# US 11,121,043 B2 · Fabrication of transistors having stressed channels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,043 B2
- Document ID: US11121043B2
- Status: Granted
- Kind: B2
- Application number: 16/230,192
- Filed: 2018-12-21
- Published: 2019-08-08
- Granted: 2021-09-14
- Earliest claimed: 2017-12-22
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Nicolas Posseme; Cyrille Le Royer; Yves Morand
- Web page: https://patentgrep.com/patent/US11121043B2

## CPC

- H10D 86/01: Manufacture or treatment
- C23C 14/0652: {Silicon nitride}
- C23C 14/48: Ion implantation
- C23C 16/345: {Silicon nitride}
- C23C 28/04: only coatings of inorganic non-metallic material
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/683: {carbon-based polymeric organic materials, e.g. polyimides, poly cyclobutene or PVC}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 30/40: into insulating materials
- H10P 32/1204: {from a plasma phase}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

There is provided a method for producing, on one same wafer, at least one first transistor surmounted at least partially on a voltage stressed layer and a second transistor surmounted at least partially on a compression stressed layer, the method including providing a wafer including the first and the second transistors; forming at least one stressed nitride-based layer, on the first and the second transistors, the layer being voltage stressed; depositing a protective layer so as to cover a first zone of the layer, the first zone covering at least partially the first transistor and leaving a second zone of the layer uncovered, the second zone at least partially covering the second transistor; and modifying a type of stress of the second zone of the layer by implanting hydrogen-based ions from a plasma in the second zone, such that the second zone of the layer is compression stressed.

## Claims

### Claim 1

A method for producing, on one same wafer, at least one first transistor surmounted at least partially on a tensile stressed layer and a second transistor surmounted at least partially on a compressive stressed layer, the method comprising:
providing a wafer comprising the at least one first transistor and the second transistor;
forming at least one stressed nitride-based layer, on the at least one first transistor and the second transistor, the stressed nitride-based layer being tensile stressed;
depositing a protective layer so as to cover a first zone of the stressed nitride-based layer, the first zone covering at least partially the at least one first transistor and leaving a second zone of the stressed nitride-based layer uncovered, the second zone at least partially covering the second transistor; and
modifying a type of stress of the second zone of the stressed nitride-based layer from a tensile stress to a compressive stress by implanting hydrogen-based ions from a plasma in the second zone, such that the second zone of the stressed nitride-based layer is compressive stressed, the modifying being performed without an exposure to ultraviolet radiation, without an exposure to a laser treatment, and without an exposure to an e-Beam treatment.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the depositing is performed so as to cover all of the at least one first transistor, and so as to leave the second transistor fully uncovered.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the at least one first transistor and the second transistor are of NMOS-type and PMOS-type, respectively.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein the at least one first transistor and the second transistor each have a channel and a gate oxide layer, and
wherein the at least one first transistor and the second transistor have different characteristics taken from among a different channel thickness and a different gate oxide thickness.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the plasma is formed from a mixture comprising at least one gas of the following gases: H2, HBr, and NH3.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a type of the plasma and an energy of the hydrogen-based ions are selected such that the implanting reduces a thickness of the stressed nitride-based layer in the second zone.

### Claim 7 (depends on 1)

The method according to claim 1,
wherein the protective layer comprises carbon, and
wherein the plasma is formed from a mixture comprising at least one gas of CxHy type, where x and y are whole numbers.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the plasma is formed from the mixture comprising the at least one gas of CxHy type, where x and y are whole numbers, and from at least one other gas of the following gases: helium (He) and argon (Ar).

### Claim 9 (depends on 1)

The method according to claim 1, wherein the forming of the at least one stressed nitride-based layer is performed such that said layer has a thickness of between 2 nm and 50 nm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the forming of the at least one stressed nitride-based layer is performed such that said layer has a thickness of between 5 nm and 40 nm.

### Claim 11 (depends on 1)

The method according to claim 1,
wherein the forming of the at least one stressed nitride-based layer comprises a conformal deposition, and
wherein the conformal deposition is performed by one of the following deposition techniques: plasma-enhanced chemical vapour deposition (PECVD), low-pressure enhanced chemical vapour deposition (LPCVD), rapid thermal chemical vapour deposition (RTCVD), and physical vapour deposition (PVD).

### Claim 12 (depends on 1)

The method according to claim 1, wherein implantation parameters, including an energy of the hydrogen-based ions, are selected so as to modify, by the implanting, all of a thickness of the second zone of the at least one stressed nitride-based layer.

### Claim 13 (depends on 1)

The method according to claim 1, wherein implantation parameters, including an energy of the hydrogen-based ions, are selected so as to modify, by the implanting, the second zone of the at least one stressed nitride-based layer, continuously from a surface of said layer to a depth of about 40 nm.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the implanting is performed at a temperature of ≤150° C.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the implanting is performed at a temperature of ≤100° C.

### Claim 16 (depends on 1)

The method according to claim 1,
wherein the first zone fully covers the at least one first transistor and the second zone fully covers the second transistor,
wherein an electrical insulation trench separates the at least one first transistor and the second transistor, and
wherein an interface defined by the first zone and the second zone is disposed so as to at least partially face the electrical insulation trench.

### Claim 17 (depends on 1)

The method according to claim 1, further comprising a plurality of sequences, each sequence of said plurality being applied on the at least one first transistor and the second transistor, and said each sequence comprising successively at least: the step of forming the at least one stressed nitride-based layer, the step of depositing the protective layer, and the step of modifying the type of stress.

### Claim 18 (depends on 17)

The method according to claim 17, wherein at said each sequence, the step of forming the at least one stressed nitride-based layer is configured such that a thickness of said layer is less than 20 nm.

### Claim 19 (depends on 17)

The method according to claim 17, wherein at said each sequence, the step of forming the at least one stressed nitride-based layer is configured such that a thickness of said layer is between 5 nm and 15 nm.

### Claim 20 (depends on 1)

The method according to claim 1,
wherein the at least one first transistor and the second transistor each have a channel formed in a semi-conductive layer, which surmounts a dielectric layer and a support substrate, and
wherein the semi-conductive layer, the dielectric layer, and the support substrate form a semi-conductor on insulator-type substrate, of FDSOI-type.

### Claim 21

A method for producing, on one same wafer, at least one first transistor surmounted at least partially on a tensile stressed layer and a second transistor surmounted at least partially on a compressive stressed layer, the method comprising:
providing a wafer comprising the at least one first transistor and the second transistor;
forming at least one stressed nitride-based layer, on the at least one first transistor and the second transistor, the stressed nitride-based layer being tensile stressed;
depositing a protective layer so as to cover a first zone of the stressed nitride-based layer, the first zone covering at least partially the at least one first transistor and leaving a second zone of the stressed nitride-based layer uncovered, the second zone at least partially covering the second transistor; and
modifying a type of stress of the second zone of the stressed nitride-based layer from a tensile stress to a compressive stress by implanting hydrogen-based ions from a plasma in the second zone, such that the second zone of the stressed nitride-based layer is compression stressed,
wherein the implanting is performed at a temperature of ≤150° C., and
wherein there is no post-implant annealing.