# US 11,121,045 B2 · Method for detecting ultra-small defect on wafer surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,045 B2
- Document ID: US11121045B2
- Status: Granted
- Kind: B2
- Application number: 16/691,180
- Filed: 2019-11-21
- Published: 2021-02-25
- Granted: 2021-09-14
- Earliest claimed: 2019-08-19
- Assignees: Shanghai Huali Microelectronics Corporation
- Applicants: Shanghai Huali Microelectronics Corporation
- Inventors: Xianghua Hu; Gaoyu Wang; Guangzhi He; Xiaofang Gu; Qiliang Ni
- Web page: https://patentgrep.com/patent/US11121045B2

## CPC

- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 50/73: {using masks for insulating materials}
- H10P 70/23: {during, before or after processing of insulating materials}
- H10P 74/235: {comprising optical enhancement of defects or not-directly-visible states}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a method for detecting an ultra-small defect on a wafer surface, film layer having ultra-small defect that causes abnormalities on the surface of the film layer; form a photoresist pattern with a pattern defect; etching the film layer according to the photoresist pattern to form a film layer pattern with an enlarged defect; and scanning the film layer pattern by using a defect scanner to capture the enlarged defect. In this method, enlarging the size of the ultra-fine particle defect through the exposure defocusing principle; or by adding the photomask consisting of the repeating units, using the repetition pattern as the exposure pattern and combing with the repeating cell to cell comparison method, the capture ability of the detection machine is further improved. Therefore, it can be detected by amplifying the defects of ultrafine particles which cannot be detected by conventional methods.

## Claims

### Claim 1

A method for detecting an ultra-small defect on a wafer surface, wherein the method at least comprises the following steps:
step 1: providing a substrate with a film layer on the surface, the upper surface of the film layer having an ultra-small defect that causes abnormalities on the surface of the film layer;
step 2: forming a photoresist layer on the upper surface of the film layer, and then exposing and developing the photoresist layer to form a photoresist pattern with a pattern defect;
step 3: etching the film layer according to the photoresist pattern to form a film layer pattern with an enlarged defect; and
step 4: scanning the film layer pattern by using a defect scanner to capture the enlarged defect.

### Claim 2 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein in step 1, the size of the ultra-small defect is 0.01 μm-0.2 μm.

### Claim 3 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein in step 2, the photoresist layer is exposed to form the enlarged pattern defect through a development defocusing principle.

### Claim 4 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein in step 2, the photoresist layer is exposed by using a photomask pattern consisting of repeating units.

### Claim 5 (depends on 4)

The method for detecting an ultra-small defect on a wafer surface according to claim 4, wherein the repeating units in the photomask used in exposure comprise a plurality of strip-shaped patterns with the same width and spacing.

### Claim 6 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein in step 2, the photoresist layer formed on the upper surface of the film layer is positive photoresist.

### Claim 7 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein in step 2, the photoresist layer formed on the upper surface of the film layer is negative photoresist.

### Claim 8 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein step 3 further comprises removing the residual photoresist on the surface of the film layer after etching the film layer.

### Claim 9 (depends on 8)

The method for detecting an ultra-small defect on a wafer surface according to claim 8, wherein a method for removing the residual photoresist on the surface of the film layer is wet removal.

### Claim 10 (depends on 8)

The method for detecting an ultra-small defect on a wafer surface according to claim 8, wherein a method for removing the residual photoresist on the surface of the film layer is dry removal.

### Claim 11 (depends on 1)

The method for detecting an ultra-small defect on a wafer surface according to claim 1, wherein the size of the enlarged defect is three times the size of the ultra-small defect.