# US 11,118,252 B2 · Galvannealed steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,252 B2
- Document ID: US11118252B2
- Status: Granted
- Kind: B2
- Application number: 17/043,283
- Filed: 2018-03-30
- Published: 2021-02-18
- Granted: 2021-09-14
- Earliest claimed: 2018-03-30
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Kohichi Sano; Hiroyuki Kawata; Yuji Yamaguchi; Satoshi Uchida; Yoshinori Imai; Riki Okamoto
- Web page: https://patentgrep.com/patent/US11118252B2

## CPC

- C21D 9/48: deep-drawing sheets
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- B32B 15/043: {of metal (B32B15/01 takes precedence)}
- B32B 15/18: comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)}
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0257: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/0263: {following hot rolling}
- C21D 8/0426: {Hot rolling}
- C21D 8/0436: {Cold rolling}
- C21D 8/0447: {characterised by the heat treatment}
- C21D 8/0457: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/0463: {following hot rolling}
- C21D 8/0478: {involving a particular surface treatment (C21D8/0494 takes precedence)}
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0222: {in a reactive atmosphere, e.g. oxidising or reducing atmosphere (C23C2/024 takes precedence)}
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/26: After-treatment (C23C2/14 takes precedence)
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C23C 28/02: only coatings {only including layers} of metallic material
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/023: {only coatings of metal elements only}
- C23C 28/025: {with at least one zinc-based layer}
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C23C 30/005: {on hard metal substrates}
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2211/009: Pearlite
- Y02P 10/20: Recycling
- Y10T 428/12792: Zn-base component
- Y10T 428/12799: Next to Fe-base component [e.g., galvanized]
- Y10T 428/12951: Fe-base component
- Y10T 428/12958: Next to Fe-base component
- Y10T 428/12965: Both containing 0.01-1.7% carbon [i.e., steel]
- Y10T 428/12979: Containing more than 10% nonferrous elements [e.g., high alloy, stainless]
- Y10T 428/2495: Thickness [relative or absolute]
- Y10T 428/24959: of adhesive layers
- Y10T 428/24967: Absolute thicknesses specified
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- Y10T 428/263: Coating layer not in excess of 5 mils thick or equivalent
- Y10T 428/264: Up to 3 mils
- Y10T 428/265: 1 mil or less
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A steel sheet includes a hot-dip galvanized layer or a galvannealed layer on a surface of the steel sheet, the steel sheet including: in mass %, C: 0.06% or more and 0.22% or less; Si: 0.50% or more and 2.00% or less; Mn: 1.50% or more and 2.80% or less; Al: 0.02% or more and 1.00% or less; P: 0.001% or more and 0.100% or less; S: 0.0005% or more and 0.0100% or less; N: 0.0005% or more and 0.0100% or less; and a balance: Fe and impurities.

## Claims

### Claim 1

A galvannealed steel sheet comprising a galvannealed layer on a surface of the steel sheet,
the steel sheet having a component composition comprising: in mass %,
C: 0.06% or more and 0.22% or less;
Si: 0.50% or more and 2.00% or less;
Mn: 1.50% or more and 2.80% or less;
Al: 0.01% or more and 1.00% or less;
P: 0.001% or more and 0.100% or less;
S: 0.0005% or more and 0.0100% or less;
N: 0.0005% or more and 0.0100% or less;
Ti: 0% or more and 0.10% or less;
Mo: 0% or more and 0.30% or less;
Nb: 0% or more and 0.050% or less;
Cr: 0% or more and 1.00% or less;
B: 0% or more and 0.0050% or less;
V: 0% or more and 0.300% or less;
Ni: 0% or more and 2.00% or less;
Cu: 0% or more and 2.00% or less;
W: 0% or more and 2.00% or less;
Ca: 0% or more and 0.0100% or less;
Ce: 0% or more and 0.0100% or less;
Mg: 0% or more and 0.0100% or less;
Zr: 0% or more and 0.0100% or less;
La: 0% or more and 0.0100% or less;
REM: 0% or more and 0.0100% or less;
Sn: 0% or more and 1.000% or less;
Sb: 0% or more and 0.200% or less; and
a balance: Fe and impurities, wherein:
a microstructure of the steel sheet in a range of a ⅛ sheet thickness to a ⅜ sheet thickness centering on a ¼ sheet thickness in a sheet thickness direction from the surface of the steel sheet comprises, in area ratio, ferrite: 15% or more and 85% or less, retained austenite: less than 5%, martensite: 15% or more and 75% or less, perlite: 5% or less, and a balance (including 0%): bainite;
in a range of a ⅛ sheet thickness to a ⅜ sheet thickness centering on a ¼ sheet thickness in a sheet thickness direction from the surface of the steel sheet, a number of ferrite agglomerates in said range having a thickness in the sheet thickness direction of 20 μm or less is 50% or more of a total number of ferrite agglomerates in said range;
a decarburized layer having a thickness of 10 μm or more and 150 μm or less is formed in a surface layer part of the steel sheet;
a grain size of ferrite in the decarburized layer is 30 μm or less; and
a number density of martensite grains in the decarburized layer having an aspect ratio of 5 or more among martensite grains in the decarburized layer is 50% or less.

