# US 11,118,079 B2 · Water-based barrier coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,079 B2
- Document ID: US11118079B2
- Status: Granted
- Kind: B2
- Application number: 16/066,779
- Filed: 2016-12-28
- Published: 2018-12-13
- Granted: 2021-09-14
- Earliest claimed: 2015-12-31
- Assignees: Kemira Oyj
- Applicants: Kemira Oyj
- Inventors: Tarja Turkki; Sai Li; Jonni Ahlgren
- Web page: https://patentgrep.com/patent/US11118079B2

## CPC

- C09D 125/14: with unsaturated esters
- B65D 65/42: Applications of coated or impregnated materials
- C08F 212/08: Styrene
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 251/00: Macromolecular compounds obtained by polymerising monomers on to polysaccharides or derivatives thereof
- C08F 261/04: on to polymers of vinyl alcohol
- C08L 29/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C09D 129/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C09D 133/06: of esters containing only carbon, hydrogen and oxygen, the oxygen atom being present only as part of the carboxyl radical
- C09D 133/10: Homopolymers or copolymers of methacrylic acid esters
- C09D 151/02: grafted on to polysaccharides
- D21H 19/40: siliceous, e.g. clays
- D21H 19/50: Proteins
- D21H 19/54: Starch
- D21H 19/56: Macromolecular organic compounds or oligomers thereof obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C08F 2800/20: as weight or mass percentages
- C08K 3/34: Silicon-containing compounds
- C08K 5/053: Polyhydroxylic alcohols
- C08L 3/02: Starch; Degradation products thereof, e.g. dextrin
- C08L 89/005: {Casein}
- C08L 93/04: Rosin
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A water-based barrier coating composition suitable for use as a barrier coating is disclosed which includes an aqueous polymer composition obtainable by free radical (co)polymerizing an ethylenically unsaturated monomer blend having an optionally substituted styrene, at least one C1-C4-alkyl (meth)acrylate, other ethylenically unsaturated copolymerizable monomers, degraded starch polyvinyl alcohol (PVA), a plasticizer; a composition having C16-C18 alkenyl ketene dimer, optionally as a mixture with rosin, of a gelling agent; and optionally a filler.

## Claims

### Claim 1

A method for barrier coating a subject, comprising:
providing a water-based barrier coating composition containing:
(A): (i) 40 to 95% by weight of a total weight of (A), an aqueous polymer composition obtainable by free radical (co)polymerizing an ethylenically unsaturated monomer blend containing:
(a) 0 to 70% by weight of at least one optionally substituted styrene,
(b) up to 100% by weight of at least one C1-C4-alkyl (meth)acrylate,
(c) 0 to 10% by weight of other ethylenically unsaturated copolymerizable monomers, in a presence of,
(d) 0 to 40% % by weight of degraded starch having a molecular weight Mn of 500 to 10,000, wherein a sum (a)+(b)+(c)+(d) is 100%;
(ii) 2 to 55% by weight of the total weight of (A) of polyvinyl alcohol (PVA), optionally polymerized together with components of (i);
(iii) 2 to 30% by weight of the total weight of (A) of a plasticizer;
(iv) 5 to 30% by weight of the total weight of (A) a composition containing C16-C18 alkenyl ketene dimer, optionally as a mixture with rosin, whereby a ratio of the C16-C18 alkenyl ketene dimer:rosin is from 100:0 to 25:75;
(v) 5 to 20% by weight of the total weight of (A) of a gelling agent; and
(B): a filler, wherein a ratio of (A):(B) is from 2:5 to 1:1; and
applying the water-based barrier coating composition to at least part of a surface of a subject by
applying the water-based barrier coating composition as a first water-based coating composition, wherein said first water-based coating composition contains (A) and (B), to at least part of a surface of a subject to obtain a precoated subject; and
then applying the second water-based barrier coating composition as a second water-based composition, wherein said second water-based coating composition comprises (A) but does not contain (B), to at least a precoated surface of the subject to obtain a top coated subject.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein the first water-based coating composition comprises:
0% by weight of (iv), and the second water-based coating composition comprises:
more than 0% by weight of (iv).

### Claim 3 (depends on 1)

A method as claimed in claim 1, wherein said subject is paper or paperboard.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein said subject is a food packaging.

### Claim 5 (depends on 1)

Method for barrier coating a subject with a water-based barrier coating composition, as claimed in claim 1 for forming a grease barrier on paper or paperboard.

