# US 11,119,066 B2 · Room temperature nitrogen dioxide gas sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,119,066 B2
- Document ID: US11119066B2
- Status: Granted
- Kind: B2
- Application number: 16/000,438
- Filed: 2018-06-05
- Published: 2019-12-05
- Granted: 2021-09-14
- Earliest claimed: 2018-06-05
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Qasem Ahmed Drmosh; Zain Hassan Yamani; Amar Kamal Mohamedkhair; Abdulmajeed Hasan Hendi; Mohammad Kamal Hossain; Abdullatif Mohammed Albaseer
- Web page: https://patentgrep.com/patent/US11119066B2

## CPC

- G01N 27/127: {comprising nanoparticles}
- G01N 33/0037: {NOx}
- Y02A 50/20: Air quality improvement or preservation, e.g. vehicle emission control or emission reduction by using catalytic converters
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- Y02A: TECHNOLOGIES FOR ADAPTATION TO CLIMATE CHANGE

## Abstract

A room temperature nitrogen dioxide gas sensor comprising tin(IV) oxide decorated with gold nanoparticles is described. The tin(IV) oxide may have an average layer thickness of 10-1,000 nm, and is topped with dispersed gold nanoparticles having an average longest dimension of 200-650 nm. The room temperature nitrogen dioxide gas sensor may be used to detect and measure levels of nitrogen dioxide gas at room temperature and at concentrations of 100 ppb-1800 ppm, with a high stability. A method of making the room temperature nitrogen dioxide sensor is also described, and involves sputtering to deposit a tin(IV) oxide layer and a gold layer on a substrate, followed by annealing.

## Claims

### Claim 1

A room temperature nitrogen dioxide gas sensor, comprising:
at least two electrodes on a substrate, the electrodes separated by 100-500 μm;
a SnO2 layer in contact with the at least two electrodes on the substrate; and
gold nanoparticles dispersed on the SnO2 layer, the gold nanoparticles having an average longest dimension of 250-650 nm,
wherein the substrate has a planar side with a surface area of 0.5-10 cm2,
wherein the gold nanoparticles consist essentially of gold and are elongated with an aspect ratio in a range of 1.20:1-4:1,
wherein the gold nanoparticles have an average nearest neighbor distance of 250-500 nm, and
wherein the SnO2 layer consists essentially of SnO2 and has an average thickness of 10 nm-1,000 nm.

### Claim 2 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, further comprising smaller gold nanoparticles on the SnO2 layer, the smaller gold nanoparticles having an average longest dimension of 10-160 nm.

### Claim 3 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, wherein the gold nanoparticles are dispersed on the SnO2 layer at a surface density of 2×105-2×1015 gold nanoparticles per m2.

### Claim 4 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, further comprising a computing device configured to transmit a data measurement.

### Claim 5 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, wherein the SnO2 is polycrystalline, having an average grain size in a range of 6-10 nm.

### Claim 6 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, wherein the substrate has a surface roughness RMS in a range of 20-50 nm.

### Claim 7 (depends on 1)

The room temperature nitrogen dioxide gas sensor of claim 1, wherein the at least two electrodes have an average thickness of 200-400 nm and comprise graphene.

### Claim 8 (depends on 1)

A method of determining a concentration of nitrogen dioxide gas with the room temperature nitrogen dioxide gas sensor of claim 1, wherein the room temperature nitrogen dioxide gas sensor further comprises a computing device connected to the at least two electrodes,
the method comprising:
contacting the gold nanoparticles with a first gas sample substantially free of nitrogen dioxide gas and measuring a first resistivity across the at least two electrodes;
contacting the gold nanoparticles with a second gas sample comprising a concentration of nitrogen dioxide gas and measuring a second resistivity across the at least two electrodes;
determining a response factor, which is the percentage difference of the first resistivity to the second resistivity, relative to the second resistivity; and
calculating the concentration of nitrogen dioxide gas in the second gas sample based on the response factor,
wherein the determining and calculating are performed by the computing device.

### Claim 9 (depends on 8)

The method of claim 8, wherein during the second contacting, the second gas sample comprises 100 ppb-1800 ppm nitrogen dioxide gas.

### Claim 10 (depends on 8)

The method of claim 8, wherein during the first contacting, the first gas sample comprises 300-12,000 ppm of at least one gas selected from the group consisting of H2, NH3, CO2, n-butane, pentane, pentene, O2, and N2.

### Claim 11 (depends on 8)

The method of claim 8, wherein during the second contacting, the second resistivity has a response time of 30-180 s.

### Claim 12 (depends on 8)

The method of claim 8, wherein during the first contacting, the first gas sample comprises 0.1-99 vol % of at least one gas selected from the group consisting of O2, CO2, H2O, Ar, and N2, relative to a total volume of the first gas sample, or the first gas sample consists essentially of O2, CO2, H2O, Ar, and/or N2.

### Claim 13 (depends on 8)

The method of claim 8, wherein during the second contacting, the room temperature nitrogen dioxide gas sensor is located in a neonatal intensive care unit.

### Claim 14 (depends on 8)

The method of claim 8, further comprising transmitting the response factor by the computing device.

### Claim 15 (depends on 8)

The method of claim 8, which has a repeatability of at least 99% in determining the concentration of nitrogen dioxide gas in the second gas sample.

### Claim 16 (depends on 8)

The method of claim 8, wherein during the first contacting, the first gas sample has a temperature of 0-50° C. and a pressure of 0.9-1.1 atm.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first gas sample has a temperature of 20-37° C.

### Claim 18

A method of making a room temperature nitrogen dioxide gas sensor, wherein the room temperature nitrogen gas sensor comprises:
at least two electrodes on a substrate, the electrodes separated by 100-500 μm;
a SnO2 layer in contact with the at least two electrodes on the substrate; and
gold nanoparticles dispersed on the SnO2 layer, the gold nanoparticles having an average longest dimension of 250-650 nm,
wherein the substrate has a planar side with a surface area of 0.5-10 cm2,
wherein the gold nanoparticles consist essentially of gold and are elongated with an aspect ratio in a range of 1.20:1-4:1,
wherein the gold nanoparticles have an average nearest neighbor distance of 250-500 nm, and
wherein the SnO2 layer consists essentially of SnO2 and has an average thickness of 10 nm-1,000 nm,
the method comprising:
sputtering SnO2 onto the at least two electrodes on the substrate to produce a SnO2 layer;
sputtering gold onto the SnO2 layer to produce a gold layer; and
annealing the SnO2 layer and the gold layer at 450-650° C. to produce the room temperature nitrogen dioxide gas sensor.

### Claim 19 (depends on 18)

The method of claim 18, wherein the gold nanoparticles are not contacted with a surfactant or a template.

### Claim 20 (depends on 18)

The method of claim 18, wherein for a wavelength in a range of 350-1,000 nm, the SnO2 layer with the gold layer before the annealing has a transmittance of 0.00-0.15, and
wherein for the same wavelength, the room temperature nitrogen dioxide gas sensor has a transmittance of 0.40-0.55.