# US 11,118,247 B2 · Highly processable single crystal nickel alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,247 B2
- Document ID: US11118247B2
- Status: Granted
- Kind: B2
- Application number: 16/352,136
- Filed: 2019-03-13
- Published: 2020-02-13
- Granted: 2021-09-14
- Earliest claimed: 2014-05-27
- Assignees: QuesTek Innovations LLC
- Applicants: Questek Innovations LLC
- Inventors: Jiadong Gong; David R. Snyder; Jason T. Sebastian
- Web page: https://patentgrep.com/patent/US11118247B2

## CPC

- C22C 19/057: {with the maximum Cr content being less 10%}
- B22D 21/005: {with high melting point, e.g. Be 1280 degrees C, Ti 1725 degrees C}
- B22D 25/02: by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)}
- C22C 1/023: {Alloys based on nickel}
- C22C 19/05: with chromium
- C22F 1/10: of nickel or cobalt or alloys based thereon
- F01D 5/28: Selecting particular materials; {Particular measures relating thereto;} Measures against erosion or corrosion
- F05D 2220/323: for aircraft propulsion, e.g. jet engines
- F05D 2230/21: by casting
- F05D 2300/17: Alloys
- F05D 2300/607: Monocrystallinity
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

Alloys, processes for preparing the alloys, and articles including the alloys are provided. The alloys can include, by weight, about 4% to about 7% aluminum, 0% to about 0.2% carbon, about 7% to about 11% cobalt, about 5% to about 9% chromium, about 0.01% to about 0.2% hafnium, about 0.5% to about 2% molybdenum, 0% to about 1.5% rhenium, about 8% to about 10.5% tantalum, about 0.01% to about 0.5% titanium, and about 6% to about 10% tungsten, the balance essentially nickel and incidental elements and impurities.

## Claims

### Claim 1

An alloy consisting of by weight, 5.5% to 6.5% aluminum, 0% to 0.2% carbon, 8.5% to 9.5% cobalt, 6.5% to 7.5% chromium, 0.05% to 0.15% hafnium, 0.6% to 1.2% molybdenum, 0.8% to 1.2 rhenium, 9% to 10% tantalum, 0.05% to 0.15% titanium, 7.5% to 8.5% tungsten, 0% to 0.5% lanthanum, 0% to 0.5% yttrium, and 0% to 0.5% boron the balance nickel and incidental impurity elements,
wherein the alloy is a single crystal; and
wherein the alloy has a reduction in liquid density of less than 0.025 g/cm3 at 40% solidification of the alloy.

### Claim 2 (depends on 1)

The alloy of claim 1, wherein the alloy has a reduction in liquid density of less than 0.015 g/cm3 at 20% solidification of the alloy.

### Claim 3 (depends on 1)

The alloy of claim 1, wherein the alloy is essentially free of freckles.

### Claim 4 (depends on 1)

The alloy of claim 1, wherein the alloy is essentially free of topologically close-packed phases.

### Claim 5 (depends on 1)

The alloy of claim 1, wherein the alloy has a γ′ phase fraction of greater than 59% at 1000° C.

### Claim 6 (depends on 1)

The alloy of claim 1, wherein the alloy has a γ′ phase fraction of greater than 45% after aging the alloy at 1150° C. for 30 hours.

### Claim 7 (depends on 1)

The alloy of claim 1, wherein the absolute value of the γ/γ′ lattice misfit of the alloy is 0 to 0.35% at 1000° C.

### Claim 8 (depends on 7)

The alloy of claim 7, wherein the γ′ precipitates have a cuboidal morphology.

### Claim 9 (depends on 1)

The alloy of claim 1, wherein the interfacial energy normalized coarsening rate constant is 7.0×10−20 or less at 1000° C.

### Claim 10 (depends on 1)

The alloy of claim 1, wherein the alloy has a hardness of greater than 440 HV after aging.

### Claim 11 (depends on 1)

The alloy of claim 1, wherein the alloy consists of, by weight: 5.9% aluminum, 9% cobalt, 7% chromium, 0.1% hafnium, 0.9% molybdenum, 1% rhenium, 9.5% tantalum, 0.11% titanium, and 7.8% tungsten, the balance nickel and incidental impurity elements.

### Claim 12

A method for producing an alloy comprising:
preparing a melt that consists of, by weight, 5.5% to 6.5% aluminum, 0% to 0.2% carbon, 8.5% to 9.5% cobalt, 6.5% to 7.5% chromium, 0.05% to 0.15% hafnium, 0.6% to 1.2% molybdenum, 0.8% to 1.2 rhenium, 9% to 10% tantalum, 0.05% to 0.15% titanium, 7.5% to 8.5% tungsten, 0% to 0.5% lanthanum, 0% to 0.5% yttrium, and 0% to 0.5% boron, the balance nickel and incidental impurity elements wherein the alloy is a single crystal; and wherein the alloy has a reduction in liquid density of less than 0.025 g/cm3 at 40% solidification of the alloy.

### Claim 13 (depends on 12)

The method of claim 12, wherein the melt is molded into a casting, wherein the casting is homogenized by treatment for 2 hours at 1282° C., 2 hours at 1292° C., 6 hours at 1300° C., and 4 hours at 1305° C., with a heating rate of 0.5° C./second between each step; and cooling to room temperature in air.

### Claim 14 (depends on 13)

The method of claim 13, wherein the casting is tempered by treatment for 4 hours at 1121° C. followed by 20 hours at 871° C.

### Claim 15

A manufactured article comprising an alloy that consists of, by weight, 5.5% to 6.5% aluminum, 0% to 0.2% carbon, 8.5% to 9.5% cobalt, 6.5% to 7.5% chromium, 0.05% to 0.15% hafnium, 0.6% to 1.2% molybdenum, 0.8% to 1.2 rhenium, 9% to 10% tantalum, 0.05% to 0.15% titanium, 7.5% to 8.5% tungsten, 0% to 0.5% lanthanum, 0% to 0.5% yttrium, and 0% to 0.5% boron the balance nickel and incidental impurity elements wherein the alloy is a single crystal; and wherein the alloy has a reduction in liquid density of less than 0.025 g/cm3 at 40% solidification of the alloy.

### Claim 16 (depends on 15)

The article of claim 15, wherein the article is the blade of an industrial gas turbine or a blade used in an aerospace application.