# US 11,119,146 B1 · Testing of bonded wafers and structures for testing bonded wafers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,119,146 B1
- Document ID: US11119146B1
- Status: Granted
- Kind: B1
- Application number: 16/997,630
- Filed: 2020-08-19
- Granted: 2021-09-14
- Earliest claimed: 2020-08-19
- Assignees: Xilinx, Inc.
- Applicants: Xilinx, Inc.
- Inventors: Nui Chong; Yan Wang; Hui-Wen Lin
- Web page: https://patentgrep.com/patent/US11119146B1

## CPC

- G01R 31/2853: {Electrical testing of internal connections or -isolation, e.g. latch-up or chip-to-lead connections (G01R31/31717 takes precedence; test of chip-to-PCB or lead-to-PCB connections G01R31/66)}
- H10P 74/207: {Electrical properties, e.g. testing or measuring of resistance, deep levels or capacitance-voltage characteristics}
- H10P 74/273: {Interconnections for measuring or testing, e.g. probe pads}
- H10P 74/277: {Circuits for electrically characterising or monitoring manufacturing processes, e.g. circuits in tested chips or circuits in testing wafers}
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Examples described herein generally relate to testing of bonded wafers and structures implemented for such testing. In an example method, power is applied to a first pad on a stack of bonded wafers. A wafer of the stack includes a process control monitor (PCM) region that includes structure regions. Each structure region is a device under test region, dummy region, and/or chain interconnect region (CIR). The stack includes a serpentine chain test structure (SCTS) electrically connected between first and second metal features in the wafer in first and second CIRs, respectively, in the PCM region. The SCTS includes segments, one or more of which are disposed between neighboring structure regions in the PCM region that are not the first and second CIRs. A signal is detected from a second pad on the stack. The first and second pads are electrically connected to the first and second metal features, respectively.

## Claims

### Claim 1

A method for testing, the method comprising:
applying power to a first pad on a stack of bonded wafers, a first wafer of the stack of bonded wafers including a first process control monitor region, the first process control monitor region including first structure regions in the first wafer, each first structure region of the first structure regions being a device under test region, a dummy region, a chain interconnect region, or a combination thereof, the stack of bonded wafers including a first serpentine chain test structure electrically connected between a first metal feature in the first wafer in a first chain interconnect region in the first process control monitor region and a second metal feature in the first wafer in a second chain interconnect region in the first process control monitor region, the first serpentine chain test structure including first segments, one or more segments of the first segments being disposed between neighboring first structure regions in the first process control monitor region that are not the first chain interconnect region and the second chain interconnect region, the first pad being electrically connected to the first metal feature; and
detecting a first signal from a second pad on the stack of bonded wafers, the second pad being electrically connected to the second metal feature, the first signal being a response of, at least in part, the first serpentine chain test structure to the applied power.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first structure regions are arranged in an array, the first chain interconnect region and the second chain interconnect region being disposed in a same row of the array, the one or more segments of the first segments being disposed between first structure regions that are in neighboring columns of the array and that are in one or more rows of the array different from the row of the array in which the first chain interconnect region and the second chain interconnect region are disposed.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first serpentine chain test structure includes serially connected through-substrate vias (TSVs) disposed in a semiconductor substrate of the first wafer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first serpentine chain test structure includes serially connected through-substrate vias (TSVs) disposed in a semiconductor substrate of a second wafer bonded to the first wafer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first serpentine chain test structure includes first bond pads on the first wafer and second bond pads on a second wafer bonded to the first wafer, ones of the first bond pads being bonded to respective ones of the second bond pads, bonded pairs of the first bond pads and the second bond pads being serially connected.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first serpentine chain test structure includes:
first bond pads on the first wafer and second bond pads on a second wafer bonded to the first wafer, ones of the first bond pads being bonded to respective ones of the second bond pads; and
through-substrate vias (TSVs) disposed in a semiconductor substrate of the first wafer or the second wafer, the TSVs and bonded pairs of the first bond pads and the second bond pads being serially connected.

### Claim 7 (depends on 1)

The method of claim 1, wherein:
a first metal stack extends from the first pad across the stack of bonded wafers, the first metal feature in the first wafer being in the first metal stack; and
a second metal stack extends from the second pad across the stack of bonded wafers, the second metal feature in the first wafer being in the second metal stack.

### Claim 8 (depends on 1)

The method of claim 1 further comprising detecting a second signal from a third pad on the stack of bonded wafers, the stack of bonded wafers including a second wafer distinct from the first wafer, the second wafer including a second process control monitor region, the second process control monitor region including second structure regions in the second wafer, each second structure region of the second structure regions being a device under test region, a dummy region, a chain interconnect region, or a combination thereof, the stack of bonded wafers including a second serpentine chain test structure electrically connected between a third metal feature in the second wafer in a third chain interconnect region in the second process control monitor region and a fourth metal feature in the second wafer in a fourth chain interconnect region in the second process control monitor region, the second serpentine chain test structure including second segments, one or more segments of the second segments being disposed between respective neighboring second structure regions in the second process control monitor region that are not the third chain interconnect region and the fourth chain interconnect region, the first pad being electrically connected to the third metal feature, the third pad being electrically connected to the fourth metal feature, the second signal being a response of, at least in part, the second serpentine chain test structure to the applied power.

