# US 11,118,057 B1 · Attenuation material composition, attenuation material and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,057 B1
- Document ID: US11118057B1
- Status: Granted
- Kind: B1
- Application number: 17/217,086
- Filed: 2021-03-30
- Granted: 2021-09-14
- Earliest claimed: 2020-04-09
- Assignees: China University of Petroleum-Beijing
- Applicants: China University of Petroleum (Beijing)
- Inventors: Pinbo Ding; Shiqi Huang; Jianxin Wei; Bangrang Di; Feng Zhang; Lianbo Zeng; Xiangyang Li
- Web page: https://patentgrep.com/patent/US11118057B1

## CPC

- C08L 83/04: Polysiloxanes
- C08G 59/4007: {Curing agents not provided for by the groups C08G59/42 - C08G59/66}
- C08G 59/4085: {silicon containing compounds}
- C08G 59/56: together with other curing agents
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- G09B 23/40: for geology
- C08G 77/04: Polysiloxanes
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- G09B: EDUCATIONAL OR DEMONSTRATION APPLIANCES; APPLIANCES FOR TEACHING, OR COMMUNICATING WITH, THE BLIND, DEAF OR MUTE; MODELS; PLANETARIA; GLOBES; MAPS; DIAGRAMS (devices for psychotechnics or for testing reaction times A61B5/16; games, sports, amusements A63; projectors, projector screens G03B)

## Abstract

The attenuation material composition disclosed in the present disclosure comprises a room temperature vulcanized silicone rubber, an epoxy resin, a first curing agent and a second curing agent, wherein the first curing agent comprises ethyl orthosilicate and dibutyltin oxide; and the weight ratio of the room temperature vulcanized silicone rubber to the epoxy resin is (0.1-1):1.

## Claims

### Claim 1

An attenuation material composition comprising a room temperature vulcanized silicone rubber, an epoxy resin, a first curing agent and a second curing agent, wherein the first curing agent comprises ethyl orthosilicate and dibutyltin oxide; the weight ratio of the room temperature vulcanized silicone rubber to the epoxy resin is (0.1-1):1; and the weight ratio of the ethyl orthosilicate to the dibutyltin oxide is 100:(2-4).

### Claim 2 (depends on 1)

The composition of claim 1, wherein the weight ratio of the ethyl orthosilicate to the dibutyltin oxide is 100:(2.5-3.5).

### Claim 3 (depends on 1)

The composition of claim 1, wherein the weight ratio of the room temperature vulcanized silicone rubber to the first curing agent is 100:(2-4).

### Claim 4 (depends on 3)

The composition of claim 3, wherein the weight ratio of the room temperature vulcanized silicone rubber to the first curing agent is 100:(2.5-3.5).

### Claim 5 (depends on 1)

The composition of claim 1, wherein the room temperature vulcanized silicone rubber is 10-100 parts by weight, the first curing agent is 0.3-3 parts by weight, and the second curing agent is 10-30 parts by weight, based on 100 parts by weight of the epoxy resin.

### Claim 6 (depends on 5)

The composition of claim 5, wherein the room temperature vulcanized silicone rubber is 45-55 parts by weight, the first curing agent is 1-2 parts by weight, and the second curing agent is 15-25 parts by weight, based on 100 parts by weight of the epoxy resin.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the second curing agent is an aliphatic amine curing agent.

### Claim 8 (depends on 7)

The composition of claim 7, wherein the aliphatic amine curing agent has a viscosity within a range of 50-120 mPa·s at a temperature of 25° C. and an amine value within a range of 600-700 mgKOH/g.

### Claim 9 (depends on 1)

The composition of claim 1, wherein the room temperature vulcanized silicone rubber has a viscosity within a range of 2,000-12,000 mPa·s at a temperature of 25° C.

### Claim 10 (depends on 1)

The composition of claim 1, wherein the epoxy resin has a viscosity within a range of 9,000-14,000 mPa·s at a temperature of 25° C. and an epoxy value within a range of 0.5-0.54 mol/100 g.

### Claim 11 (depends on 1)

A method for preparing an attenuation material with the attenuation material composition of claim 1, including:
(1) subjecting the room temperature vulcanized silicone rubber to a first heat treatment and then subjecting to a first mixing with the first curing agent to obtain a modified silicone rubber;
(2) subjecting the epoxy resin to a second heat treatment and then subjecting to a second mixing with the second curing agent and the modified silicone rubber;
(3) injecting the mixture obtained in step (2) into a mould and performing a curing process.

### Claim 12 (depends on 11)

The method of claim 11, wherein the first heat treatment in step (1) is performed by means of constant temperature heating, and the heating is kept at a temperature of 20-50° C. for 1-48 hours.

### Claim 13 (depends on 11)

The method of claim 11, wherein the conditions of the first mixing in step (1) comprise: the stirring velocity is within a range of 70-95 rpm, and the stirring time is within a range of 6-12 min.

### Claim 14 (depends on 13)

The method of claim 13, wherein the stirring velocity is within a range of 80-90 rpm, and the stirring time is within a range of 8-10 min.

### Claim 15 (depends on 11)

The method of claim 11, wherein the second heat treatment in step (2) is performed by means of constant temperature heating, and the heating is kept at a temperature of 20-50° C. for 1-48 hours.

### Claim 16 (depends on 11)

The method of claim 11, wherein the conditions of the second mixing in step (2) comprise: the stirring velocity is within a range of 70-95 rpm, and the stirring time is within a range of 6-12 min.

### Claim 17 (depends on 11)

The method of claim 11, wherein the conditions of the curing treatment in step (3) comprise: the temperature is within a range of 18-32° C., and the time is within a range of 24-96 hours.

### Claim 18 (depends on 11)

An attenuation material prepared with the method of the claim 11.

### Claim 19 (depends on 18)

A seismic physical model comprised of the attenuation material of claim 18.