### Claim 19 (depends on 15)

The method of claim 15, wherein the GST layer has a thickness less than 200 nm.

### Claim 20 (depends on 15)

The method of claim 15, wherein the GST layer has a thickness between 20 nm and 50 nm.