# US 11,121,027 B2 · High aspect ratio via etch using atomic layer deposition protection layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,027 B2
- Document ID: US11121027B2
- Status: Granted
- Kind: B2
- Application number: 16/213,628
- Filed: 2018-12-07
- Published: 2019-06-13
- Granted: 2021-09-14
- Earliest claimed: 2017-12-08
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Yen-Tien Lu; Xinghua Sun; Eric Chih-Fang Liu; Andrew W. Metz
- Web page: https://patentgrep.com/patent/US11121027B2

## CPC

- H10W 20/089: {using processes for implementing desired shapes or dispositions of the openings, e.g. double patterning}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/283: {by chemical means}
- H10P 50/73: {using masks for insulating materials}
- H10W 20/076: {in via holes or trenches}
- H10W 20/092: {by smoothing the dielectric parts}
- H10W 20/0765: {the thin functional dielectric layers being temporary, e.g. sacrificial layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for the via etching steps of a substrate manufacturing process flow is provided. The substrate processing techniques described provide for etching vias by providing a protection layer on the via sidewall during at least portions of the via etching process. In one embodiment, an atomic layer deposition (ALD) layer is formed on the via sidewalls to protect the dielectric layers through which the via is formed. The ALD layer may lessen bowing effects in low k dielectric layers which may result from etching barrier low k (blok) layers or from other process steps. After via formation, the ALD layer may be removed. The techniques are particularly suited for forming skip vias and other high aspect ratio vias formed in low k and ultra-low k dielectric layers.

## Claims

### Claim 1

A method for processing a substrate to form a via, comprising:
providing the substrate with a patterned layer having a via pattern;
providing at least a first low k dielectric layer underlying the patterned layer;
providing at least a first barrier layer underlying the first low k dielectric layer;
providing an organic planarization layer between the patterned layer and the first low k dielectric layer;
etching the first low k dielectric layer to form the via pattern in the first low k dielectric layer;
after etching the first low k dielectric layer, performing an atomic layer deposition process to deposit a protective layer on via sidewalls of the first low k dielectric layer, the atomic layer deposition process being separate from the etching the first low k dielectric layer step;
after performing the atomic layer deposition process, etching the first barrier layer, wherein the protective layer protects the via sidewalls of the first low k dielectric layer during the etching of the first barrier layer to limit bowing of the first low k dielectric layer; and
removing the organic planarization layer after etching the first barrier layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the via is a skip via.

### Claim 3 (depends on 1)

The method of claim 1, wherein the protective layer comprises a silicon oxide.

### Claim 4 (depends on 3)

The method of claim 3, wherein the first low k dielectric layer is a first ultra-low k dielectric layer.

### Claim 5 (depends on 4)

The method of claim 4, the first barrier layer is a nitrogen doped low k barrier layer.

### Claim 6 (depends on 5)

The method of claim 5, further comprising removing the protective layer after etching the first barrier layer.

### Claim 7

A method for processing a substrate to form a skip via, comprising:
providing the substrate with a patterned layer having a via pattern;
providing at least an upper low k dielectric layer underlying the patterned layer;
providing at least an upper barrier layer underlying the upper low k dielectric layer;
providing at least a lower low k dielectric layer underlying the upper barrier layer;
providing at least a lower barrier layer underlying the lower low k dielectric layer;
etching the upper low k dielectric layer to form the via pattern in the upper low k dielectric layer;
after etching the upper low k dielectric layer, performing a first atomic layer deposition (ALD) process to deposit a first protective layer on via sidewalls of the upper low k dielectric layer;
after performing the first ALD process, etching the upper barrier layer, wherein the first protective layer protects the via sidewalls of the upper low k dielectric layer during the etching of the upper barrier layer to limit bowing of the upper low k dielectric layer;
etching the lower low k dielectric layer to form the via pattern in the lower low k dielectric layer;
after etching the lower low k dielectric layer, performing a second atomic layer deposition (ALD) process to deposit a second protective layer on via sidewalls of the lower low k dielectric layer; and
after performing the second ALD process, etching the lower barrier layer, wherein the second protective layer protects the via sidewalls of the lower low k dielectric layer during the etching of the lower barrier layer to limit bowing of the lower low k dielectric layer.

### Claim 8 (depends on 7)

The method of claim 7, further comprising:
providing an organic planarization layer between the patterned layer and the upper low k dielectric layer; and
removing the organic planarization layer before performing the first ALD process.

### Claim 9 (depends on 7)

The method of claim 7, further comprising:
providing an organic planarization layer between the patterned layer and the upper low k dielectric layer; and
removing the organic planarization layer after etching the lower barrier layer.

### Claim 10 (depends on 7)

The method of claim 7, wherein the first protective layer and the second protective layer comprise silicon oxide.

### Claim 11 (depends on 10)

The method of claim 10, wherein the upper low k dielectric layer is an upper ultra-low k dielectric layer and the lower low k dielectric layer is a lower ultra-low k dielectric layer.

### Claim 12 (depends on 11)

The method of claim 11, the upper barrier layer is an upper low k barrier layer and the lower barrier layer is a lower low k barrier layer.

### Claim 13 (depends on 12)

The method of claim 12, further comprising removing the first protective layer and the second protective layer after the etching the lower barrier layer.

### Claim 14 (depends on 7)

The method of claim 7, further comprising removing the first protective layer and the second protective layer after the etching the lower barrier layer.

### Claim 15

A method of patterning a substrate, the method comprising:
providing the substrate with a via patterned structure, the patterned structure having an organic planarization layer (OPL), a hard mask layer, a first ultra-low K (ULK) layer, a first nitrogen doped low k barrier (nblok) layer, a second ULK layer, a second nblok layer, and an underlying layer;
performing a first ULK layer etching process;
performing a first atomic layer deposition oxide deposition to form a first atomic layer deposition oxide layer;
performing a first nblok etching process, the first atomic layer deposition oxide layer protecting at least portions of the first ULK layer during the first nblok etching process;
performing a second ULK layer etching process;
performing a second atomic layer deposition oxide deposition to form a second atomic layer deposition oxide layer;
performing a second nblok etching process, the second atomic layer deposition oxide layer protecting at least portions of the second ULK layer during the second nblok etching process; and
performing an atomic layer deposition oxide removal process.

### Claim 16 (depends on 15)

The method of claim 15, further comprising:
removing the OPL before performing the first atomic layer deposition oxide deposition.

### Claim 17 (depends on 15)

The method of claim 15, further comprising:
removing the OPL after performing the second nblok etching process.

### Claim 18 (depends on 15)

The method of claim 15, wherein the first atomic layer deposition oxide layer prevents bowing of the first ULK layer during the first nblok etching process and the second atomic layer deposition oxide layer prevents bowing of the second ULK layer during the second nblok etching process.

### Claim 19 (depends on 18)

The method of claim 18, wherein the method of patterning a substrate is utilized to form a skip via.