# US 11,118,088 B2 · Adhesive articles including a cushion layer and a continuous shell layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,088 B2
- Document ID: US11118088B2
- Status: Granted
- Kind: B2
- Application number: 15/733,208
- Filed: 2018-12-14
- Published: 2020-11-26
- Granted: 2021-09-14
- Earliest claimed: 2017-12-21
- Assignees: 3M Innovative Properties Company
- Applicants: 3M Innovative Properties Company
- Inventors: David J. Yarusso; Ross E. Behling; Peter M. Simone; Chaodi Li; Zhong Chen; Sharon Wang; Jingjing Ma; Eric D. Shockey
- Web page: https://patentgrep.com/patent/US11118088B2

## CPC

- C09J 7/385: {Acrylic polymers}
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2301/208: the adhesive layer being constituted by at least two or more adjacent or superposed adhesive layers, e.g. multilayer adhesive
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2433/00: Presence of (meth)acrylic polymer
- Y10T 428/28: Web or sheet containing structurally defined element or component and having an adhesive outermost layer
- Y10T 428/2848: Three or more layers
- Y10T 428/2891: including addition polymer from alpha-beta unsaturated carboxylic acid [e.g., acrylic acid, methacrylic acid, etc.] Or derivative thereof
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An adhesive article including: a flexible backing; a first cushion layer permanently bonded to a first surface of the flexible backing, wherein the first cushion layer: has an average thickness of at least 10 micrometers; and includes an acrylate pressure-sensitive adhesive having a Fox Tg of up to −30° C., wherein the acrylate pressure-sensitive adhesive includes a (meth)acrylate copolymer; and a first continuous shell layer adjacent the first cushion layer, wherein: the first continuous shell layer has an average thickness of up to 25 micrometers; the ratio of the first cushion layer average thickness to the first shell layer average thickness is at least 2:1; the first continuous shell layer includes an adhesive having a Fox Tg of −20° C. to +50° C.; and the first continuous shell layer adhesive includes a copolymer having a weight average molecular weight of at least 100,000 Daltons.

## Claims

### Claim 1

An adhesive article comprising:
a flexible backing;
a first cushion layer permanently bonded to a first surface of the flexible backing, wherein the first cushion layer:
has an average thickness of at least 10 micrometers; and
comprises an acrylate pressure-sensitive adhesive having a Fox Tg of up to −30° C., wherein the acrylate pressure-sensitive adhesive comprises a (meth)acrylate copolymer comprising:
a) one or more first (meth)acrylate monomeric units of Formula (I) in an amount of at least 60 wt-%, based on a total weight of monomeric units in the (meth)acrylate copolymer:
wherein:
R1 is hydrogen or a methyl group; and
R2 is an alkyl, heteroalkyl, aryl, aralkyl, or alkaryl group with the proviso that the one or more first (meth)acrylate monomeric units of Formula (I) with R2 having at least 8 carbon atoms is present in an amount of at least 20 wt-%, based on a total weight of monomeric units in the (meth)acrylate copolymer; and
b) one or more polar monomeric units in an amount of up to 7 wt-%, based on a total weight of monomeric units in the (meth)acrylate copolymer;
wherein a total weight of all monomeric units of the (meth)acrylate copolymer of the first cushion layer (meth)acrylate copolymer equals 100% by weight; and
a first continuous shell layer adjacent the first cushion layer, wherein:
the first continuous shell layer has an average thickness of up to 25 micrometers;
the ratio of the first cushion layer average thickness to the first continuous shell layer average thickness is at least 2:1;
the first continuous shell layer comprises an adhesive having a Fox Tg of −20° C. to +50° C.; and
the adhesive of the first continuous shell layer comprises a copolymer having a weight average molecular weight of at least 100,000 Daltons, wherein the copolymer comprises:
a) one or more low Tg (meth)acrylate monomeric units of Formula (II) in an amount of at least 25 wt-%, based on a total weight of monomeric units in the copolymer, wherein the one or more low Tg (meth)acrylate monomeric units is characterized as a homopolymer of the one or more (meth)acrylate monomeric units having a Tg of no greater than 0° C.:
wherein:
R1 is hydrogen or a methyl group; and
R3 is an alkyl, heteroalkyl, aryl, aralkyl, or alkaryl group having 2 to 24 carbon atoms;
b) one or more polar monomeric units in an amount of up to 5 wt-%, based on a total weight of monomeric units in the copolymer; and
c) one or more high Tg nonpolar monomeric units in an amount of at least 35 wt-%, based on a total weight of monomeric units in the copolymer, wherein the one or more high Tg (meth)acrylate monomeric units is characterized as a homopolymer of the one or more (meth)acrylate monomeric units having a Tg of greater than 0° C.;
wherein a total weight of all monomeric units of the copolymer of the first continuous shell layer equals 100% by weight.

### Claim 2 (depends on 1)

The adhesive article of claim 1 wherein the acrylate pressure-sensitive adhesive of the first cushion layer has a Fox Tg of at least −85° C.

### Claim 3 (depends on 1)

The adhesive article of claim 1 wherein the ratio of the first cushion layer average thickness to the first continuous shell layer average thickness is at least 3:1 and up to 300:1.

### Claim 4 (depends on 1)

The adhesive article of claim 1 wherein R2 of the one or more (meth)acrylate monomeric units of Formula (I) in the first cushion layer is an alkyl group having 1 to 24 carbon atoms.

