# US 11,119,399 B2 · Mask blank, phase shift mask and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,119,399 B2
- Document ID: US11119399B2
- Status: Granted
- Kind: B2
- Application number: 15/760,265
- Filed: 2016-09-08
- Published: 2018-09-06
- Granted: 2021-09-14
- Earliest claimed: 2015-09-18
- Assignees: Hoya Corporation
- Applicants: Hoya Corporation
- Inventors: Atsushi Matsumoto; Hiroaki Shishido; Takashi Uchida
- Web page: https://patentgrep.com/patent/US11119399B2

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- G03F 1/20: Masks or mask blanks for imaging by charged particle beam [CPB] radiation, e.g. by electron beam; Preparation thereof
- G03F 1/38: Masks having auxiliary features, e.g. special coatings or marks for alignment or testing; Preparation thereof
- G03F 1/42: Alignment or registration features, e.g. alignment marks on the mask substrates
- G03F 1/48: Protective coatings
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G03F 1/80: Etching
- H10P 76/4085: {characterised by the processes involved to create the masks}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

According to the present invention, provided is a mask blank (10), in which: a light shielding film (4) has a single layer structure or a laminate structure of a plurality of layers; at least one layer of the light shielding film (4) is formed of a material which contains a transition metal and silicon and is free from nitrogen and oxygen, or a material which contains a transition metal, silicon, and nitrogen and satisfies a condition of the following expression (1); a phase shift film (2) has a surface layer and a layer other than the surface layer; and the layer other than the surface layer is formed of a material which contains a transition metal, silicon, nitrogen, and oxygen, has a content of oxygen of 3 atom % or more, and satisfies a condition of the following expression (A). CN≤9.0×10−6×RM4−1.65×10−4×RM3−7.718×10−2×RM2+3.611×RM−21.084 Expression (1) 0.04×AS−0.06×AM>1 Expression (A)

## Claims

### Claim 1

A mask blank comprising:
a transparent substrate;
a phase shift film on the transparent substrate;
an etching stopper film on the phase shift film; and
a light shielding film on the etching stopper film,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (A):
(0.04×AS)−(0.06×AM)>1 Expression (A)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, and where AS represents a content [atom %] of silicon in the layer other than the surface layer.

### Claim 2 (depends on 1)

The mask blank according to claim 1, wherein a content of oxygen in the surface layer of the phase shift film is larger than a content of oxygen in the layer other than the surface layer.

### Claim 3 (depends on 1)

The mask blank according to claim 1, wherein a multilayer structure comprises the phase shift film, the etching stopper film, and the light shielding film and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 4 (depends on 1)

The mask blank according to claim 1, further comprising a hard mask film on the light shielding film, the hard mask film comprising chromium.

### Claim 5 (depends on 1)

The mask blank according to claim 1, wherein the etching stopper film essentially consists of silicon and oxygen.

### Claim 6 (depends on 1)

The mask blank according to claim 1, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 7 (depends on 1)

The mask blank according to claim 1, wherein a content of oxygen in the upper layer is 10 atom % or more.

### Claim 8

A mask blank comprising:
a transparent substrate;
a phase shift film on the transparent substrate;
an etching stopper film on the phase shift film; and
a light shielding film on the etching stopper film,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (B):
(0.04×AS)−(0.06×AM)−(0.03×AN)>1 Expression (B)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, AS represents a content [atom %] of silicon in the layer other than the surface layer, and AN represents a content [atom %] of nitrogen in the layer other than the surface layer.

### Claim 9 (depends on 8)

The mask blank according to claim 8, wherein a content of oxygen in the surface layer of the phase shift film is larger than a content of oxygen in the layer other than the surface layer.

### Claim 10 (depends on 8)

The mask blank according to claim 8, wherein a multilayer structure comprises the phase shift film, the etching stopper film, and the light shielding film and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 11 (depends on 8)

The mask blank according to claim 8, further comprising a hard mask film on the light shielding film, the hard mask film comprising chromium.

### Claim 12 (depends on 8)

The mask blank according to claim 8, wherein the etching stopper film essentially consists of silicon and oxygen.

### Claim 13 (depends on 8)

The mask blank according to claim 8, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 14 (depends on 8)

The mask blank according to claim 8, wherein a content of oxygen in the upper layer is 10 atom % or more.

### Claim 15

A mask blank comprising:
a transparent substrate;
a phase shift film on the transparent substrate;
an etching stopper film on the phase shift film; and
a light shielding film on the etching stopper film,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (C):
(0.04×AS)−(0.06×AM)−(0.03×AN)+(0.02×AO)>0 Expression (C)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, AS represents a content [atom %] of silicon in the layer other than the surface layer, AN represents a content [atom %] of nitrogen in the layer other than the surface layer, and AO represents a content [atom %] of oxygen in the layer other than the surface layer.

### Claim 16 (depends on 15)

The mask blank according to claim 15, wherein a content of oxygen in the surface layer of the phase shift film is larger than a content of oxygen in the layer other than the surface layer.

### Claim 17 (depends on 15)

The mask blank according to claim 15, wherein a multilayer structure comprises the phase shift film, the etching stopper film, and the light shielding film and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 18 (depends on 15)

The mask blank according to claim 15, further comprising a hard mask film on the light shielding film, the hard mask film comprising chromium.

### Claim 19 (depends on 15)

The mask blank according to claim 15, wherein the etching stopper film essentially consists of silicon and oxygen.

### Claim 20 (depends on 15)

The mask blank according to claim 15, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 21 (depends on 15)

The mask blank according to claim 15, wherein a content of oxygen in the upper layer is 10 atom % or more.