### Claim 2 (depends on 1)

The galvannealed steel sheet according to claim 1, wherein the component composition comprises one or two or more of: in mass %,
Ti: 0.01% or more and 0.10% or less;
Mo: 0.01% or more and 0.30% or less;
Nb: 0.005% or more and 0.050% or less;
Cr: 0.01% or more and 1.00% or less;
B: 0.0002% or more and 0.0050% or less;
V: 0.001% or more and 0.300% or less;
Ni: 0.01% or more and 2.00% or less;
Cu: 0.01% or more and 2.00% or less;
W: 0.01% or more and 2.00% or less;
Ca: 0.0001% or more and 0.0100% or less;
Ce: 0.0001% or more and 0.0100% or less;
Mg: 0.0001% or more and 0.0100% or less;
Zr: 0.0001% or more and 0.0100% or less;
La: 0.0001% or more and 0.0100% or less;
REM: 0.0001% or more and 0.0100% or less;
Sn: 0.001% or more and 1.000% or less; and
Sb: 0.001% or more and 0.200% or less.

### Claim 3 (depends on 1)

The galvannealed steel sheet according to claim 1, further comprising a fine-grain layer having an average thickness of 0.1 μm to 5.0 μm between the galvannealed layer and the decarburized layer.

### Claim 4 (depends on 3)

The galvannealed steel sheet according to claim 3, wherein the component composition comprises one or two or more of: in mass %,
Ti: 0.01% or more and 0.10% or less;
Mo: 0.01% or more and 0.30% or less;
Nb: 0.005% or more and 0.050% or less;
Cr: 0.01% or more and 1.00% or less;
B: 0.0002% or more and 0.0050% or less;
V: 0.001% or more and 0.300% or less;
Ni: 0.01% or more and 2.00% or less;
Cu: 0.01% or more and 2.00% or less;
W: 0.01% or more and 2.00% or less;
Ca: 0.0001% or more and 0.0100% or less;
Ce: 0.0001% or more and 0.0100% or less;
Mg: 0.0001% or more and 0.0100% or less;
Zr: 0.0001% or more and 0.0100% or less;
La: 0.0001% or more and 0.0100% or less;
REM: 0.0001% or more and 0.0100% or less;
Sn: 0.001% or more and 1.000% or less; and
Sb: 0.001% or more and 0.200% or less.

### Claim 5 (depends on 3)

The galvannealed steel sheet according to claim 3, wherein a difference in Fe concentration in mass % in a width direction in the galvannealed layer is less than 1.0%, and a difference in the number density of martensite grains each having an aspect ratio of 5 or more in the width direction is 10% or less.

### Claim 6 (depends on 5)

The galvannealed steel sheet according to claim 5, wherein the component composition comprises one or two or more of: in mass %,
Ti: 0.01% or more and 0.10% or less;
Mo: 0.01% or more and 0.30% or less;
Nb: 0.005% or more and 0.050% or less;
Cr: 0.01% or more and 1.00% or less;
B: 0.0002% or more and 0.0050% or less;
V: 0.001% or more and 0.300% or less;
Ni: 0.01% or more and 2.00% or less;
Cu: 0.01% or more and 2.00% or less;
W: 0.01% or more and 2.00% or less;
Ca: 0.0001% or more and 0.0100% or less;
Ce: 0.0001% or more and 0.0100% or less;
Mg: 0.0001% or more and 0.0100% or less;
Zr: 0.0001% or more and 0.0100% or less;
La: 0.0001% or more and 0.0100% or less;
REM: 0.0001% or more and 0.0100% or less;
Sn: 0.001% or more and 1.000% or less; and
Sb: 0.001% or more and 0.200% or less.

### Claim 7 (depends on 1)

The galvannealed steel sheet according to claim 1, wherein a difference in Fe concentration in mass % in a width direction in the galvannealed layer is less than 1.0%, and a difference in the number density of martensite grains each having an aspect ratio of 5 or more in the width direction is 10% or less.

### Claim 8 (depends on 7)

The galvannealed steel sheet according to claim 7, wherein the component composition comprises one or two or more of: in mass %,
Ti: 0.01% or more and 0.10% or less;
Mo: 0.01% or more and 0.30% or less;
Nb: 0.005% or more and 0.050% or less;
Cr: 0.01% or more and 1.00% or less;
B: 0.0002% or more and 0.0050% or less;
V: 0.001% or more and 0.300% or less;
Ni: 0.01% or more and 2.00% or less;
Cu: 0.01% or more and 2.00% or less;
W: 0.01% or more and 2.00% or less;
Ca: 0.0001% or more and 0.0100% or less;
Ce: 0.0001% or more and 0.0100% or less;
Mg: 0.0001% or more and 0.0100% or less;
Zr: 0.0001% or more and 0.0100% or less;
La: 0.0001% or more and 0.0100% or less;
REM: 0.0001% or more and 0.0100% or less;
Sn: 0.001% or more and 1.000% or less; and
Sb: 0.001% or more and 0.200% or less.