# US 11,121,024 B2 · Tunable hardmask for overlayer metrology contrast

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,024 B2
- Document ID: US11121024B2
- Status: Granted
- Kind: B2
- Application number: 16/542,502
- Filed: 2019-08-16
- Published: 2019-12-05
- Granted: 2021-09-14
- Earliest claimed: 2018-01-04
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Ekmini A. De Silva; Nelson Felix; Indira Seshadri; Stuart A. Sieg
- Web page: https://patentgrep.com/patent/US11121024B2

## CPC

- H10W 10/10: Isolation regions comprising dielectric materials
- G03F 7/70633: {Overlay, i.e. relative alignment between patterns printed by separate exposures in different layers, or in the same layer in multiple exposures or stitching}
- G03F 9/7076: {Mark details, e.g. phase grating mark, temporary mark}
- G03F 9/7084: {Position of mark on substrate, i.e. position in (x, y, z) of mark, e.g. buried or resist covered mark, mark on rearside, at the substrate edge, in the circuit area, latent image mark, marks in plural levels}
- H10P 76/202: {for lift-off processes}
- H10W 10/018: {using selective deposition of crystalline silicon, e.g. using epitaxial growth of silicon}
- H10W 20/01: {Manufacture or treatment}
- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- H10W 72/50: Bond wires
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 40/00: Manufacture or treatment of nanostructures
- H10W 46/301: {for alignment}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A tunable amorphous silicon layer for use with multilayer patterning stacks can be used to maximize transparency and minimize reflections so as to improve overlay metrology contrast. By increasing the hydrogen content in the amorphous silicon layer, the extinction coefficient (k) value and the refractive index (n) value can be decreased to desired values. Methods for improving overlay metrology contrast with the tunable amorphous silicon layer are disclosed.

## Claims

### Claim 1

A method of improving overlay metrology contrast, the method comprising:
forming at least one alignment feature in a dielectric oxide layer;
removing a portion of the dielectric oxide layer;
depositing, in a deposition chamber, an amorphous silicon layer on the dielectric oxide layer corresponding to the removed portion;
varying hydrogen content in the deposition chamber such that the amorphous silicon layer comprises hydrogen; and
depositing a multilayer patterning stack overlaying the amorphous silicon layer, wherein transmission of visible light from the multilayer patterning stack to the alignment feature is increased relative to not removing the portion of the dielectric oxide layer and depositing the amorphous silicon layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the amorphous silicon has an extinction coefficient (k) within a range of 0.4 to 0.03 at a wavelength of 633 nm and a refractive index (n) within a range of 4.1 to 3.2.

### Claim 3 (depends on 1)

The method of claim 1, wherein the amorphous silicon has an extinction coefficient (k) within a range of 0.09 to 0.03 at a wavelength of 633 nm and a refractive index (n) within a range of 3.5 to 3.2.

### Claim 4 (depends on 1)

The method of claim 1, wherein depositing the amorphous silicon layer comprises a vapor deposition process from a gas mixture comprising silane and hydrogen gas at a temperature within a range of about 30° C. to about 600° C. and a pressure within a range of about 0.1 Torr to about 10 Torr.

### Claim 5 (depends on 4)

The method of claim 4, wherein the hydrogen gas is greater than 10 mol % of the gas mixture and further reduces the extinction coefficient k value within a range from about 0.09 to about 0.03 and the refractive index value within a range of about 3.5 to about 3.2.

### Claim 6 (depends on 1)

The method of claim 1, wherein the amorphous silicon has an extinction coefficient (k) within a range of about 0.09 to about 0.03 at a wavelength of 633 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein depositing the amorphous silicon layer in the removed portion of the dielectric oxide layer comprises varying a hydrogen content in the amorphous silicon to reduce an extinction coefficient (k) at a wavelength of 633 nm and a refractive index (n) of the amorphous silicon.

