# US 11,121,152 B2 · Three-dimensional memory device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,152 B2
- Document ID: US11121152B2
- Status: Granted
- Kind: B2
- Application number: 16/679,265
- Filed: 2019-11-10
- Published: 2021-04-01
- Granted: 2021-09-14
- Earliest claimed: 2019-09-26
- Assignees: Yangtze Memory Technologies Co., Ltd.
- Applicants: Yangtze Memory Technologies Co., Ltd.
- Inventors: Qiguang Wang; Lei Jin; An Zhang; Jianwei Lu
- Web page: https://patentgrep.com/patent/US11121152B2

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- C23C 28/04: only coatings of inorganic non-metallic material
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- C23C 28/40: {Coatings including alternating layers following a pattern, a periodic or defined repetition}
- C23C 28/42: {characterized by the composition of the alternating layers}
- H10B 43/35: with cell select transistors, e.g. NAND
- H10D 30/693: {Vertical IGFETs having charge trapping gate insulators}
- H10D 30/694: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 64/037: {comprising charge-trapping insulators}
- H10D 64/516: {the thicknesses being non-uniform}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10B: ELECTRONIC MEMORY DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A three-dimensional (3D) memory device and a manufacturing method thereof are provided. The method includes the following steps. An alternating dielectric stack is formed on a substrate. An opening is formed penetrating the alternating dielectric stack in a thickness direction of the substrate. A blocking layer is formed on a sidewall of the opening. A trapping layer is formed in the opening, and the trapping layer is formed on the blocking layer. The trapping layer includes a lower portion and an upper portion disposed above the lower portion. A thickness of the upper portion in a horizontal direction is greater than a thickness of the lower portion in the horizontal direction. The thickness distribution of the trapping layer is modified for improving the electrical performance of the 3D memory device.

## Claims

### Claim 1

A manufacturing method of a three-dimensional (3D) memory device, comprising:
forming an alternating dielectric stack on a substrate,
forming an opening penetrating the alternating dielectric stack in a thickness direction of the substrate;
forming a blocking layer on a sidewall of the opening; and
forming a trapping layer in the opening, wherein the trapping layer is formed on the blocking layer, and the trapping layer comprises:
a lower portion; and
an upper portion disposed above the lower portion, wherein a thickness of the upper portion in a horizontal direction is greater than a thickness of the lower portion in the horizontal direction, and a material composition of the lower portion of the trapping layer is different from a material composition of the upper portion of the trapping layer.

### Claim 2 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein a ratio of the thickness of the upper portion in the horizontal direction to the thickness of the lower portion in the horizontal direction ranges from 1.25 to 2.

### Claim 3 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein the lower portion of the trapping layer is disposed between the upper portion of the trapping layer and the substrate in the thickness direction of the substrate.

### Claim 4 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein the horizontal direction is orthogonal to the thickness direction of the substrate.

### Claim 5 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein a top width of the opening is greater than a bottom width of the opening.

### Claim 6 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein a thickness of the trapping layer is gradually increased from the lower portion toward the upper portion.

### Claim 7 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein a forming method of the blocking layer comprises:
forming a base layer on the sidewall of the opening; and
performing an oxidation process to the base layer, wherein the base layer is oxidized by the oxidation process to be the blocking layer.

### Claim 8 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, further comprising:
forming a tunneling layer in the opening, wherein the tunneling layer is formed on the trapping layer in the opening; and
forming a semiconductor layer in the opening, wherein the semiconductor layer is elongated in the thickness direction of the substrate, and the semiconductor layer is surrounded by the tunneling layer, the trapping layer, and the blocking layer in the horizontal direction.

### Claim 9 (depends on 8)

The manufacturing method of the 3D memory device according to claim 8, further comprising:
forming a filling layer in the opening, wherein the filling layer is surrounded by the semiconductor layer, the tunneling layer, the trapping layer, and the blocking layer in the horizontal direction.

### Claim 10 (depends on 8)

The manufacturing method of the 3D memory device according to claim 8, wherein the alternating dielectric stack comprises dielectric layers and sacrificial layers alternately stacked in the thickness direction of the substrate, and the manufacturing method of the 3D memory device further comprises:
replacing the sacrificial layers with conductive layers so as to form an alternating conductive/dielectric stack after the step of forming the semiconductor layer.

### Claim 11 (depends on 1)

The manufacturing method of the 3D memory device according to claim 1, wherein a part of the lower portion of the trapping layer is removed for reducing the thickness of the lower portion of the trapping layer.

### Claim 12

A three-dimensional (3D) memory device, comprising:
a substrate;
an alternating conductive/dielectric stack disposed on the substrate;
an opening penetrating the alternating conductive/dielectric stack in a thickness direction of the substrate;
a blocking layer disposed in the opening and disposed on a sidewall of the opening; and
a trapping layer disposed in the opening and disposed on the blocking layer, wherein the trapping layer comprises:
a lower portion; and
an upper portion disposed above the lower portion, wherein a thickness of the upper portion in a horizontal direction is greater than a thickness of the lower portion in the horizontal direction, and a material composition of the lower portion of the trapping layer is different from a material composition of the upper portion of the trapping layer.

### Claim 13 (depends on 12)

The 3D memory device according to claim 12, wherein a ratio of the thickness of the upper portion in the horizontal direction to the thickness of the lower portion in the horizontal direction ranges from 1.25 to 2.

### Claim 14 (depends on 12)

The 3D memory device according to claim 12, wherein the lower portion of the trapping layer is disposed between the upper portion of the trapping layer and the substrate in the thickness direction of the substrate.

### Claim 15 (depends on 12)

The 3D memory device according to claim 12, wherein the horizontal direction is orthogonal to the thickness direction of the substrate.

### Claim 16 (depends on 12)

The 3D memory device according to claim 12, wherein a top width of the opening is greater than a bottom width of the opening.

### Claim 17 (depends on 12)

The 3D memory device according to claim 12, wherein a thickness of the trapping layer is gradually increased from the lower portion toward the upper portion.

### Claim 18 (depends on 12)

The 3D memory device according to claim 12, further comprising:
a semiconductor layer disposed in the opening and elongated in the thickness direction of the substrate, wherein the semiconductor layer is surrounded by the trapping layer in the horizontal direction; and
a tunneling layer disposed between the semiconductor layer and the trapping layer.