### Claim 5 (depends on 4)

The adhesive article of claim 4 wherein the one or more (meth)acrylate monomeric units of Formula (I) is derived from monomers selected from the group of 2-ethylhexyl (meth)acrylate, methyl (meth)acrylate, ethyl (meth)acrylate, n-butyl (meth)acrylate, isobutyl (meth)acrylate, cyclohexyl (meth)acrylate, hexyl (meth)acrylate, 2-octyl (meth)acrylate, isooctyl (meth)acrylate, isononyl (meth)acrylate, isobornyl (meth)acrylate, norbornyl (meth)acrylate, isostearyl (meth)acrylate, behenyl (meth)acrylate, 2-methylbutyl (meth)acrylate, and combinations thereof.

### Claim 6 (depends on 1)

The adhesive article of claim 1 wherein the one or more polar monomeric units in the (meth)acrylate copolymer of the first cushion layer is derived from monomers selected from the group of (meth)acrylic acid, (meth)acrylamide, alkyl-substituted (meth)acrylamides, and combinations thereof.

### Claim 7 (depends on 1)

The adhesive article of claim 1 wherein the one or more polar monomeric units of the copolymer in the first continuous shell layer is present in an amount of 0.5 wt-% to 5 wt-%, based on a total weight of monomeric units in the copolymer.

### Claim 8 (depends on 1)

The adhesive article of claim 1 wherein R3 in the one or more low Tg (meth)acrylate monomeric units of Formula (II) of the copolymer in the first continuous shell layer is an alkyl group having 2 to 24 carbon atoms.

### Claim 9 (depends on 8)

The adhesive article of claim 8 wherein the one or more low Tg (meth)acrylate monomeric units of Formula (II) in the first continuous shell layer is derived from monomers selected from the group of 2-ethylhexyl (meth)acrylate, ethyl acrylate, n-butyl acrylate, isobutyl acrylate, hexyl (meth)acrylate, 2-octyl acrylate, isooctyl acrylate, isononyl acrylate, isostearyl acrylate, 2-methylbutyl acrylate, and combinations thereof.

### Claim 10 (depends on 1)

The adhesive article of claim 1 wherein the one or more polar monomeric units in the copolymer of the first continuous shell layer is derived from monomers selected from the group of (meth)acrylic acid, (meth)acrylamide, alkyl-substituted (meth)acrylamides, and combinations thereof.

### Claim 11 (depends on 1)

The adhesive article of claim 1 wherein the one or more high Tg nonpolar monomeric units in the copolymer of the first continuous shell layer is derived from monomers selected from the group of styrene, substituted styrene, isobornyl (meth)acrylate, methyl (meth)acrylate, tert-butyl (meth)acrylate, iso-butyl methacrylate, cyclohexyl (meth)acrylate, norbornyl (meth)acrylate, and combinations thereof.

### Claim 12 (depends on 1)

The adhesive article of claim 1 wherein the (meth)acrylate copolymer in the first cushion layer further comprises vinyl acetate monomeric units in an amount of up to 7 wt-%, based on the total weight of monomeric units in the copolymer.

### Claim 13 (depends on 1)

The adhesive article of claim 1 wherein the copolymer in the first continuous shell layer further comprises vinyl acetate monomeric units in an amount of up to 7 wt-%, based on the total weight of monomeric units in the copolymer.

### Claim 14 (depends on 1)

The adhesive article of claim 1 wherein the one or more polar monomeric units of the (meth)acrylate copolymer in the first cushion layer has an acid group and the one or more polar monomeric units of the copolymer in the first continuous shell layer has a basic group.

### Claim 15 (depends on 1)

The adhesive article of claim 1 wherein the one or more polar monomeric units of the (meth)acrylate copolymer in the first cushion layer has a basic group and the one or more polar monomeric units of the copolymer in the first continuous shell layer has an acidic group.

### Claim 16 (depends on 1)

The adhesive article of claim 1 wherein the (meth)acrylate copolymer of the first cushion layer has a weight average molecular weight of at least 100,000 Daltons and up to 2,000,000 Daltons.

### Claim 17 (depends on 1)

The adhesive article of claim 1 which demonstrates an increase in 180° angle peel adhesion strength at a peel rate of 0.2 in/min (0.08 mm/sec) from stainless steel at room temperature compared to an adhesive article having the same flexible backing and first cushion layer but without the first continuous shell layer.

### Claim 18 (depends on 17)

The adhesive article of claim 17 which demonstrates at least an increase in 180° angle peel adhesion strength at a peel rate of 0.2 in/min (0.08 mm/sec) from stainless steel or polypropylene at a temperature of up to 65° C. compared to an adhesive article having the same flexible backing and first cushion layer but without the first continuous shell layer.

### Claim 19 (depends on 17)

The adhesive article of claim 17 which demonstrates an average rolling ball stopping distance according to a Rolling Ball Tack Test of at least 200 mm.

### Claim 20 (depends on 1)

The adhesive article of claim 1 further comprising:
a second cushion layer permanently bonded to a second surface of the flexible backing, wherein the second cushion:
has an average thickness of at least 10 micrometers; and
comprises the acrylate pressure-sensitive adhesive of the first cushion layer; and
a second continuous shell layer adjacent the second cushion layer, wherein:
the second continuous shell layer has an average thickness of up to 25 micrometers;
the ratio of the second cushion layer average thickness to the second shell layer average thickness is at least 2:1; and
the second continuous shell layer comprises the adhesive having a Fox Tg of −20° C. to +50° C. of the first continuous shell layer.