# US 11,118,250 B2 · Fe—Cr—Ni alloy and method for production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,250 B2
- Document ID: US11118250B2
- Status: Granted
- Kind: B2
- Application number: 16/335,042
- Filed: 2017-06-21
- Published: 2020-11-05
- Granted: 2021-09-14
- Earliest claimed: 2016-10-04
- Assignees: Nippon Yakin Kogyo Co., Ltd.
- Applicants: Nippon Yakin Kogyo Co., Ltd.
- Inventors: Kenji Mizuno; Hidekazu Todoroki; Yosuke Baba; Yusuke Kobayashi; Waki Nishijima
- Web page: https://patentgrep.com/patent/US11118250B2

## CPC

- C22C 38/50: with titanium or zirconium
- B22D 11/00: Continuous casting of metals, i.e. casting in indefinite lengths (metal drawing, metal extruding B21C)
- C21C 5/52: Manufacture of steel in electric furnaces {(C21C5/005 takes precedence)}
- C21C 5/54: Processes yielding slags of special composition
- C21C 7/00: Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/00 - C21C5/00 (treating molten metals during moulding B22D1/00, B22D27/00)
- C21C 7/04: Removing impurities by adding a treating agent
- C21C 7/06: Deoxidising, e.g. killing
- C21C 7/064: Dephosphorising; Desulfurising
- C21C 7/068: Decarburising
- C21C 7/072: Treatment with gases (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C21C 7/076: Use of slags or fluxes as treating agents (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C21C 7/10: Handling in a vacuum
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 30/00: Alloys containing less than 50% by weight of each constituent
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/44: with molybdenum or tungsten
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS

## Abstract

Ti, N, Al, Mg, and Ca concentrations are controlled in order to prevent aggregation of TiN inclusions. Furthermore, not only is a Fe—Cr—Ni alloy having superior surface property provided, but also a method is proposed in which the Fe—Cr—Ni alloy is produced at low cost using commonly used equipment. The Fe—Cr—Ni alloy includes C≤0.05%, Si: 0.1 to 0.8%, Mn: 0.2 to 0.8%, P≤0.03%, S≤0.001%, Ni:16 to 35%, Cr: 18 to 25%, Al: 0.2 to 0.4%, Ti: 0.25 to 0.4%, N≤0.016%, Mg: 0.0015 to 0.008%, Ca≤0.005%, O: 0.0002 to 0.005%, freely selected Mo: 0.5 to 2.5% in mass % and Fe and inevitable impurities as the remainder, wherein Ti and N satisfy % N×% Ti≤0.0045 and the number of TiN inclusions not smaller than 5 μm is 20 to 200 pieces/cm2 at a freely selected cross section.

## Claims

### Claim 1

Fe—Cr—Ni alloy comprising:
C<0.05%, Si: 0.1 to 0.8%, Mn: 0.2 to 0.8%, P<0.03%, S<0.001%, Ni:16 to 35%, Cr: 18 to 23%, Al: 0.2 to 0.4%, Ti: 0.25 to 0.4%, N<0.016%, Mg: 0.0015 to 0.008%, Ca<0.005%, 0: 0.0002 to 0.005% in mass %, and Fe and inevitable impurities as the remainder,
wherein Ti and N satisfy % N×% Ti<0.0045 and the number of TiN inclusions not smaller than 5 μm is 20 to 200 pieces/cm2 at a freely selected cross section, and
the alloy contains CaO—MgO—Al2O3 as an oxide type inclusion as a necessary component, contains one or more kinds selected from MgO.Al2O3, MgO and CaO as a freely selected component, and a percentage of the total numbers of MgO and CaO inclusions with respect to total oxides (CaO—MgO—Al2O3, MgO.Al2O3, MgO and CaO) inclusions is not more than 50%.

### Claim 2 (depends on 1)

The Fe—Cr—Ni alloy according to claim 1, wherein the number of TiN inclusions not smaller than 10 μm is not more than 30 pieces/cm2 at a freely selected cross section.

### Claim 3 (depends on 1)

The Fe—Cr—Ni alloy according to claim 1, wherein compositions of the CaO—MgO—Al2O3 inclusion are CaO: 20 to 40%, MgO: 20 to 40% and Al2O3: 20 to 50% and compositions of the MgO.Al2O3 inclusion are MgO: 20 to 40% and Al2O3: 60 to 80%.

### Claim 4 (depends on 3)

The Fe—Cr—Ni alloy according to claim 3, wherein compositions of the CaO—MgO—Al2O3 inclusion are CaO: 20 to less than 30%, MgO: more than 30 to 40% and Al2O3: 30 to 50%.

### Claim 5 (depends on 1)

The Fe—Cr—Ni alloy according to claim 1, wherein the alloy further comprises Mo: 0.5 to 2.5% in mass %.

### Claim 6 (depends on 1)

A method for production of Fe—Cr—Ni alloy according to claim 1, comprising steps of:
melting raw materials in an electric furnace,
decarburizing in AOD and/or VOD,
adding Si and Al,
adding lime and fluorite so as to form CaO—SiO2—MgO—Al2O3—F slag
in order to perform Cr reduction, deoxidation and desulfuration,
adding Ti, and
forming into a slab by a continuous casting apparatus.

### Claim 7 (depends on 6)

The method for production of Fe—Cr—Ni alloy according to claim 6, wherein compositions of the CaO—SiO2—MgO—Al2O3—F slag are CaO: 50 to 70%, SiO2: not more than 10%, MgO: 7 to 15%, Al2O3: 10 to 20% and F: 4 to 15%.
