- Number: US 11,118,314 B2
- Document ID: US11118314B2
- Status: Granted
- Kind: B2
- Application number: 17/236,426
- Filed: 2021-04-21
- Published: 2021-08-05
- Granted: 2021-09-14
- Earliest claimed: 2019-08-05
- Assignees: Intpro, LLC
- Applicants: Intpro, LLC
- Inventors: Herbert B. Kohler
- Web page: https://patentgrep.com/patent/US11118314B2

## CPC

- D21H 27/34: Continuous materials, e.g. filaments, sheets, nets
- B31F 1/28: combined with uniting the corrugated webs to flat webs {; Making double-faced corrugated cardboard}
- B31F 1/284: {Warp prevention}
- B31F 1/2845: {Details, e.g. provisions for drying, moistening, pressing}
- B32B 29/005: {next to another layer of paper or cardboard layer}
- B32B 29/08: Corrugated paper or cardboard
- B32B 37/20: involving the assembly of continuous webs only
- B32B 41/00: Arrangements for controlling or monitoring lamination processes; Safety arrangements
- D21F 7/003: {Indicating or regulating the moisture content of the layer}
- D21F 9/02: of the Fourdrinier type
- D21F 11/04: paper or board consisting on two or more layers
- D21H 17/28: Starch
- D21H 19/54: Starch
- D21H 27/40: at least one of the sheets being non-planar, e.g. crêped (crêping or corrugating paper B31F)
- B31F 1/2804: {Methods}
- B32B 2250/26: All layers being made of paper or paperboard
- B32B 2255/12: on paper layer
- B32B 2255/26: Polymeric coating
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- B31F: MECHANICAL WORKING OR DEFORMATION OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUS TO PAPER (making layered products not composed wholly of paper or cardboard B32B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- D21F: PAPER-MAKING MACHINES; METHODS OF PRODUCING PAPER THEREON

## Abstract

A network-based system and method for providing desired moisture set point values for individual papers lines based on the physical properties of each liner and the atmospheric conditions associated with a corrugator is disclosed. The desired moisture set point values are based on the hygroexpansivity of each individual paper liner. Once the moisture set point value has been determined, a conditioning apparatus adjusts a moisture value for each liner in order to tune the post-warp characteristics of the final corrugated product.

## Claims

### Claim 1

A method of conditioning a traveling web, comprising:
a. assigning a first hygroexpansivity attribute value to a first liner to be used in making a corrugated composite;
b. determining a first moisture setpoint value for the first liner based on the first hygroexpansivity attribute value; and
c. conditioning the first liner by applying a first thin film of a liquid to the first liner to adjust its moisture content based on the first moisture setpoint value,
thereafter heating the first liner and then bonding the first liner to a first side of a fluted medium, wherein the moisture adjustments in said first liner followed by heating thereof yields a first hygroexpansivity therein such that the corrugated product exhibits no more than 5% relative deflection in a radius of curvature thereof at 24 hours after being made from said first liner and said fluted medium.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
aggregating in a data storage a plurality of respective corrugator input data sets relative to conditions prevalent and/or feedstock materials used at respective corrugators, wherein said data sets have been correlated with respective hygroexpansivity attribute values representative of hygroexpansivities of paper webs;
receiving specific corrugator input data comprising data relating to the first liner from a specific corrugator for making the corrugated composite;
comparing the specific corrugator input data against the aggregated data sets in said data storage and identifying or calculating therefrom the first hygroexpansivity attribute value representative of hygroexpansivity behavior of said first liner;
the first moisture setpoint value being determined in step (b) to adjust the moisture content in the first liner to be within a first range of greater than 10 wt. % and up to 30 wt. %; and
transmitting said first moisture setpoint value to said specific corrugator for use in making said corrugated composite.

### Claim 3 (depends on 2)

The method of claim 2, each said corrugator input data set comprising data values pertaining to any or all of: (i) relative humidity, (ii) temperature, (iii) pressure, (iv) composition content of the feedstock materials, and (v) moisture content of the feedstock materials.

### Claim 4 (depends on 3)

The method of claim 3, said specific corrugator input data further comprising data relating to a second liner used or to be used at said specific corrugator for making said specific corrugated composite; the method further comprising:
identifying or calculating, via comparison of the specific corrugator input data against said aggregated data sets, a second hygroexpansivity attribute value representative of hygroexpansivity behavior of said second liner;
based on said second hygroexpansivity attribute value, determining a second moisture setpoint value for said second liner calculated to adjust a moisture content therein to be within a second range of greater than 10 wt. % and up to 30 wt. %; and
transmitting said second moisture setpoint value to said specific corrugator for use in making said specific corrugated composite.

### Claim 5 (depends on 4)

The method of claim 4, wherein said first and second moisture setpoint values are calculated to yield respective cooperating hygroexpansivities in the first and second liners such that the corrugated composite made therefrom will exhibit no more than 5% relative deflection in a radius of curvature thereof at 24 hours after being made.

### Claim 6 (depends on 4)

The method of claim 4, said first range being 11 wt. % to 15 wt. %.

### Claim 7 (depends on 2)

The method of claim 2, wherein said specific corrugator input data is added to and aggregated with said plurality of corrugator input data sets in said data storage and correlated with hygroexpansivity attribute values.

### Claim 8 (depends on 2)

The method of claim 2, said plurality of corrugators being competitors with one another, their respective data sets aggregated in said data storage being anonymized such that the competitors are unaware of what, whether, or when any particular data set came from any particular competitor.

### Claim 9 (depends on 2)

The method of claim 2, wherein the first hygroexpansivity attribute value is calculated based on multivariate statistical process control.

### Claim 10 (depends on 2)

The method of claim 2, said first range being 11 wt. % to 15 wt. %.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
d. assigning a second hygroexpansivity attribute value to a second liner to be used in making the corrugated composite;
e. determining a second moisture setpoint value for the second liner based on the second hygroexpansivity attribute value; and
f. conditioning the second liner by applying a second thin film of a liquid to the second liner to adjust its moisture content based on the second moisture setpoint value.

### Claim 12 (depends on 11)

The method of claim 11, said first and second moisture setpoint values being selected so that once said corrugated composite is made, the first and second liners therein have substantially matched hygroexpansivities.

### Claim 13 (depends on 1)

The method of claim 1, wherein the moisture content of the first liner is adjusted to a first range of greater than 10 wt. % and up to 30 wt. %.

### Claim 14 (depends on 1)

The method of claim 1, wherein the moisture content of the first liner is adjusted to a first range of 11 wt. % to 15 wt. %.

### Claim 15 (depends on 1)

The method of claim 1, wherein the moisture adjustments in said first liner followed by heating thereof yields the first hygroexpansivity therein such that the corrugated product exhibits no more than 1% relative deflection in the radius of curvature thereof at 24 hours after being made from said first liner and said fluted medium.