# US 11,121,267 B2 · Antireflective coating for glass applications and method of forming same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,267 B2
- Document ID: US11121267B2
- Status: Granted
- Kind: B2
- Application number: 14/771,451
- Filed: 2014-03-03
- Published: 2016-01-07
- Granted: 2021-09-14
- Earliest claimed: 2013-03-01
- Assignees: Board of Trustees of the University of Arkansas
- Applicants: Board of Trustees of the University of Arkansas
- Inventors: Min Zou; Corey Thompson; Robert A. Fleming
- Web page: https://patentgrep.com/patent/US11121267B2

## CPC

- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- C03C 17/001: {General methods for coating; Devices therefor}
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- G02B 1/118: having sub-optical wavelength surface structures designed to provide an enhanced transmittance, e.g. moth-eye structures
- C03C 2217/734: comprising an alternation of high and low refractive indexes
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

One aspect of the disclosure is directed to a method for forming an antireflective coating on a substrate, which includes providing a polymer solution and a silica solution, depositing the polymer solution on a surface of the substrate to forming a polymer film thereon, depositing the silica solution on the formed polymer film on the substrate to form a silica film thereon, thereby forming a stack structure having the silica film formed on the polymer film that is, in turn, formed on the substrate, and drying the stack structure to form the antireflective coating on the substrate, wherein the antireflective coating comprises silica nanoparticles.

## Claims

### Claim 1

A method for forming an antireflective coating on a substrate, comprising:
(a) providing a polyvinylpyrrolidone (PVP) solution and a silica solution, wherein the PVP solution has a concentration of the PVP in a range of 1-20 wt %, and wherein the silica solution consists of a colloidal silica solution diluted by deionized water so that the silica solution comprises 5 wt % of silica in a colloidal form;
(b) depositing the PVP solution directly on a surface of the substrate to form a PVP film in contact with the substrate; and
(c) depositing the silica solution directly on the formed PVP film on the substrate to form a silica film in contact with the PVP film, thereby forming a stack structure having the silica film formed on the PVP film that is, in turn, formed on the substrate, wherein the PVP film is an adhesion promoting layer facilitating deposition of the silica film on the substrate,
wherein the substrate is glass having a refractive index being 1.5, the PVP film has a refractive index being 1.48 and a thickness of 200 nm, and the silica film has a refractive index being 1.23 and a thickness of 120-300 nm, such that the stack structure has an average transmittance of greater than 98% in the wavelength range of 450-1050 nm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the PVP film dissolves in the silica solution of the silica film as the silica film is formed on the PVP film.

### Claim 3 (depends on 1)

The method of claim 1, wherein each of the depositing steps (b) and (c) is performed by a dip coating, spray coating, or roll coating process, or any combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, further comprising drying the stack structure to form the antireflective coating on the substrate, wherein the antireflective coating comprises silica nanoparticles adhered on the surface of the substrate.

### Claim 5 (depends on 4)

The method of claim 4, wherein the drying step is performed at a temperature in a range of 10-1200° C.

### Claim 6 (depends on 1)

The method of claim 1, further comprising, prior to depositing the PVP solution, cleaning the substrate.

### Claim 7 (depends on 6)

The method of claim 6, wherein the cleaning step is performed by ultra-sonication.

### Claim 8

A method for forming an antireflective coating on a substrate, comprising:
(a) providing a polymer solution and a silica solution containing silica nanoparticles, wherein the silica solution consists of a colloidal silica solution diluted by deionized water so that the silica solution comprises 5 wt % of silica in a colloidal form;
(b) depositing the polymer solution directly on a surface of the substrate to form a polymer film in contact with the substrate; and
(c) depositing the silica solution directly on the formed polymer film on the substrate to form a silica film in contact with the polymer film, thereby forming a stack structure having the silica film formed on the polymer film that is, in turn, formed on the substrate, wherein the polymer film is an adhesion promoting layer facilitating deposition of the silica film on the substrate,
wherein the substrate is glass having a refractive index being 1.5;
wherein the polymer solution contains a transparent polymer having a refractive index, np, wherein the refractive index np of the transparent polymer is between the refractive index of air being 1 and a refractive index ns of the substrate being 1.5, and the polymer film has a refractive index being equal to, or less than the refractive index of the substrate being 1.5;
wherein the transparent polymer is selected from the group consisting of polyethylene, polystyrene, polypropylene, polysiloxanes, polyamide, and a combination of them; and
wherein the silica film has a refractive index being 1.23.

### Claim 9 (depends on 8)

The method of claim 8, wherein the transparent polymer is soluble in the solvent of the silica solution.

### Claim 10 (depends on 9)

The method of claim 9, wherein the polymer film dissolves in the silica solution of the silica film as the silica film is formed on the polymer film.

### Claim 11 (depends on 10)

The method of claim 10, wherein the silica nanoparticles are adhered on the surface of the substrate.

### Claim 12 (depends on 8)

The method of claim 8, wherein the transparent polymer is insoluble in the solvent of the silica solution.

### Claim 13 (depends on 12)

The method of claim 12, wherein the silica film of silica nanoparticles is formed from the silica solution on the transparent polymer film that is formed on the surface of the substrate and the silica nanoparticles are uniformly adhered on the polymer film.

### Claim 14 (depends on 8)

The method of claim 8, wherein the polymer solution has a concentration of the transparent polymer in a range of 1-20 wt %.

### Claim 15 (depends on 8)

The method of claim 8, wherein the polymer film has a thickness in a range of 5-300 nm.

### Claim 16 (depends on 8)

The method of claim 8, wherein the silica film has a thickness in a range of 5-300 nm.

### Claim 17 (depends on 8)

The method of claim 8, wherein each of the depositing steps (b) and (c) is performed by a dip coating, spray coating, or roll coating process, or any combination thereof.

### Claim 18 (depends on 8)

The method of claim 8, further comprising drying the stack structure.

### Claim 19 (depends on 18)

The method of claim 18, wherein the drying step is performed at a temperature in a range of 10-1200° C.

### Claim 20 (depends on 8)

The method of claim 8, further comprising, prior to depositing the polymer solution, cleaning the substrate.

### Claim 21 (depends on 20)

The method of claim 20, wherein the cleaning step is performed by ultra-sonication.