# US 11,120,922 B2 · Method for producing solidified radioactive waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,120,922 B2
- Document ID: US11120922B2
- Status: Granted
- Kind: B2
- Application number: 16/308,619
- Filed: 2017-06-22
- Published: 2019-05-23
- Granted: 2021-09-14
- Earliest claimed: 2016-06-23
- Assignees: Nippon Chemical Industrial Co., Ltd.
- Applicants: Nippon Chemical Industrial Co., Ltd.
- Inventors: Yutaka Kinose; Shinsuke Miyabe
- Web page: https://patentgrep.com/patent/US11120922B2

## CPC

- G21F 9/12: by absorption; by adsorption; by ion-exchange
- B01J 20/0211: {Compounds of Ti, Zr, Hf}
- B01J 20/041: {Oxides or hydroxides}
- B01J 20/10: comprising silica or silicate
- G21F 9/305: {Glass or glass like matrix (C03B5/005 takes precedence; compositional aspects C03C)}
- G21F 9/308: {by melting the waste (G21F9/305, G21F9/32 take precedence)}
- B01J 2220/42: Materials comprising a mixture of inorganic materials (materials coated or impregnated on a carrier B01J20/32)
- G21F: PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR (radiation protection by pharmaceutical means A61K8/00, A61Q17/04; in cosmonautic vehicles B64G1/54; combined with a reactor G21C11/00; combined with X-ray tubes H01J35/16; combined with X-ray apparatus H05G1/02)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The present invention provides solidified radioactive waste into which a titanium-containing adsorbent having a radioactive element adsorbed thereto is vitrified, the solidified radioactive waste being capable of confining a large amount of the titanium-containing adsorbent having a radioactive element adsorbed thereto, and furthermore elution of the radioactive element from the vitrified waste being suppressed. The method of the present application includes a step of heat-melting a mixture that includes a titanium-containing adsorbent having a radioactive element adsorbed thereto, a SiO2 source, and an M2O source (M represents an alkali metal element) to form vitrified waste. The titanium-containing adsorbent is preferably one or two or more kind such as silicotitanate, an alkali nonatitanate, and titanium hydroxide.

## Claims

### Claim 1

A method for producing solidified radioactive waste, comprising heat-melting a mixture that comprises a titanium-containing adsorbent having a radioactive element adsorbed thereto, a SiO2 source, and an M2O source (M represents an alkali metal element) to form vitrified waste,
wherein the SiO2 source and the M2O source are each an alkali silicate.

### Claim 2 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein the titanium-containing adsorbent is one or two or more selected from the group consisting of silicotitanate, an alkali nonatitanate, and titanium hydroxide.

### Claim 3 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein the radioactive element is cesium and/or strontium.

### Claim 4 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein the alkali silicate is an anhydride.

### Claim 5 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein the alkali silicate is sodium metasilicate.

### Claim 6

A method for producing solidified radioactive waste, comprising heat-melting a mixture that comprises a titanium-containing adsorbent having a radioactive element adsorbed thereto, a SiO2 source, and an M2O source (M represents an alkali metal element) to form vitrified waste,
wherein the mixture comprises at least M2O: 15 to 35% by mass, TiO2: 25 to 50% by mass, and SiO2: 15 to 35% by mass.

### Claim 7 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein a melt-heating temperature is 1000° C. or more.

### Claim 8 (depends on 1)

The method for producing solidified radioactive waste according to claim 1, wherein the mixture further comprises a metal oxide source comprising one or two or more metal elements selected from the group consisting of Zr, Al, Nb, Zn, Ca, and Mg.