# US 11,118,278 B2 · Enhanced plating bath and additive chemistries for cobalt plating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,278 B2
- Document ID: US11118278B2
- Status: Granted
- Kind: B2
- Application number: 16/656,026
- Filed: 2019-10-17
- Published: 2020-02-13
- Granted: 2021-09-14
- Earliest claimed: 2016-02-26
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Ismail Emesh; Roey Shaviv; Chris Pabelico
- Web page: https://patentgrep.com/patent/US11118278B2

## CPC

- C25D 3/18: Heterocyclic compounds
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Implementations of the disclosure may include methods of electroplating features formed on a semiconductor device, such as the trenches and vias formed by single or dual Damascene processes using a cobalt plating bath. The cobalt electroplating bath may contain “additive packages” or “additive systems” that include a combination of additives in certain ratios that facilitate the metal filling of high aspect ratio sub-micrometer features. Implementations of the disclosure provide new cobalt plating bath methods and chemistries and that include alkyl modified imidazoles, imidazolines, and imidazolidines suppressor compounds.

## Claims

### Claim 1

A method of forming a cobalt layer on a substrate, comprising:
immersing a substrate having a conductive layer disposed thereon in a cobalt plating bath, wherein the cobalt plating bath comprises:
a first amount of a cobalt ion; and
a first amount of at least one suppressor compound comprising an imidazole, imidazoline, or imidazolidine group, and wherein the imidazole, imidazoline, or imidazolidine group comprises an alkyl group; and
biasing the conductive layer relative to an anode that is in electrical communication with the cobalt plating bath and the conductive layer to form a cobalt layer on a surface of the conductive layer, wherein the alkyl group is an oligomeric or polymeric polypropylene glycol group.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polypropylene glycol group is of a molecular weight from between about 100 g/mole to about 30,000 g/mole.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cobalt plating bath has a pH of between about 5 and about 7.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first amount of the cobalt ion is introduced into the cobalt plating bath in the form of a cobalt sulfamate solution or a cobalt glycine complex containing solution, wherein a concentration of the cobalt ion in the cobalt plating bath is between about 0.001 moles/L and 0.25 moles/L.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first amount of the cobalt ion is introduced into the cobalt plating bath in the form of the cobalt sulfamate solution.

### Claim 6 (depends on 1)

The method of claim 1, wherein the cobalt plating bath further comprises a first amount of boric acid.

### Claim 7 (depends on 1)

The method of claim 1, wherein the imidazole, imidazoline, or imidazolidine group comprising the polypropylene glycol group has the structure:
wherein the R group comprises the polypropylene glycol group.

### Claim 8 (depends on 1)

The method of claim 1, wherein the imidazole, imidazoline, or imidazolidine group comprising the polypropylene glycol group has the structure:
wherein the R group comprises the polypropylene glycol group.

### Claim 9 (depends on 1)

The method of claim 1, wherein the imidazole, imidazoline, or imidazolidine group comprising the polypropylene glycol group has the structure:
wherein the R group comprises the polypropylene glycol group.

### Claim 10 (depends on 1)

The method of claim 1, wherein the substrate has a feature coated with the conductive layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the conductive layer is a conductive seed layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the cobalt plating bath has a pH of at least 5.

### Claim 13 (depends on 11)

The method of claim 11, wherein the conductive seed layer comprises a material selected from cobalt, copper, manganese, doped copper, ruthenium, or a combination thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the feature is a trench having an opening of 30 nanometers or less.

### Claim 15 (depends on 10)

The method of claim 10, wherein the first amount of the cobalt ion is from between about 0.001 moles/L and about 0.25 moles/L and the first amount of the suppressor compound is from between about 10 parts per million and about 1000 parts per million.

### Claim 16 (depends on 15)

The method of claim 15, wherein the cobalt plating bath further comprises a first amount of boric acid.

### Claim 17 (depends on 10)

The method of claim 10, wherein the imidazole, imidazoline, or imidazolidine group comprising the polypropylene glycol group has the structure:
wherein the R group comprises the polypropylene glycol group.

### Claim 18 (depends on 1)

The method of claim 1, wherein the substrate has a feature coated with a barrier layer and the barrier layer is coated with the conductive layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the conductive layer is a conductive seed layer and the conductive seed layer comprises a material selected from cobalt, copper, manganese, doped copper, ruthenium, or a combination thereof.

### Claim 20 (depends on 18)

The method of claim 18, wherein the barrier layer is a TiN layer or a TaN layer and the conductive layer is a cobalt seed layer.