# US 11,121,000 B2 · Etching method and substrate processing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,121,000 B2
- Document ID: US11121000B2
- Status: Granted
- Kind: B2
- Application number: 16/983,229
- Filed: 2020-08-03
- Published: 2021-02-11
- Granted: 2021-09-14
- Earliest claimed: 2019-08-09
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Seiichi Watanabe; Hiroki Yamada; Manabu Sato
- Web page: https://patentgrep.com/patent/US11121000B2

## CPC

- H10P 50/283: {by chemical means}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 50/73: {using masks for insulating materials}
- H10B 43/50: characterised by the boundary region between the core and peripheral circuit regions
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

There is provision of a method for etching a substrate above which a first underlying film, a second underlying film positioned deeper than the first underlying film, a silicon oxide film formed on the first and second underlying films, and a mask on the silicon oxide film are provided. In the mask, first and second openings are formed above the first and second underlying films respectively. After the first underlying film is exposed by etching the silicon oxide film using a first gas, the silicon oxide film is etched by using a second gas while depositing deposits on the first underlying film, and the silicon oxide film is etched by using a third gas while removing the deposits on the first underlying film. The etching using the second gas and the etching using the third gas are repeated multiple times.

## Claims

### Claim 1

A method comprising:
a) preparing a substrate above which a first underlying film, a second underlying film formed at a deeper location than the first underlying film, a silicon oxide film formed on the first underlying film and the second underlying film, and a mask formed on the silicon oxide film are provided, the mask having a first opening formed above the first underlying film and a second opening formed above the second underlying film;
b) etching the silicon oxide film above the first underlying film and the second underlying film by using a first gas, thereby exposing the first underlying film;
c) etching the silicon oxide film above the second underlying film by using a second gas, while depositing deposits on the first underlying film;
d) etching the silicon oxide film above the second underlying film by using a third gas, while removing the deposits on the first underlying film; and
e) repeating step c) and step d) a plurality of times.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
the third gas contains a first CF-containing gas and oxygen gas; and
the second gas contains a second CF-containing gas different from the first CF-containing gas, and oxygen gas.

### Claim 3 (depends on 2)

The method according to claim 2, wherein a C/F ratio of the second CF-containing gas is smaller than a C/F ratio of the first CF-containing gas.

### Claim 4 (depends on 2)

The method according to claim 2, wherein an adsorption coefficient of the second CF-containing gas in a predetermined temperature range is smaller than an adsorption coefficient of the first CF-containing gas in the predetermined temperature range.

### Claim 5 (depends on 2)

The method according to claim 2, wherein the first CF-containing gas is C4F6, and the second CF-containing gas is C3F8.

### Claim 6 (depends on 2)

The method according to claim 2, wherein a C/O ratio of the third gas is smaller than 1.3, and a C/O ratio of the second gas is equal to or greater than 1.3.

### Claim 7 (depends on 2)

The method according to claim 2, wherein a flow rate of the oxygen gas contained in the second gas is less than a flow rate of the oxygen gas contained in the third gas.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the predetermined temperature range is between 110° C. and 160° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first underlying film and the second underlying film are formed of tungsten.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the first underlying film and the second underlying film are formed of silicon.

### Claim 11 (depends on 1)

The method according to claim 1, wherein a time for etching the silicon oxide film by using the second gas is shorter than a time for etching the silicon oxide film by using the third gas.

### Claim 12 (depends on 1)

The method according to claim 1, wherein step e) is performed before the second underlying film is exposed.

### Claim 13 (depends on 12)

The method according to claim 12, wherein
a third underlying film is further formed above the substrate, at a deeper location than the second underlying film;
the silicon oxide film is formed on the third underlying film; and
the method further includes
f) etching the silicon oxide film above the third underlying film by using the second gas, while depositing the deposits on the first underlying film and the second underlying film;
g) etching the silicon oxide film above the third underlying film by using the third gas, while removing the deposits on the first underlying film and the second underlying film; and
h) repeating step f) and step g) a plurality of times, after the second underlying film is exposed and before the third underlying film is exposed.

### Claim 14 (depends on 13)

The method according to claim 13, wherein
the third gas contains a first CF-containing gas and oxygen gas; and
the second gas contains a second CF-containing gas different from the first CF-containing gas, and oxygen gas.

### Claim 15 (depends on 14)

The method according to claim 14, wherein a C/F ratio of the second CF-containing gas is smaller than a C/F ratio of the first CF-containing gas.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the first CF-containing gas is C4F6, and the second CF-containing gas is C3F8.

### Claim 17 (depends on 16)

The method according to claim 16, wherein a flow rate of the oxygen gas contained in the second gas is less than a flow rate of the oxygen gas contained in the third gas.

### Claim 18 (depends on 17)

The method according to claim 17, wherein a C/O ratio of the third gas is smaller than 1.3, and a C/O ratio of the second gas is equal to or greater than 1.3.

### Claim 19 (depends on 18)

The method according to claim 18, wherein a time for etching the silicon oxide film by using the second gas is shorter than a time for etching the silicon oxide film by using the third gas.