# US 11,118,266 B2 · Method for depositing protection film of light-emitting element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,266 B2
- Document ID: US11118266B2
- Status: Granted
- Kind: B2
- Application number: 16/189,660
- Filed: 2018-11-13
- Published: 2019-03-14
- Granted: 2021-09-14
- Earliest claimed: 2016-05-18
- Assignees: Tes Co., Ltd
- Applicants: Tes Co., Ltd
- Inventors: Hong-Jae Lee; Jong-Hwan Kim; Woo-Pil Shim; Woo-Jin Lee; Sung-Yean Yoon; Don-Hee Lee
- Web page: https://patentgrep.com/patent/US11118266B2

## CPC

- C23C 16/345: {Silicon nitride}
- C23C 16/401: {containing silicon}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/45555: {applied in non-semiconductor technology}
- C23C 16/505: using radio frequency discharges
- H10H 20/01: Manufacture or treatment
- H10H 20/80: Constructional details
- H10H 20/81: Bodies
- H10H 20/84: Coatings, e.g. passivation layers or antireflective coatings
- H10K 59/8731: {multilayered coatings having a repetitive structure, e.g. having multiple organic-inorganic bilayers}
- H10H 20/034: {of coatings}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present invention relates to a method for depositing a protection film of a light-emitting element, the method comprising the steps of: depositing a first protection layer on a light-emitting element of a substrate by means of the atomic layer deposition method; and depositing at least one additional protection layer on the first protection layer by means of the plasma-enhanced chemical vapor deposition method.

## Claims

### Claim 1

A method of depositing a protection film for a light emitting diode (LED), the method comprising:
depositing a first protection layer on an LED substrate by atomic layer deposition (ALD);
depositing a second protection layer on the first protection layer by plasma enhanced chemical vapor deposition; and
depositing a third protection layer on the second protection layer by plasma enhanced chemical vapor deposition,
wherein internal stress of the first protection layer is greater than that of the second protection layer, and internal stress of the second protection layer is greater than that of the third protection layer, such that the internal stress is reduced upward from an upper surface of the LED, and
wherein depositing of the second protection layer and depositing of the third protection layer are continuously performed in a same chamber.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first protection layer is formed of an aluminum oxide (AlOx) layer deposited by ALD, the second protection layer is formed of silicon nitride (SiNx) deposited on the first protection layer by plasma enhanced chemical vapor deposition, and the third protection layer is formed of silicon oxide (SiOx) deposited on the second protection layer by plasma enhanced chemical vapor deposition.

### Claim 3 (depends on 2)

The method of claim 2, wherein, in the depositing of the first protection layer, a compound including aluminum (Al) is supplied as source gas and N2O is supplied as reaction gas.

### Claim 4 (depends on 2)

The method of claim 2, wherein, in the depositing of the second protection layer, silane (SiH4) gas is supplied as precursor gas, NH3 or N2 is supplied as reaction gas, and RF power density for plasma generation has a value of 0.34 to 0.58 W/cm2.

### Claim 5 (depends on 2)

The method of claim 2, wherein, in the depositing of the third protection layer, any one selected from an organic precursor group consisting of tetramethyl-disiloxane (TMDSO), hexaethyl-disilane (HEDS), hexamethyl-disiloxane (HMDSO), and bisdiethylamino-silane (BDEAS) is supplied, O2 or Ar is supplied as reaction gas, and RF power density for plasma generation has a value of 0.63 to 0.87 W/cm2.

### Claim 6 (depends on 2)

The method of claim 2, further comprising depositing a buffer layer on the third protection layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein the buffer layer is formed of silicon oxide including carbon.

### Claim 8 (depends on 7)

The method of claim 7, wherein the depositing of the buffer layer and the depositing of the third protection layer use the same organic precursor.

### Claim 9 (depends on 8)

The method of claim 8, wherein the depositing of the third protection layer and the depositing of the buffer layer are successively performed.

### Claim 10 (depends on 9)

The method of claim 9, wherein, as the depositing of the third protection layer proceeds to the depositing of the buffer layer, a supply amount of the reaction gas is relatively reduced while a supply amount of the organic precursor is relatively increased.

### Claim 11 (depends on 2)

The method of claim 2, wherein a thickness ratio of the second protection layer and the third protection layer is about 0.2 to 0.4:1.

### Claim 12 (depends on 2)

The method of claim 2, wherein a total thickness including the first to third protection layers is 60 to 200 nm.

### Claim 13 (depends on 2)

The method of claim 2, wherein the first protection layer has a thickness of 10 to 20 nm, the second protection layer has a thickness of 10 to 40 nm, and the third protection layer has a thickness of 40 to 140 nm.

### Claim 14 (depends on 2)

The method of claim 2, wherein, in the depositing of the first, second, and third protection layers, the first, second, and third protection layers have reduced internal stress upward from the LED.

### Claim 15 (depends on 1)