### Claim 9 (depends on 8)

The method of claim 8, wherein:
a first metal stack extends from the first pad across the stack of bonded wafers, the first metal feature in the first wafer and the third metal feature in the second wafer each being in the first metal stack;
a second metal stack extends from the second pad across the stack of bonded wafers, the second metal feature in the first wafer being in the second metal stack; and
a third metal stack extends from the third pad across the stack of bonded wafers, the fourth metal feature in the second wafer being in the third metal stack.

### Claim 10

A method for fabrication, the method comprising:
bonding a first wafer to a second wafer, the first wafer and the second wafer being included in a stack of bonded wafers, the first wafer including a process control monitor region, the process control monitor region including an array of structure regions, each structure region of the structure regions being a device under test region, a dummy region, a chain interconnect region, or a combination thereof, the stack of bonded wafers including a serpentine chain test structure electrically connected between a first metal feature in the first wafer in a first chain interconnect region in the process control monitor region and a second metal feature in the first wafer in a second chain interconnect region in the process control monitor region, the first chain interconnect region being in a first row of the array, the second chain interconnect region being in a second row of the array, the serpentine chain test structure including segments, one or more segments of the segments being disposed laterally between respective structure regions that are in neighboring columns of the array and that are outside of the first row and the second row; and
testing the stack of bonded wafers, the testing including:
applying power to a first pad on the stack of bonded wafers, the first pad being electrically connected to the first metal feature; and
detecting a signal from a second pad on the stack of bonded wafers, the second pad being electrically connected to the second metal feature, the signal being a response of, at least in part, the serpentine chain test structure to the applied power.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first row and the second row are a same row of the array.

### Claim 12 (depends on 10)

The method of claim 10, wherein the serpentine chain test structure includes serially connected through-substrate vias (TSVs) disposed in a semiconductor substrate of the first wafer.

### Claim 13 (depends on 10)

The method of claim 10, wherein the serpentine chain test structure includes serially connected through-substrate vias (TSVs) disposed in a semiconductor substrate of the second wafer.

### Claim 14 (depends on 10)

The method of claim 10, wherein the serpentine chain test structure includes first bond pads on the first wafer and second bond pads on the second wafer, ones of the first bond pads being bonded to respective ones of the second bond pads, bonded pairs of the first bond pads and the second bond pads being serially connected.

### Claim 15 (depends on 10)

The method of claim 10, wherein the serpentine chain test structure includes:
first bond pads on the first wafer and second bond pads on the second wafer, ones of the first bond pads being bonded to respective ones of the second bond pads; and
through-substrate vias (TSVs) disposed in a semiconductor substrate of the first wafer or the second wafer, the TSVs and bonded pairs of the first bond pads and the second bond pads being serially connected.

### Claim 16 (depends on 10)

The method of claim 10 further comprising, after testing the stack of bonded wafers, singulating a multi-die stack from the stack of bonded wafers.

### Claim 17

A method for testing, the method comprising:
applying power to a first pad on a stack of bonded wafers, the stack of bonded wafers including a process control monitor region, the process control monitor region including an array of structure regions, each structure region of the structure regions being a device under test region, a dummy region, a chain interconnect region, or a combination thereof, the stack of bonded wafers including a serpentine chain test structure electrically connected between a first chain interconnect region in the array of the process control monitor region and a second chain interconnect region in the array of the process control monitor region, the serpentine chain test structure including serially connected segments, one or more segments of the segments being disposed in a region between neighboring structure regions that are in different columns in the array and that are in a row of the array different from a row in which the first chain interconnect region or the second chain interconnect region is disposed, the first pad being electrically connected to the first chain interconnect region; and
detecting a signal from a second pad on the stack of bonded wafers, the second pad being electrically connected to the second chain interconnect region, the signal being a response of, at least in part, the serpentine chain test structure to the applied power.

### Claim 18 (depends on 17)

The method of claim 17, wherein the serpentine chain test structure includes serially connected through-substrate vias (TSVs) disposed in a semiconductor substrate of the stack of bonded wafers.

### Claim 19 (depends on 17)

The method of claim 17, wherein the serpentine chain test structure includes bonded pairs of pads at a bonding interface in the stack of bonded wafers, the bonded pairs of pads being serially connected.

### Claim 20 (depends on 17)

The method of claim 17, wherein the serpentine chain test structure includes:
through-substrate vias (TSVs) disposed in a semiconductor substrate of the stack of bonded wafers; and
bonded pairs of pads at a bonding interface in the stack of bonded wafers, the TSVs and the bonded pairs of pads being serially connected.