# US 11,118,260 B2 · Zirconium alloy cladding with improved oxidation resistance at high temperature and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,260 B2
- Document ID: US11118260B2
- Status: Granted
- Kind: B2
- Application number: 16/762,247
- Filed: 2018-11-14
- Published: 2020-09-10
- Granted: 2021-09-14
- Earliest claimed: 2017-11-14
- Assignees: Korea Atomic Energy Research Institute
- Applicants: Korea Atomic Energy Research Institute
- Inventors: Jung Hwan Park; Hyun Gil Kim; Yang Il Jung; Dong Jun Park; Byoung Kwon Choi; Young Ho Lee; Jae Ho Yang
- Web page: https://patentgrep.com/patent/US11118260B2

## CPC

- C22C 28/00: Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00
- C23C 14/16: on metallic substrates or on substrates of boron or silicon
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- C22C 16/00: Alloys based on zirconium
- C23C 14/32: by explosion; by evaporation and subsequent ionisation of the vapours {, e.g. ion-plating}(C23C14/34 - C23C14/48 take precedence)
- C23C 14/325: {Electric arc evaporation}
- G21C 3/07: characterised by their material, e.g. alloys
- C23C 14/00: Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C 14/22: characterised by the process of coating
- C23C 14/24: Vacuum evaporation
- Y02E 30/30: Nuclear fission reactors
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a zirconium alloy cladding with improved oxidation resistance at a high temperature and a method of manufacturing the same. More particularly, the zirconium alloy cladding includes a zirconium alloy cladding; and a Cr—Al thin film coated on the cladding, wherein the thin film is deposited through arc ion plating and the content of Al in the thin film is 5% by weight to 20% by weight.

## Claims

### Claim 1

A method of manufacturing a zirconium alloy cladding with improved oxidation resistance at a high temperature, the method comprising:
(a) manufacturing a target comprising Cr and Al; and
(b) depositing a Cr—Al thin film on a zirconium alloy cladding through arc ion plating in which a current and a bias voltage are applied to the target, wherein the content of Al in the target is 7% by weight to 23% by weight;
wherein, in step (b), the applied current is 30 A to 120 A and the applied bias voltage is 120 V to 400 V,
wherein, in step (b), a working pressure during the deposition is maintained at 5 mTorr to 20 mTorr, and
wherein an arithmetical average roughness (Ra) of the Cr—Al thin film deposited in step (b) is 5 μm or less.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in step (b), the deposition is performed at 200° C. to 300° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in step (b), the deposition is performed at a rate of 2 μm/h to 15 μm/h.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, after the zirconium alloy cladding and the Cr—Al thin film deposited in step (b) is-being oxidized at 1200° C. for 2,000 seconds under a steam atmosphere condition, a weight increase of the zirconium alloy cladding and the Cr—Al thin film deposited in step (b) ranges 1 mg/dm2 to 3,000 mg/dm2.