# US 11,118,087 B2 · Film-forming resin composition, laminated film, and article to which laminated film is attached

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,087 B2
- Document ID: US11118087B2
- Status: Granted
- Kind: B2
- Application number: 16/978,495
- Filed: 2019-02-13
- Published: 2021-01-14
- Granted: 2021-09-14
- Earliest claimed: 2018-03-13
- Assignees: Natoco Co., Ltd.
- Applicants: Natoco Co., Ltd.
- Inventors: Susumu Ono; Takashi Tanaka; Takafumi Yoshino
- Web page: https://patentgrep.com/patent/US11118087B2

## CPC

- C08G 18/44: Polycarbonates
- C09D 183/04: Polysiloxanes
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/40: comprising polyurethanes
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08G 18/10: Prepolymer processes involving reaction of isocyanates or isothiocyanates with compounds having active hydrogen in a first reaction step
- C08G 18/4063: {Mixtures of compounds of group C08G18/62 with other macromolecular compounds}
- C08G 18/4072: {Mixtures of compounds of group C08G18/63 with other macromolecular compounds}
- C08G 18/4216: {from mixtures or combinations of aromatic dicarboxylic acids and aliphatic dicarboxylic acids and dialcohols}
- C08G 18/4238: {derived from dicarboxylic acids and dialcohols}
- C08G 18/4615: {containing nitrogen}
- C08G 18/61: Polysiloxanes
- C08G 18/6229: {Polymers of hydroxy groups containing esters of acrylic or methacrylic acid with aliphatic polyalcohols}
- C08G 18/6254: {Polymers of alpha-beta ethylenically unsaturated carboxylic acids and of esters of these acids containing hydroxy groups}
- C08G 18/6295: {Polymers of silicium containing compounds having carbon-to-carbon double bonds}
- C08G 18/755: {and at least one isocyanate or isothiocyanate group linked to a secondary carbon atom of the cycloaliphatic ring, e.g. isophorone diisocyanate}
- C08G 18/757: {containing at least two isocyanate or isothiocyanate groups linked to the cycloaliphatic ring by means of an aliphatic group}
- C08G 18/758: {containing two or more cycloaliphatic rings}
- C08G 18/7614: {containing only one aromatic ring}
- C08G 18/7621: {being toluene diisocyanate including isomer mixtures}
- C08G 18/7642: {containing at least two isocyanate or isothiocyanate groups linked to the aromatic ring by means of an aliphatic group having a primary carbon atom next to the isocyanate or isothiocyanate groups, e.g. xylylene diisocyanate or homologues substituted on the aromatic ring}
- C08G 18/7831: {containing biuret groups}
- C08G 18/7837: {containing allophanate groups}
- C08G 18/792: {formed by oligomerisation of aliphatic and/or cycloaliphatic isocyanates or isothiocyanates}
- C09D 133/14: of esters containing halogen, nitrogen, sulfur or oxygen atoms in addition to the carboxy oxygen
- C09D 175/04: Polyurethanes
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Provided is a film-forming resin composition for protecting an article that an organic polymer is exposed, including a polyurethane resin (A) having a hydroxyl group, a (meth)acrylic resin (B) having a hydroxyl group, and a polyfunctional isocyanate (C), in which the composition has a cross-linking density n of 1.0×10−4 to 5.0×10−3 mol/cm3, which is determined according to Mathematical Formula (1) n=E′min/(3RT). Here, E′min represents a minimum value E′min of storage elastic modulus of a cured film obtained by curing the resin composition at 80° C. for 16 hours in a case where the cured film is subjected to viscoelasticity measurement at a frequency of 1.0 Hz and a temperature range of −40° C. to 160° C., T represents an absolute temperature at the minimum value E′min, and R represents a gas constant.