### Claim 8 (depends on 1)

The method of claim 1, wherein depositing the amorphous silicon layer comprises a vapor deposition process from a gas mixture comprising silane at a temperature within a range of about 30° C. to about 600° C. and a pressure within a range of about 0.1 Torr to about 10 Torr to form the amorphous silicon layer; and doping the amorphous silicon layer with hydrogen to reduce the extinction coefficient (k) of the amorphous silicon within a range of about 0.4 to about 0.03 at a wavelength of 633 nm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the multilayer patterning stack comprises an organic planarizing layer, a hardmask on the organic planarizing layer, and a photoresist on the hardmask layer.

### Claim 10

A method of improving overlay metrology contrast, the method comprising:
forming at least one alignment feature in a dielectric oxide layer;
depositing an amorphous silicon layer on the dielectric oxide layer, wherein the depositing of the amorphous silicon layer comprises varying hydrogen content in a deposition chamber such that the amorphous silicon layer comprises hydrogen and is tuned to minimize reflection and maximize transmission; and
depositing a multilayer patterning stack on the tuned amorphous silicon layer, wherein the transmission of visible light from the multilayer patterning stack to the alignment feature is increased relative to not depositing the amorphous silicon layer.

### Claim 11 (depends on 10)

The method of claim 10, depositing an amorphous silicon layer in the removed portion of the dielectric oxide layer, wherein depositing the amorphous silicon comprises increasing a hydrogen content during deposition of the amorphous silicon layer to simultaneously reduce an extinction coefficient (k) at a wavelength of 633 nm and a refractive index (n) of the amorphous silicon.

### Claim 12 (depends on 10)

The method of claim 10, wherein the multilayer patterning stack comprises an organic planarizing layer, a hardmask on the organic planarizing layer, and a photoresist on the hardmask layer.

### Claim 13 (depends on 10)

The method of claim 10, wherein the amorphous silicon layer has a thickness within a range from about 5 nanometers to about 10 nanometers.

### Claim 14 (depends on 10)

The method of claim 10, wherein depositing the amorphous silicon layer comprises a vapor deposition process from a gas mixture comprising silane and hydrogen gas at a temperature within a range of about 30° C. to about 600° C. and a pressure within a range of about 0.1 Torr to about 10 Torr.

### Claim 15 (depends on 14)

The method of claim 14, wherein the hydrogen gas is greater than 10 mol % of the gas mixture and further reduces the extinction coefficient k value to within a range from about 0.09 to about 0.03 and the refractive index value to within a range of about 3.5 to about 3.2.

### Claim 16 (depends on 12)

The method of claim 12, wherein the multilayer patterning stack further comprises an adhesion layer, an antireflective layer or a combination thereof.

### Claim 17

A method for tuning an amorphous silicon layer, the method comprising:
depositing an amorphous silicon layer under a multilayer patterning stack, wherein tuning the amorphous silicon layer comprises increasing hydrogen content in the amorphous silicon to simultaneously provide the amorphous silicon with an extinction coefficient (k) value within a range of about 0.4 to about 0.03 at a wavelength of about 633 nm and a refractive index of the amorphous silicon within a range of from about 4.1 to about 3.2.

### Claim 18 (depends on 17)

The method of claim 17, wherein increasing the hydrogen content in the amorphous silicon is in an amount effective to reduce the extinction coefficient (k) value to within a range from about 0.09 to about 0.03 and the refractive index (n) to within about 3.5 to about 3.2.

### Claim 19 (depends on 17)

The method of claim 17, wherein depositing the amorphous silicon layer comprises a vapor deposition process selected from the group consisting of chemical vapor deposition, plasma enhanced chemical vapor deposition, and plasma vapor deposition from a silane gas.

### Claim 20 (depends on 17)

The method of claim 17, wherein depositing the amorphous silicon layer comprises a vapor deposition process from a gas mixture comprising a silane gas and a hydrogen gas at a temperature within a range of about 30° C. to about 600° C. and a pressure within a range of about 0.1 Torr to about 10 Torr.