# US 11,118,245 B2 · Alkaline solution method for recovering rare earth elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,245 B2
- Document ID: US11118245B2
- Status: Granted
- Kind: B2
- Application number: 15/844,127
- Filed: 2017-12-15
- Published: 2018-06-21
- Granted: 2021-09-14
- Earliest claimed: 2016-12-16
- Assignees: Pioneer Astronautics
- Applicants: Pioneer Astronautics
- Inventors: Mark Berggren; Robert Zubrin; John T Henri; Boris Nizamov
- Web page: https://patentgrep.com/patent/US11118245B2

## CPC

- C22B 59/00: Obtaining rare earth metals
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/008: {by an alkaline or ammoniacal leaching}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Novel methods of recovering neodymium and related rare earth elements from permanent magnets of various compositions are described. The methods employ processing steps including converting the magnet material to a higher surface area form such as a powder, treating the mixture with alkaline solutions to form product concentrated in neodymium and rare earth metals. Inexpensive materials such as ammonia, ammonium carbonate, carbon dioxide, water are recycled in a process that uses moderate temperatures, pressures and non-corrosive and environmentally-friendly chemicals.

## Claims

### Claim 1

A method of recovering a rare earth element (REE) comprising the steps of:
converting a variable composition mixture to a higher surface area form;
treating the converted variable composition mixture with an alkaline solution;
isolating the rare earth element in the alkaline solution; and
treating the alkaline solution, after isolating the rare earth element, with carbon dioxide to form solids concentrated in said rare earth element.

### Claim 2 (depends on 1)

The method of claim 1 where said variable composition mixture before being converted to the higher surface area form is a permanent neodymium iron boron magnet.

### Claim 3 (depends on 1)

The method of claim 1 where the alkaline solution is an ammonium hydroxide/ammonium carbonate solution.

### Claim 4 (depends on 1)

The method of claim 1 where said variable composition mixture before being converted to the higher surface area form is a permanent samarium-cobalt magnet.

### Claim 5 (depends on 1)

The method of claim 1 where said variable composition mixture before being converted to the higher surface area form is a REE-containing waste.

### Claim 6 (depends on 1)

A method of claim 1 where ammonium carbonate of the alkaline solution is recycled as ammonia and carbon dioxide gas after use.

### Claim 7 (depends on 1)

A method of claim 1 where ammonium carbonate of the alkaline solution is directly recycled after use.

### Claim 8 (depends on 1)

A method of claim 1 where the converted variable composition mixture is obtained as a powder of neodymium and other elements by hydrogen decrepitation of a neodymium magnet.

### Claim 9 (depends on 1)

A method of claim 1 where the converted variable composition mixture is obtained as a powder of neodymium and other elements by crushing and grinding.

### Claim 10 (depends on 1)

A method of claim 1 where magnetic properties of the converted variable composition mixture are removed by exposure to temperatures approaching or exceeding its Curie temperature.

### Claim 11 (depends on 1)

A method of claim 1 where the converted variable composition mixture is converted to oxide form.

### Claim 12 (depends on 1)

A method of claim 1 where the alkaline solution comprises a saturated ammonium carbonate solution.

### Claim 13 (depends on 1)

A method of claim 1 where the alkaline solution comprises a solution of ammonia and ammonium carbonate.

### Claim 14 (depends on 13)

A method of claim 13 where a concentration of the solution of the ammonia and the ammonium carbonate is between 1% and saturated.

### Claim 15 (depends on 13)

A method of claim 13 where the solution of the ammonia and the ammonium carbonate is heated to a temperature between −20 and 100° C.

### Claim 16 (depends on 1)

A method of claim 1 further comprising treating the converted variable composition mixture with the alkaline solution at a pressure between 0 and 500 psi.

### Claim 17 (depends on 1)

A method of claim 1 further comprising treating the converted variable composition mixture with the alkaline solution in an oxygen free inert atmosphere.

### Claim 18 (depends on 1)

A method of claim 1 further comprising treating the converted variable composition mixture with the alkaline solution in an oxygen-containing atmosphere.

### Claim 19 (depends on 1)

A method of claim 1 where ultrasonic waves are used in the treating the converted variable composition mixture with an alkaline solution step.

### Claim 20 (depends on 1)

A method of claim 1 further comprising treating the converted variable composition mixture with the alkaline solution under ambient conditions.

### Claim 21 (depends on 1)

A method of claim 1 further comprising treating the converted variable composition mixture with the alkaline solution in a continuous loop over the converted variable composition mixture.

### Claim 22 (depends on 1)

A method of claim 1 where dysprosium and praseodymium are isolated along with neodymium.

### Claim 23 (depends on 1)

A method of claim 1 where a filtrate of the converted variable composition mixture and the alkaline solution are treated by evaporation.