## Claims

### Claim 1

A film-forming resin composition for protecting a surface of an article, on which an organic polymer is exposed, comprising:
a polyurethane resin (A) having a hydroxy group;
a (meth)acrylic resin (B) having a hydroxy group; and
a polyfunctional isocyanate (C),
wherein a cured film obtained by curing the resin composition at 80° C. for 16 hours has a cross-linking density n of 1.0×10−4 to 5.0×10−3 mol/cm3, which is determined from a minimum value E′min of storage elastic modulus of the cured film in a case where the cured film is subjected to viscoelasticity measurement at a frequency of 1.0 Hz and a temperature range of −40° C. to 160° C., an absolute temperature T at the minimum value E′min, and a gas constant R, according to Mathematical Formula (1)
Mathematical Formula (1): n=E′min/(3RT), and
wherein a cured film obtained by curing the resin composition at 80° C. for 16 hours has a glass transition temperature of −20° C. to 60° C. obtained in a case where the cured film is subjected to viscoelasticity measurement at a frequency of 1.0 Hz and a temperature range of −40° C. to 160° C., and has a loss tangent (tan δ) of equal to or more than 0.5 at the glass transition temperature.

### Claim 2 (depends on 1)

The film-forming resin composition according to claim 1,
wherein the polyurethane resin (A) having a hydroxy group has a weight average molecular weight of 1,000 to 50,000.

### Claim 3 (depends on 1)

The film-forming resin composition according to claim 1,
wherein the (meth)acrylic resin (B) has a hydroxyl value of 10 to 200 mgKOH/g.

### Claim 4 (depends on 1)

The film-forming resin composition according to claim 1,
wherein the polyurethane resin (A) has at least any partial structure selected from the group consisting of polycaprolactone, polycaprolactam, polycarbonate, polyester, and polyether.

### Claim 5 (depends on 1)

The film-forming resin composition according to claim 1,
wherein the (meth)acrylic resin (B) has at least any partial structure selected from the group consisting of polycaprolactone, polycaprolactam, polycarbonate, polyester, and polyether.

### Claim 6 (depends on 1)

The film-forming resin composition according to claim 1,
wherein the polyurethane resin (A) and/or the (meth)acrylic resin (B) has a polysiloxane partial structure.

### Claim 7 (depends on 1)

The film-forming resin composition according to claim 1, further comprising:
a polysiloxane compound (D) having a hydroxy group.

### Claim 8 (depends on 1)

The film-forming resin composition according to claim 1, further comprising:
a polyol (E) as a component different from the polyurethane resin (A).

### Claim 9

A laminated film for protecting a surface of an article, on which an organic polymer is exposed, comprising:
a base material layer; and
a protective layer,
wherein the protective layer has a cross-linking density n of 1.0×10−4 to 5.0×10−3 mol/cm3, which is determined from a minimum value E′min of storage elastic modulus of the protective layer in a case where the protective layer is subjected to viscoelasticity measurement at a frequency of 1.0 Hz and a temperature range of −40° C. to 160° C., an absolute temperature T at the minimum value E′min, and a gas constant R, according to Mathematical Formula (1),
wherein the protective layer has a glass transition temperature of −20° C. to 60° C. obtained in a case where the protective layer is subjected to viscoelasticity measurement at a frequency of 1.0 Hz and a temperature range of −40° C. to 160° C., and has a loss tangent (tan δ) of equal to or more than 0.5 at the glass transition temperature
Mathematical Formula (1): n=E′min/(3RT), and
wherein the protective layer is a cured product of a film-forming resin composition comprising:
a polyurethane resin (A) having a hydroxy group;
a (meth)acrylic resin (B) having a hydroxy group; and
a polyfunctional isocyanate (C).

### Claim 10 (depends on 9)

The laminated film according to claim 9,
wherein a material of the base material layer is at least any selected from the group consisting of polyester, polyurethane, polyvinyl chloride, triacetyl cellulose, polyacrylic resin, polycarbonate, and thermoplastic polyimide.

### Claim 11 (depends on 9)

An article to which the laminated film according to claim 9 is attached.