# US 11,118,265 B2 · Film deposition method and computer program storage medium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,265 B2
- Document ID: US11118265B2
- Status: Granted
- Kind: B2
- Application number: 15/811,919
- Filed: 2017-11-14
- Published: 2018-03-22
- Granted: 2021-09-14
- Earliest claimed: 2010-08-27
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Shigenori Ozaki; Hitoshi Kato; Takeshi Kumagai
- Web page: https://patentgrep.com/patent/US11118265B2

## CPC

- C23C 16/45548: {having arrangements for gas injection at different locations of the reactor for each ALD half-reaction}
- C23C 16/402: {Silicon dioxide}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A film deposition method includes steps of: placing a substrate in a substrate receiving area of a susceptor provided in a vacuum chamber; evacuating the vacuum chamber; alternately supplying plural kinds of reaction gases to the substrate in the substrate receiving area from corresponding reaction gas supplying parts thereby to form a thin film on the substrate; supplying plasma including a chemical component that reacts with second reaction gas adsorbed on the substrate from a plasma generation part to the substrate when the thin film is being formed, thereby to alter the thin film on the substrate; and changing plasma intensity of the plasma supplied to the substrate, at a predetermined point of time to a different plasma intensity of the plasma that is generated and supplied to the substrate by the plasma generation part before the predetermined point of time.

## Claims

### Claim 1

A film deposition method that forms a thin film on a substrate by repeating a cycle of alternately supplying plural kinds of reaction gases to the substrate under vacuum, wherein a first reaction gas among the plural kinds of the reaction gases reacts with a second reaction gas among the plural kinds of the reaction gases, the second reaction gas being adsorbed on the substrate, to produce a reaction product, the film deposition method comprising steps of:
placing a substrate in a substrate receiving area of a susceptor provided in a vacuum chamber;
evacuating the vacuum chamber;
alternately supplying plural kinds of the reaction gases to the substrate in the substrate receiving area from corresponding nozzles to form a thin film on the substrate;
supplying plasma including a chemical component that reacts with the second reaction gas adsorbed on the substrate from sheath pipes and electrodes to the substrate when the thin film is being formed, to alter the thin film on the substrate;
keeping plasma intensity of the plasma supplied to the substrate at zero until a thickness of the thin film reaches 1 nm; and
changing the plasma intensity of the plasma supplied to the substrate after the thickness of the thin film reaches 1 nm so as to increase the plasma intensity from a plasma intensity corresponding to the oxide film thickness of 1.5 nm to a plasma intensity corresponding to the oxide film thickness of 2 nm as a thickness of the reaction product is increased from 1 to 4 nm, keeping the plasma intensity zero when a thickness of the thin film is from 4 nm to 7 nm, and increasing the plasma intensity from a plasma intensity corresponding to the oxide film thickness of 3 nm to a plasma intensity corresponding to 5.3 nm as a thickness of the reaction product is increased from 7 nm to 10 nm,
wherein the film deposition method further includes predetermining a plasma intensity corresponding to an oxide film thickness of n nm by measuring at least one of the power supplied to an electrode pair, the inner pressure of the vacuum chamber, the exposure time of the plasma to the wafer, and the distance between the electrode pair that is required to generate the oxide film thickness of n nm by irradiating the plasma for 180 seconds.

### Claim 2 (depends on 1)

The film deposition method of claim 1, wherein the first reaction gas serves as an oxidizing or nitriding gas with respect to the second reaction gas adsorbed on the substrate, and
wherein the thin film is formed of one of metal oxide, silicon oxide metal nitride, and silicon nitride.

### Claim 3 (depends on 2)

The film deposition apparatus of claim 2, wherein an underlying film of the thin film to be formed thereon includes metal or silicon.

### Claim 4 (depends on 1)

The film deposition method of claim 1, wherein the plasma intensity is changed by adjusting an inner pressure in the vacuum chamber.

### Claim 5 (depends on 1)

The film deposition method of claim 1, wherein the susceptor is rotated around a vertical axis with respect to the plural nozzles arranged at predetermined intervals along a rotation direction of the susceptor so that the substrate receiving area of the susceptor passes alternately through areas to which the plural nozzles supply the corresponding reaction gases in the forming of the thin film,
wherein the plasma generated is supplied to the substrate in one of a first area to which the first reaction gas is supplied and a second area located downstream relative to the first area along a rotation direction of the susceptor in the altering of the thin film, and
the film deposition method further comprising supplying a separation gas to separation areas that are located between the areas to which the plural nozzles supply the corresponding reaction gases in order to separate the areas.

### Claim 6

A film deposition method that forms a thin film on a substrate by repeating a cycle of alternately supplying plural kinds of reaction gases to the substrate under vacuum, wherein a first reaction gas among the plural kinds of the reaction gases reacts with a second reaction gas among the plural kinds of the reaction gases, the second reaction gas being adsorbed on the substrate, to produce a reaction product, the film deposition method comprising steps of:
placing a substrate in a substrate receiving area of a susceptor provided in a vacuum chamber;
evacuating the vacuum chamber;
supplying the plural kinds of the reaction gases from corresponding nozzles toward the susceptor;
supplying plasma including a chemical component that reacts with one of the second reaction gas adsorbed on the substrate and at least a part of the substrate from sheath pipes and electrodes toward the susceptor; and
rotating the susceptor around a vertical axis so that the substrate receiving area passes alternately through a supplying area to which the second reaction gas is supplied, a reaction area where the first reaction gas reacts with the second reaction gas adsorbed on the substrate, and a plasma area that is arranged downstream relative to the reaction area along a rotation direction of the susceptor and where the plasma is supplied, wherein the supplying area, the reaction area, and the plasma area are arranged at intervals along a circumferential direction of the vacuum chamber,
wherein the method further comprises:
keeping plasma intensity of the plasma supplied to the substrate at zero until a thickness of the thin film reaches 1 nm; and
changing the plasma intensity of the plasma supplied to the substrate after the thickness of the thin film reaches 1 nm so as to increase the plasma intensity from a plasma intensity corresponding to the oxide film thickness of 1.5 nm to a plasma intensity corresponding to the oxide film thickness of 2 nm as a thickness of the reaction product is increased from 1 to 4 nm, keeping the plasma intensity zero when a thickness of the thin film is from 4 nm to 7 nm, and increasing the plasma intensity from a plasma intensity corresponding to the oxide film thickness of 3 nm to a plasma intensity corresponding to 5.3 nm as a thickness of the reaction product is increased from 7 nm to 10 nm,
wherein the film deposition method further includes predetermining a plasma intensity corresponding to an oxide film thickness of n nm by measuring at least one of the power supplied to an electrode pair, the inner pressure of the vacuum chamber, the exposure time of the plasma to the wafer, and the distance between the electrode pair that is required to generate the oxide film thickness of n nm by irradiating the plasma for 180 seconds.

### Claim 7 (depends on 1)

A computer readable storage medium that stores a computer program to be used in a film deposition apparatus that forms a thin film on a substrate by repeating a cycle of alternately supplying plural kinds of reaction gases to the substrate, the computer program including groups of instructions that cause the film deposition apparatus to perform the film deposition method of claim 1.