# US 11,118,053 B2 · Polyaryletherketone/polyarylene sulfide composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,053 B2
- Document ID: US11118053B2
- Status: Granted
- Kind: B2
- Application number: 16/292,393
- Filed: 2019-03-05
- Published: 2019-09-12
- Granted: 2021-09-14
- Earliest claimed: 2018-03-09
- Assignees: Ticona LLC
- Applicants: Ticona LLC
- Inventors: Xiaowei Zhang; Suresh Subramonian; Xinyu Zhao; Christopher McGrady
- Web page: https://patentgrep.com/patent/US11118053B2

## CPC

- C08L 71/123: {not modified by chemical after-treatment}
- C08G 65/40: from phenols (I) and other compounds (II), e.g. OH-Ar-OH + X-Ar-X, where X is halogen atom, i.e. leaving group
- C08J 5/043: {with glass fibres}
- C08L 71/00: Compositions of polyethers obtained by reactions forming an ether link in the main chain (of polyacetals C08L59/00; of epoxy resins C08L63/00; of polythioether-ethers C08L81/02; of polyether-sulfones C08L81/06); Compositions of derivatives of such polymers
- B29C 45/0001: {characterised by the choice of material}
- B29K 2071/00: Use of polyethers {, e.g. PEEK, i.e. polyether-etherketone or PEK, i.e. polyetherketone or derivatives thereof}, as moulding material
- B29K 2309/08: Glass
- C08J 2371/12: Polyphenylene oxides
- C08J 2481/04: Polysulfides
- C08L 2203/20: use in electrical or conductive gadgets
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A polymer composition comprising at least one polyaryletherketone, at least one polyarylene sulfide, and a plurality of reinforcing fibers is provided. The composition has a melt viscosity of about 250 Pa-s or less as determined in accordance with ISO Test No. 11443:2005 at a shear rate of 1,000 seconds−1 and temperature of about 380° C.

## Claims

### Claim 1

A polymer composition comprising at least one polyaryletherketone, at least one polyarylene sulfide, and a plurality of reinforcing fibers, wherein the polyaryletherketone constitutes from about 40 wt. % to about 80 wt. % of the polymer composition and the polyarylene sulfide constitutes from about 0.5 wt. % to about 15 wt. % of the polymer composition, wherein the composition has a melt viscosity of 250 Pa-s or less as determined in accordance with ISO Test No. 11443:2005 at a shear rate of 1,000 seconds−1 and temperature of about 380° C., wherein the composition exhibits a deflection temperature under load of about 280° C. or more as determined in accordance with ISO Test No. 75-2:2013 at a specified load of 1.8 MPa, and wherein the composition exhibits a tensile strength of from 100 to about 400 MPa as determined in accordance with ISO Test No. 527:2012 at 23° C.

### Claim 2 (depends on 1)

The polymer composition of claim 1, wherein the polyaryletherketone has a glass transition temperature of from about 130° C. to about 230° C.

### Claim 3 (depends on 1)

The polymer composition of claim 1, wherein the polyaryletherketone has a melt viscosity of about 150 Pa-s or more, as determined in accordance with ISO Test No. 11443:2005 at a shear rate of 1,000 s−1 and temperature of about 400° C.

### Claim 4 (depends on 1)

The polymer composition of claim 1, wherein the polyaryletherketone contains a moiety having the structure of Formula (I) and/or Formula (II):
wherein,
m and r are independently zero or a positive integer;
s and w are independently zero or a positive integer;
E and E′ are independently an oxygen atom or a direct link;
G is an oxygen atom, a direct link, or —O-Ph-O— where Ph is a phenyl group; and
Ar is one of the following moieties (i) to (vi), which is bonded via one or more of phenyl moieties to adjacent moieties:

### Claim 5 (depends on 4)

The polymer composition of claim 4, wherein the polyaryletherketone contains a repeat unit of the following general Formula (III):
wherein,
A and B are independently 0 or 1.

### Claim 6 (depends on 4)

The polymer composition of claim 4, wherein the polyaryletherketone contains a repeat unit of the following general Formula (IV):
wherein,
A and B are independently 0 or 1.

### Claim 7 (depends on 1)

The polymer composition of claim 1, wherein the polyaryletherketone is polyetheretherketone, polyetherketone, polyetherketoneketone, polyetherketoneetherketoneketone, polyetheretherketoneketone, polyether-diphenyl-ether-ether-diphenyl-ether-phenyl-ketone-phenyl, or a blend or copolymer thereof.

### Claim 8 (depends on 1)

The polymer composition of claim 1, wherein the polyarylene sulfide is a polyphenylene sulfide.

### Claim 9 (depends on 1)

The polymer composition of claim 1, wherein the polyarylene sulfide has a melt viscosity of about 150 Pa-s or les, as determined in accordance with ISO Test No. 11443:2005 at a shear rate of 1,200 seconds−1 and temperature of about 310° C.

### Claim 10 (depends on 1)

The polymer composition of claim 1, wherein the polyarylene sulfide is present in an amount of from about 1 to about 60 parts per 100 parts by weight of the polyaryletherketone.

### Claim 11 (depends on 1)

The polymer composition of claim 1, wherein the polyarylene sulfide constitutes from about 2 wt. % to about 15 wt. % of the polymer composition.

### Claim 12 (depends on 1)

The polymer composition of claim 1, wherein the reinforcing fibers have an aspect ratio of from about 1.5 to about 10, the aspect ratio being defined as the cross-sectional width of the fibers divided by the cross-sectional thickness of the fibers.

### Claim 13 (depends on 1)

The polymer composition of claim 1, wherein the reinforcing fibers include glass fibers.

### Claim 14 (depends on 1)

The polymer composition of claim 1, wherein the reinforcing fibers are present in an amount of from about 20 to about 80 parts per 100 parts by weight of the polyaryletherketone.

### Claim 15 (depends on 1)

The polymer composition of claim 1, wherein the reinforcing fibers constitute from about 5 wt. % to about 60 wt. % of the polymer composition.

### Claim 16 (depends on 1)

The polymer composition of claim 1, wherein the polyaryletherketone constitutes from about 45 wt. % to about 75 wt. % of the polymer composition.

### Claim 17 (depends on 1)

The polymer composition of claim 1, wherein the ratio of the melt viscosity of the polymer composition to the melt viscosity of the polyaryletherketone is about 0.98 or less.

### Claim 18 (depends on 1)

The polymer composition of claim 1, further comprising an organosilane compound.

### Claim 19 (depends on 1)

The polymer composition of claim 1, wherein after being submerged in an aqueous solution containing 20% by volume of water and heated at a temperature of 150° C. for 2,000 hours, the composition exhibits a hydrolytic tensile strength, wherein the ratio of the hydrolytic tensile strength to the tensile strength prior to being submerged in the aqueous solution is about 0.5 or more.

### Claim 20 (depends on 1)

The polymer composition of claim 1, wherein the composition exhibits a V0 rating as determined in accordance with UL94 at a thickness of 1.6 mm.

### Claim 21 (depends on 1)

The polymer composition of claim 1, wherein the composition exhibits a V0 rating as determined in accordance with UL94 at a thickness of 0.4 mm after conditioning for 48 hours at 23° C. and 50% relative humidity.

### Claim 22 (depends on 1)

A shaped part comprising the polymer composition of claim 1.

### Claim 23 (depends on 22)

The shaped part of claim 22, wherein the shaped part is injection molded.

### Claim 24 (depends on 22)

An electronic component comprising the shaped part of claim 22.

### Claim 25 (depends on 1)

The polymer composition of claim 1, wherein the composition is free of an organosilane compound.