# US 11,121,282 B2 · Method for producing a CdTe thin-film solar cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,282 B2
- Document ID: US11121282B2
- Status: Granted
- Kind: B2
- Application number: 16/064,636
- Filed: 2016-12-27
- Published: 2021-07-08
- Granted: 2021-09-14
- Earliest claimed: 2016-12-27
- Assignees: China Triumph International Engineering Co., Ltd.; Ctf Solar GmbH
- Applicants: China Triumph International Engineering Co., Ltd.; Ctf Solar GmbH
- Inventors: Christian Drost; Sven Frauenstein; Michael Harr; Shou Peng
- Web page: https://patentgrep.com/patent/US11121282B2

## CPC

- H10F 71/125: {The active layers comprising only Group II-VI materials, e.g. CdS, ZnS or CdTe}
- H10F 19/30: comprising thin-film photovoltaic cells
- H10F 71/131: {Recrystallisation; Crystallization of amorphous or microcrystalline semiconductors}
- H10F 71/138: {Manufacture of transparent electrodes, e.g. transparent conductive oxides [TCO] or indium tin oxide [ITO] electrodes}
- H10F 77/123: comprising only Group II-VI materials, e.g. CdS, ZnS or HgCdTe
- H10F 77/1696: {the films including Group II-VI materials, e.g. CdTe or CdS}
- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- Y02E 10/543: Solar cells from Group II-VI materials
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention describes a method for producing CdTe thin-film solar cells, in which special parameters of different processing steps and a special sequence of processing steps result in improved characteristics of the produced CdTe solar cells.

## Claims

### Claim 1

A method for producing a CdTe thin film solar cell, the method comprising the steps:
providing a transparent substrate with a transparent conducting layer as a front contact on it,
applying a CdS layer on the transparent conducting layer using closed space sublimation technique, wherein the CdS layer is applied with a thickness in the range between 20 nm to 40 nm,
applying a CdTe layer on the CdS layer using closed space sublimation technique, wherein the CdTe layer is applied with a thickness in the range between 3 μm and 5 μm,
applying a crystalline layer of CdCl2 with a thickness in the range of 50 nm to 100 nm on a first surface of the CdTe layer,
performing a first temperature treatment step after applying the CdCl2 layer at a temperature in the range of 380° C. to 430° C. for a time in the range of 15 minutes to 45 minutes under atmospheric conditions,
performing a first cleaning step after the first temperature treatment step, wherein the layer stack resulting from the previous processing steps is dipped into a solution of diammonium hydrogen citrate with a concentration in the range of 0.1% to 50% for a time in the range of 15 seconds to 5 minutes,
applying a back contact layer on the first surface after the first cleaning step, wherein the back contact layer is applied with a thickness in the range of 200 nm to 400 nm and comprises molybdenum,
providing copper ions to a first surface of the back contact layer by dipping a layer stack resulting from the previous process steps into a CuCl2 solution with a concentration in the range of 0.05 mmol/l to 1 mmol/l for a time in the range of 30 seconds to 2 minutes,
performing a second temperature treatment step after removing the layer stack from the CuCl2 solution at a temperature in the range of 180° C. to 250° C. for a time period with a duration in the range of 10 minutes to 45 minutes under atmospheric conditions,
performing an artificial aging step after performing the second cleaning step, wherein the artificial aging step includes an illumination of the layer stack resulting from the previous process steps for a time in the range of 1 minute to 48 hours with an illuminance in the range of 5000 lx to 200000 lx at a temperature in the range of 70° C. to 80° C. under atmospheric conditions, and
performing a second cleaning step after performing the artificial aging step, wherein the layer stack resulting from the previous processing steps is cleaned by dipping the layer stack into a dimethylformamide solution with a concentration in the range of 50% to 100% for a time in the range of 1 minute to 10 minutes and subsequently rinsed with water and isopropanol.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising performing a further cleaning step after the second temperature treatment step and before the artificial aging step, wherein the layer stack resulting from the previous processing steps is cleaned by dipping the layer stack into a solution of dimethylformamide with a concentration in the range of 50% to 100% for a time in the range of 1 minute to 10 minutes.

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that the layer stack is dipped into a 100%-solution of dimethylformamide for 5 minutes in the second cleaning step or in the further cleaning step.

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that the CdS layer is applied with a thickness of 30 nm.

### Claim 5 (depends on 1)

The method according to claim 1, characterized in that the CdTe layer is applied with a thickness of 4 μm.

### Claim 6 (depends on 1)

The method according to claim 1, characterized in that the crystalline CdCl2 layer is applied with a thickness of 80 nm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the CdCl2 is preferably applied as an aqueous salt solution by roller coating.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first temperature treatment step is performed at a temperature of 410° C. for 25 minutes.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first cleaning step is performed with a 1%-solution of diammonium hydrogen citrate for 1 minute.

### Claim 10 (depends on 1)

The method according to claim 1, characterized in that the back contact layer is made of molybdenum and is applied with a thickness of 300 nm.

### Claim 11 (depends on 1)

The method according to claim 1, wherein providing copper ions is performed by dipping the layer stack into a 0.1 mmol/l CuCl2 solution for 1 minute.

### Claim 12 (depends on 1)

The method according to claim 1, characterized in that the second temperature treatment step is performed at a temperature of 200° C. for 15 minutes.

### Claim 13 (depends on 1)

The method according to claim 1, characterized in that, during the artificial aging step, the layer stack is held at a temperature of 75° C., while it is illuminated with an illuminance of about 35000 lx for 48 hours.

### Claim 14 (depends on 2)

The method according to claim 2, characterized in that the layer stack is dipped into a 100%-solution of dimethylformamide for 5 minutes in the second cleaning step or in the further cleaning step.