### Claim 6 (depends on 1)

A method as claimed in claim 1, wherein a sum (i)+(ii)+(iii)+(iv)+(v) is 100%.

### Claim 7 (depends on 1)

A method as claimed in claim 1, wherein the PVA (ii) is selected from a group consisting of fully or partially hydrolyzed grades having molecular weight equal to or less than 50000.

### Claim 8 (depends on 1)

A method as claimed in claim 1, wherein the plasticizer (iii) is selected from a group consisting of glycerol, polyethylene glycol (PEG), sorbitol, and mixtures thereof.

### Claim 9 (depends on 1)

A method as claimed in claim 1, wherein the gelling agent (v) is a protein or an alginate.

### Claim 10 (depends on 9)

A method as claimed in claim 9, wherein the gelling agent (v) is selected from a group consisting of corn, zein, whey, casein, soy protein, carboxy methyl cellulose and gluten.

### Claim 11 (depends on 10)

A method as claimed in claim 10, wherein the gelling agent (v) is gluten.

### Claim 12 (depends on 1)

A method as claimed in claim 1, wherein the filler (B) is talc or kaolin.

### Claim 13 (depends on 1)

A method as claimed in claim 1, wherein the aqueous polymer composition (i) is obtained by free radical (co)polymerization of ethylenically unsaturated monomer blend comprising:
(a) 0 to 70% by weight of at least one optionally substituted styrene,
(b) up to 100% by weight of at least one C1-C4-alkyl (meth)acrylate, and
(c) 0 to 10% by weight of other ethylenically unsaturated copolymerizable monomers, in a presence of,
(d) 0 to 40% by weight of degraded starch having a molecular weight Mn of 500 to 10,000, and
(e) a graft-linking, water-soluble redox system as free radical initiator for the free radical emulsion copolymerization,
wherein a sum (a)+(b)+(c)+(d) is 100%.

### Claim 14 (depends on 1)

A method as claimed in claim 1, wherein components of (i) and (ii) are polymerized together.

### Claim 15 (depends on 14)

A method as claimed in claim 14, wherein a mixture of (i) and (ii) is a free radical emulsion copolymerization of ethylenically unsaturated monomers comprising:
(a) 0 to 60% by weight of at least one optionally substituted styrene,
(b) up to 100% by weight of at least one C1-C4-alkyl (meth)acrylate, and
(c) 0 to 10% by weight of other ethylenically unsaturated copolymerizable monomers, and (ii), in the presence of:
(d) 0 to 40% by weight of degraded starch having a molecular weight Mn of 500 to 10,000, and
(e) a graft-linking, water-soluble redox system as free radical initiator for the free radical emulsion copolymerization.

### Claim 16 (depends on 15)

A method as claimed in claim 15, wherein the amount of starch (d) is 0% by weight.

### Claim 17 (depends on 15)

A method as claimed in claim 15, wherein a ratio of (i):(ii) is from 45:55 to 60:40.

### Claim 18 (depends on 14)

A method as claimed in claim 14, wherein an amount of (i) is 45 to 60% by weight of the total weight of (A) and the amount of (ii) is 40 to 55% by weight of the total weight of (A).

### Claim 19 (depends on 1)

A method as claimed in claim 1, wherein the mixture of (i) and (ii) is a blended mixture.

### Claim 20 (depends on 1)

A method as claimed in claim 1, wherein an amount of (i) is 50 to 95% by weight of the total weight of (A), and an amount of (ii) is 2 to 20% by weight of the total weight of (A).

### Claim 21 (depends on 19)

A method as claimed in claim 19, wherein an amount of starch (d) is 20 to 40% by weight.

### Claim 22 (depends on 21)

A method as claimed in claim 21, wherein an amount of component (iv) is from 2 to 15% by weight of the total weight of (A).

### Claim 23 (depends on 1)

A method as claimed in claim 1, wherein a ratio of alkenyl ketene dimer:rosin (iv) is from 8:2 to 2:8.

### Claim 24 (depends on 1)

A method as claimed in claim 1, wherein a glass transition temperature (Tg) of the (co)polymer is from −40° C. to 50° C.

### Claim 25 (depends on 1)

A method as claimed in claim 1, wherein an amount of (a) is 20 to 60%, by weight.

### Claim 26 (depends on 1)

A method as claimed in claim 1, wherein the monomer component (b) is n-butyl acrylate.