### Claim 24

A method of recovering a rare earth element (REE) from an ore mineral composition comprising the steps of:
converting the ore mineral composition to a higher surface form,
treating the converted ore mineral composition with an alkaline solution,
isolating the REE from the treated and converted ore mineral composition in the alkaline solution, and
treating the alkaline solution, after isolating the REE, with carbon dioxide to form solids concentrated in said REE.

### Claim 25 (depends on 24)

A method of claim 24 where ammonium carbonate of the alkaline solution is recycled as ammonia and carbon dioxide gas after use.

### Claim 26 (depends on 24)

A method of claim 24 where ammonium carbonate of the alkaline solution is directly recycled after use.

### Claim 27 (depends on 24)

A method of claim 24 where the alkaline solution comprises a saturated ammonium carbonate solution.

### Claim 28 (depends on 24)

A method of claim 24 where a solution of ammonia and ammonium carbonate is used in isolating the REE from the treated and converted ore mineral composition and the alkaline solution.

### Claim 29 (depends on 24)

A method of claim 24 where the converted ore mineral composition is obtained as a powder of neodymium compounds and other chemical compounds by crushing and grinding.

### Claim 30 (depends on 24)

A method of claim 24 where the converted ore mineral composition is converted to oxide form.

### Claim 31 (depends on 28)

A method of claim 28 where a concentration of the ammonia and ammonium carbonate solution is between 1% and saturated.

### Claim 32 (depends on 28)

A method of claim 28 where the ammonia and ammonium carbonate solution is heated to a temperature between −20 and 100° C.

### Claim 33 (depends on 24)

A method of claim 24 further comprising treating the converted ore mineral composition with the alkaline solution in an oxygen free inert atmosphere.

### Claim 34 (depends on 24)

A method of claim 24 further comprising treating the converted ore mineral composition with the alkaline solution in an oxygen-containing atmosphere.

### Claim 35 (depends on 24)

A method of claim 24 where ultrasonic waves are used in the treating the converted ore mineral composition with an alkaline solution step.

### Claim 36 (depends on 24)

A method of claim 24 further comprising treating the converted ore mineral composition with the alkaline solution under ambient conditions.

### Claim 37 (depends on 24)

A method of claim 24 further comprising treating the converted ore mineral composition with the alkaline solution in a continuous loop over the converted ore mineral composition.

### Claim 38 (depends on 24)

A method of claim 24 where dysprosium and praseodymium are isolated along with neodymium.

### Claim 39 (depends on 24)

A method of claim 24 where the alkaline solution is treated with hydrogen peroxide.

### Claim 40 (depends on 24)

A method of claim 24 where pretreatment of the converted ore mineral composition, by exposure to hydrogen at temperatures up to 1500° C., is used to reduce oxidation of iron and other metals.

### Claim 41 (depends on 24)

A method of claim 24 where an ammonium carbonate solution is used to selectively dissolve the REE in isolating the REE from the treated and converted ore mineral composition upon oxidation of the treated and converted ore mineral composition.

### Claim 42 (depends on 24)

A method of claim 24 where an ammonium carbonate plus an ammonia solution are used to selectively dissolve the REE from the ore mineral composition upon oxidation of the ore mineral composition.

### Claim 43 (depends on 24)

A method of claim 24 where an addition of NH3 or NH4OH to the converted ore mineral composition causes precipitation of the REE when treating the converted ore mineral composition with the alkaline solution.

### Claim 44 (depends on 24)

A method of claim 24 where addition of NH3 or NH4OH to the converted ore mineral composition causes precipitation of iron when treating the converted ore mineral composition with the alkaline solution.

### Claim 45 (depends on 24)

A method of claim 24 where at least one of CO2, air, oxygen, or hydrogen peroxide is used to change pH, Eh to cause precipitation of the REE when treating the converted ore mineral composition with the alkaline solution.

### Claim 46 (depends on 24)

A method of claim 24 further comprising adjusting pH to cause precipitation of the REE when treating the converted ore mineral composition with the alkaline solution.

### Claim 47 (depends on 24)

A method of claim 24 where heat, steam, or evaporation is employed to cause precipitation of the REE when treating the converted ore mineral composition with the alkaline solution.

### Claim 48 (depends on 24)

A method of claim 24 where vacuum or evaporation is employed to cause precipitation of the REE when treating the converted ore mineral composition with the alkaline solution.

### Claim 49 (depends on 24)

A method of claim 24 where at least one of metal, H2, CO, or carbon are employed to adjust pH, Eh of the REE when treating the converted ore mineral composition with the alkaline solution to cause precipitation of the REE.

### Claim 50 (depends on 24)

A method of claim 24 further comprising recycling an ammonium carbonate/ammonia solution after a precipitation of solids when treating the converted ore mineral composition with the alkaline solution.

### Claim 51 (depends on 24)

A method of claim 24 further comprising steam stripping the alkaline solution to recover clean NH3 and CO2.

### Claim 52 (depends on 24)

A method of claim 24 where multiple dissolution stages are employed to further separate the REE from iron.