### Claim 22

A phase shift mask comprising:
a transparent substrate;
a phase shift film pattern on the transparent substrate;
an etching stopper film pattern on the phase shift film pattern; and
a light shielding film pattern on the etching stopper film pattern,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film pattern has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (A):
(0.04×AS)−(0.06×AM)>1 Expression (A)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, and where AS represents a content [atom %] of silicon in the layer other than the surface layer.

### Claim 23 (depends on 22)

The phase shift mask according to claim 22, wherein a content of oxygen in the surface layer of the phase shift film pattern is larger than a content of oxygen in the layer other than the surface layer.

### Claim 24 (depends on 22)

The phase shift mask according to claim 22, wherein a multilayer structure comprises the phase shift film pattern, the etching stopper film pattern, and the light shielding film pattern and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 25 (depends on 22)

A method of manufacturing a semiconductor device, comprising transferring a transfer pattern on a resist film formed on a transfer substrate by placing the phase shift mask of claim 22 in an exposure apparatus comprising an exposure light source configured to emit ArF excimer laser light.

### Claim 26 (depends on 22)

The phase shift mask according to claim 22, wherein the etching stopper film pattern essentially consists of silicon and oxygen.

### Claim 27 (depends on 22)

The phase shift mask according to claim 22, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 28 (depends on 22)

The phase shift mask according to claim 22, wherein a content of oxygen in the upper layer is 10 atom % or more.

### Claim 29

A phase shift mask comprising:
a transparent substrate;
a phase shift film pattern on the transparent substrate;
an etching stopper film pattern on the phase shift film pattern; and
a light shielding film pattern on the etching stopper film pattern,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film pattern has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (B):
(0.04×AS)−(0.06×AM)−(0.03×AN)>1 Expression (B)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, AS represents a content [atom %] of silicon in the layer other than the surface layer, and AN represents a content [atom %] of nitrogen in the layer other than the surface layer.

### Claim 30 (depends on 29)

The phase shift mask according to claim 29, wherein a content of oxygen in the surface layer of the phase shift film pattern is larger than a content of oxygen in the layer other than the surface layer.

### Claim 31 (depends on 29)

The phase shift mask according to claim 29, wherein a multilayer structure comprises the phase shift film pattern, the etching stopper film pattern, and the light shielding film pattern and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 32 (depends on 29)

A method of manufacturing a semiconductor device, comprising transferring a transfer pattern on a resist film formed on a transfer substrate by placing the phase shift mask of claim 29 in an exposure apparatus comprising an exposure light source configured to emit ArF excimer laser light.

### Claim 33 (depends on 29)

The phase shift mask according to claim 29, wherein the etching stopper film pattern essentially consists of silicon and oxygen.

### Claim 34 (depends on 29)

The phase shift mask according to claim 29, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 35 (depends on 29)

The phase shift mask according to claim 29, wherein a content of oxygen in the upper layer is 10 atom % or more.

### Claim 36

A phase shift mask comprising:
a transparent substrate;
a phase shift film pattern on the transparent substrate;
an etching stopper film pattern on the phase shift film pattern; and
a light shielding film pattern on the etching stopper film pattern,
wherein the etching stopper film contains silicon and oxygen, and
wherein the light shielding film has a lower layer and an upper layer formed on the lower layer, and
wherein the lower layer contains a transition metal, silicon, and nitrogen and satisfies the following expression (1):
CN≤(9.0×10−6×RM4)−(1.65×10−4×RM3)−(7.718×10−2×RM2)+(3.611×RM)−21.084 Expression (1)
where RM represents a ratio [%] of a content [atom %] of the transition metal to a total content [atom %] of the transition metal and silicon in the at least one layer and where CN [atom %] represents a content [atom %] of nitrogen in the at least one layer, and
wherein the upper layer contains a transition metal, silicon, oxygen and nitrogen, and
wherein a total content of nitrogen and oxygen in the upper layer is 30 atom % or more, and
wherein a content of transition metal in the upper layer is less than 10 atom %, and
wherein the phase shift film pattern has a surface layer and a layer other than the surface layer having a different composition than the surface layer, and
wherein the layer other than the surface layer contains a transition metal, silicon, nitrogen, and oxygen; has a content of oxygen of 3 atom % or more; and satisfies the following expression (A):
(0.04×AS)−(0.06×AM)−(0.03×AN)+(0.02×AO)>0 Expression (C)
where AM represents a content [atom %] of the transition metal in the layer other than the surface layer, AS represents a content [atom %] of silicon in the layer other than the surface layer, AN represents a content [atom %] of nitrogen in the layer other than the surface layer, and AO represents a content [atom %] of oxygen in the layer other than the surface layer.

### Claim 37 (depends on 36)

The phase shift mask according to claim 36, wherein a content of oxygen in the surface layer of the phase shift film pattern is larger than a content of oxygen in the layer other than the surface layer.

### Claim 38 (depends on 36)

The phase shift mask according to claim 36, wherein a multilayer structure comprises the phase shift film pattern, the etching stopper film pattern, and the light shielding film pattern and has an optical density for ArF excimer laser light of at least 2.7.

### Claim 39 (depends on 36)

A method of manufacturing a semiconductor device, comprising transferring a transfer pattern on a resist film formed on a transfer substrate by placing the phase shift mask of claim 36 in an exposure apparatus comprising an exposure light source configured to emit ArF excimer laser light.

### Claim 40 (depends on 36)

The phase shift mask according to claim 36, wherein the etching stopper film pattern essentially consists of silicon and oxygen.

### Claim 41 (depends on 36)

The phase shift mask according to claim 36, wherein a content of oxygen in the lower layer is 5 atom % or less.

### Claim 42 (depends on 36)

The phase shift mask according to claim 36, wherein a content of oxygen in the upper layer is 10 atom % or more.